Export:  BibTeX | EndNote (RIS)      
Abstract  The application of PHACOMP with a view to estimating the amount of σ-phase in complex iron-base superalloys has been carried out. Results obtained on certain commercial as well as experimental heats sustained its usefulness. The formula:△N′_V= Ni-3Ti-3.5A1-1.7Si-0.9Cr-4.7 has been found to be useful in predicting the conditions with regard to the formation of σ-phase of a 25Ni-15Cr type alloy as an example. When △N_V>0, the alloy remained σ-free after prolonged exposure at 650℃.
Received:  18 April 1978     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1978/V14/I4/440

[1] Beattie, H. J., J. Appl. Phys., 24 (1953) , 1322.
[2] Boesch, W. J. and Slaney, J. S., Metal Progr., 86 (1964) , 109.
[3] Woodyatt, L. R. et al., Trans. AIME, 236 (1966) , 519.
[4] Sims, C. T., J. Metals, 18 (1966) , 1119.
[5] Dreshfield, R. L., ASM Trans. Quart., 61 (1968) , 352.
[6] Dreshfleld, R. L., Met. Trans., 2 (1971) , 1341.
[7] Barrows, R. G. and Newkirk, J. B., Met. Trans., 3 (1972) , 2889.
[8] Sims, C. T., J. Metals, 21 (1969) , № 12, 27.
[9] Murphy, H. J. et al., J. Metals, 20 (1968) , № 11, 46.
[10] Cowan, T.W., J. Metals, 20 (1968) , № 11, 22.
[11] Collins, H. E. and Kortovich, C. S., J. Mater., 4 (1969) , 62.
[12] Restall, J. E. and Toulson, E. C., Metals Mater., 7 (1973) , № 3, 134.
[13] Kreige, O. H. and Baris, J. M., ASM Trans. Quart., 62 (1969) , 195.
[14] Gow, J. T. and Harder, O.E., Trans. Amer. Soc. Metals, 30 (1942) , № 3-4, 855.
[15] 铁基高温合金研究组,金属学报,14(1978) ,227.
[16] Hattersley, B. and Hume-Rothery, W., J. Iron Steel Inst., London, 204 (1966) , 683.
[17] Jones, J. D, and Hume-Rothery, W., J. Iron Steel Inst., London, 204 (1966) , 1.
[18] 北京钢铁学院、大冶钢厂,未发表资料.
[19] Cook, A. J. and Brown, B. R., J. Iron Steel Inst., London, 171 (1952) , 345.
No related articles found!
No Suggested Reading articles found!