| EFFECT OF COPPER ON THE RECRYSTALLIZATION TEXTURE OF COLD ROLLED LOW CARBON STEEL SHEET |
| Zhou Yong-xin Huang Qing-zhu Chen Qian-ti Deng Ding-qing Pu Shao-kang(Research Institute of Wuhan Iron and Steel Company) |
|
Cite this article:
Zhou Yong-xin Huang Qing-zhu Chen Qian-ti Deng Ding-qing Pu Shao-kang(Research Institute of Wuhan Iron and Steel Company). EFFECT OF COPPER ON THE RECRYSTALLIZATION TEXTURE OF COLD ROLLED LOW CARBON STEEL SHEET. Acta Metall Sin, 1978, 14(3): 292-338.
|
|
|
Abstract The recrystallization texture of cold-rolled low-carbon steel sheets containing copper up to 0.355% has been studied by means of X-ray pole density measurement, plastic strain ratio measurement and metallographic etching-pit technique. It is shown that the {111} texture component, which is beneficial to the deep-drawing ability, appears to be enhanced with increasing copper content, especially when the copper content exceeds the limit of solubility. Fine precipitates of ε-Cu phase around dislocation in specimens containing 0.355% Cu have been observed by transmission electron microscopy. The presence of such precipitates may be regarded as the cause of the enhancement of the {111} texture component.
|
|
Received: 18 March 1978
|
[1] 大橋延夫,川畸制鉄技報,5(1973) ,№ 2,164. [2] Rickett, R. L. and Leslie, W. C., Trans. Amer. Soc. Metals, 51 (1959) , 310. [3] Leslie, W. C., Trans. AIME, 221 (1961) , 752. [4] Wacquez, P. and Van Daele, R., Sheet Metal Ind., 44 (1967) , № 477, 21. [5] 清水峰男,鉄鋼,58(1972) ,№ 4,S.267. [6] 须藤正俊,橋本俊一,铁鋼,58(1972) ,№ 11,S.476. [7] 稻垣裕辅,铁鋼,59(1973) ,№ 4,S.198. [8] 小西元幸,鉄鋼,59(1973) ,№ 4,S.200. [9] 阿部秀夫,铁鋼,59(1973) ,№ 4,S.199. [10] 阿部秀夫,鉄鋼,60(1974) ,217. [11] 阿部秀夫鈴木竹四,鉄鋼,60(1974) ,№ 11,S.487. [12] 金子輝雄,寺畸富久長,日本特開昭50-75114,(1975) . [13] Guimaraes, J. R. C. et al., Metallography, 9 (1976) , 1. [14] Mould, P. R. and Gray, J. M., Met. Trans., 3 (1972) , 3121. [15] Strassburger, C., Stahl Eisen, 94 (1974) , 409. [16] Tassy-Betz, E. and J., Metallography, 7 (1974) , 91. [17] 野村伸吾,鉄鋼,61(1975) ,54. [18] Wriedt, H. A. and Darken, L. S., Trans. AIME, 218 (1960) , 30. |