Abstract The very severe attack of the dolomite lining of oxygen-blown steel-making converters by high P_2O_5 containing slags has been considered on phase relations. In steel-making practice, no difference was observed between slags of high and of low P_2O_5 content in their attack upon MgO in dolomite linings, but upon CaO in the same linings was more severe and the higher the P_2O_5 content of the slag, the greater the attack. Reasons for these are as follows:1. At 1600℃ the slag of high P_2O_5 content is a homogeneous liquid or a heterogeneous liquid of high reactivity with CaO, whereas the slag of low P_2O_5 content is a heterogeneous liquid of low reactivity with CaO.2. At 1600℃ the slag of high P_2O_5 content sometimes appears to be a twophase liquid, which attacks CaO severey, whereas the slag of low P_2O_5 content is always an one-phase liquid.3. with slags of high P_2O_5 content, the greater the amount of SiO_2 present, the higher will be its saturation for CaO, thus rendering the attack on CaO more severe. This is not the case, however, with slags of low P_2O_5 content.The above problem may be remedied by introducing more CaO in slag.
|
Received: 18 March 1978
|
[1] Bobrownicki, W. and Slawski, K., Rocz. Chem., 33 (1959) , 251; referred to Arch. Eisenhuettenw.. 38 (1967) , 595. [2] Drewes, E. J. and Olette, M., Arch. Eisenhuettenw. 38 (1967) , 163. [3] Tromel, G. et al., ibid. 38 (1967) , 595. [4] Tromel, A. et al., ibid, 45 (1974) , 671. [5] Fleischer, H. J. and Fischer, W. A., ibid, 38 (1967) , 185. [6] Knuppel, H. and Oters, F., Stahl Eisen, 81 (1961) , 1437. [7] Siegers, S., Dip.-Arb. T. U. Berlin, 1968, referred to Arch. Eisenhuettenw, 44 (1973) , 451. [8] Euler, R., Ber. Deut. Keram. Ges., 44 (1967) , 345. |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|