Acta Metall Sin  1978, Vol. 14 Issue (2): 188-216    DOI:
Current Issue | Archive | Adv Search |
A REVIEW ON THE BEHAVIOR OF THE ADDITION OF RARE-EARTH IN STEEL
Chen Pei-fang
Cite this article: 

Chen Pei-fang. A REVIEW ON THE BEHAVIOR OF THE ADDITION OF RARE-EARTH IN STEEL. Acta Metall Sin, 1978, 14(2): 188-216.

Download:  PDF(2723KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  1. Effect of rare earth elements on the properties of steel2. Functions of rare-earth in steel2.1 Cleaning effect and modification of inclusion morphology(1) Deoxidation(2) Desulphurization and sulphide-control(3) Others2.2 Alloying effect and its interaction with interstitials3. Methods of addition of rare-earth elements in steelmaking4. Blockade of ladle nozzle during teeming
Received:  18 February 1978     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1978/V14/I2/188

[1] 北京钢铁学院金属物理教研组,鞍山钢铁公司汽车钢板研究组,金属学报,10(1974) ,27.
[2] Croll, J. E. and McDonald, J. K., J. Aust. Inst. Metals, 19 (1974) , № 3, 161.
[3] Gondoh, H., Sugimura, S. and Yamanoto, S., AWRA Symposium on Development in Gas Pipeline Technology, May 1973.
[4] Lorenz, L., Gammal, T. El. and Dahl, W., Arch. Eisenhuettenw., 44 (1973) , 843.
[5] Lorenz, L., Gammal,T. El. and Dahl, W., Arch. Eisenhuettenw., 45 (1974) , 645.
[6] Bittence, C. J., Mach. Des., 46 (1974) , № 30, 134.
[7] Luyckx, L., Bell, J. R., McLean. A. and Korchynsky, M., Met. Trans., 1 (1970) , 3341.
[8] #12
[9] Fuchs, A., Arch. Eisenhuettenw., 46; (1975) , 127.
[10] Lorenz, L., Gammal, T. El. and Dahl, W., Arch. Eisenhuettenw., 45 (1974) , 891.
[11] Brownrigg, A. and Chambers, F. M., J. Iron Steel Inst., 208 (1970) , 1078.
[12] 小指軍夫,鉄と鋼,61(1975) .2998.
[13] Wilson, W. G., Weld. J., 53 (1974) , 691.
[14] 刘怀文,钢铁评述,1976.
[15] Wilson, W. G., Weld. J., 50 (1971) , 42s.
[16] 上田修三,船越督己,田中哲夫,腰塚典明,石川正明,铁と鋼,60(1974) ,S.549.
[17] 上田修三,石川正明,上林邦彦,船越督己,铁と鋼,61(1975) ,S.598.
[18] #12
[19] #12
[20] 包头钢铁公司中央实验室,稀土金属在碳素铸钢中的应用,(1976年3月).
[21] 长谷川正義,佐野正之,田辺伊佐雄,鉄と鋼,51(1965) ,1163.
[22] Rahmel, A. and Scholz, W., Werks. Korros., 22 (1971) , 510.
[23] 庄司雄次,秋山俊一郎,私市 優,永利匡辅,星 弘充,鉄と鋼,63(1977) ,700.
[24] 饭泉省三,衣笠雅晋,藤岡外喜夫,鉄と鋼,63(1977) ,715.
[25] Hillinger, H., Werks. Korros., 22 (1971) , 504.
[26] 深瀨幸重,遅沢浩一郎,根本力男,日本金属学会誌,33(1969) ,40.
[27] 深瀨幸重,遅沢浩一郎,根本力男,日本金属学会誌,33(1969) ,46.
[28] 庄司雄次,鉄と鋼,62(1976) ,S.755.
[29] Barrett, C. A. and Lowell, C. E., Oxid. Metals., 9 (1975) , 307.
[30] Wood, G. C. and Boustead, J., Corros. Sci., 8 (1968) , 719.
[31] Tien, J. K. and Rand, W. H., Scr. Met., 6 (1972) , 55.
[32] Tien, J. K. and Pettit, F. S., Met. Trans., 3(1972) , 1587.
[33] Seybolt, A. N., Corros. Sci., 6 (1966) , № 6, 263.
[34] Yoshikazu Nakamura, Met. Trans., 5 (1974) , 909.
[35] Wood, G. C., Werks. Korros., 22 (1974) , 491.
[36] 甘粕知一郎,三菱制鋼技報,8(1974) ,№ 2,85.
[37] 斎藤安俊,桐生 堅,木村 孝,天野忠昭,矢島聖使,日本金属学会誌,39(1975) ,1100.
[38] 矢島聖使,斎藤安俊,天野忠昭,電気制鋼,45(1974) ,№ 3,144.
[39] 中村義一,鉄と鋼,60(1974) ,S.590.
[40] #12
[41] 北京钢铁研究院,MoVWBSiRE钢,(1975年).
[42] 西安钢厂,包头钢铁公司冶金研究所,稀土元素对Fe-Cr-Al高温电热合金的作用,(1975年)。
[43] 北京钢丝厂等,低铬FeCrAl电热合金研制的初步结果,(1976年).
[44] 骆继勋等,金属学报,13(1977) 263.
[45] 釜沢謙一,大町良治,特殊鋼,20(1971) ,№ 7,50.
[46] Francis, J. M. and Whitlow, W. H., J. Iron Steel Inst., 204 (1966) , 355.
[47] Francis, J. M. and Whitlow, W. H., Corros. Sci., 5 (1965) , 701.
[48] Felten, E. J., J. Electrochem. Soc., 108 (1961) , 490.
[49] Kvernes, I. A., Oxid. Metals, 6 (1973) , 45.
[50] Horn, L., Z. Metallk., 40 (1949) , 73.
[51] Wenderott, B., Z. Metallk., 56 (1965) , 63.
[52] 鞍山钢铁公司钢铁研究所,稀土元素在65犁铧钢中的应用,(1975年).
[53] 包头钢铁公司,稀土重轨试验小结,(1972年).
[54] 高橋俊夫,五十嵐賢,角 清,関 正雄,高僑洼雄,特公昭46 2742(1971) .
[55] Anon, U. S. Pat., № 2, 876, 095 (1959) .
[56] #12
[57] #12
[58] #12
[59] 兰州化工机械研究所等,耐浓硝酸用钢,(1975年)。
[60] #12
[61] 广州重型机器厂,含稀土18-8Ti不锈铸钢的研究和生产,(1975年8月).
[62] 浙江冶金研究所等,碳铵用钢试验总结,(1974年).
[63] 包头钢铁公司冶金研究所,耐硫酸用钢,(1974年).
[64] 包头钢铁公司中央试验室,耐海水腐蚀用钢试验小结,(1975年).
[65] 包头钢铁公司冶金研究所,稀土对弹簧钢疲劳性能的影响,(1975年).
[66] 川村和郎,渡辺四郎,鈴木節雄,鉄と鋼,60(1974) ,1935.
[67] Wilson, W. G., J. Metals, 26 (1974) , № 5, 14.
[68] Kor, G. J. W., Met. Trans., 4 (1973) , 377.
[69] Fischer, W. A. and Hermann, B., Arch. Eisenhuettenw., 44 (1973) , 97.
[70] #12
[71] Wilson, W, G., Elec. Furnace Conf., Proc., 31 (1973) , 154.
[72] Lu, K. W. and McLean, A., Ironmaking Steelmaking, 1 (1974) , 228.
[73] 包头钢铁公司冶金研究所,金属铈在纯铁中作用的研究,(1975年)。
[74] Leary, R. J. and Wilson, W. G., U. S., Bur. Mines, Rep. Invest. RI-7091, March 1968, 28.
[75] Langenberg, F. C. and Chipman, J., Trans. AIME, 212 (1958) , 290.
[76] Singleton, R. E., Trans. AIME, 215 (1959) , 675.
[77] 草川隆次,大谷利勝,鉄と鋼,51(1965) ,1987.
[78] Schindlerova, V. and Buzek, Z., Hutn. Listy, 21 (1966) , 169.
[79] Schindlerova, V. and Buzek, Z., Hutn. Listy, 21 (1966) , 89.
[80] Fischer, W. A. and Hermann, B., Arch. Eisenhuettenw., 44 (1973) , 87.
[81] 三代祐嗣,数上文夫,飯田義沼,江見俊彦,铁と鋼,59(1973) ,№ 4,S.143.
[82] 成田貴一,宫本 醇,高橋栄沼,鉄と鋼,50(1964) ,2011.
[83] 苟清泉,苏文辉,戴守愚,吉林大学自然科学学报,12(1962) ,№ 1,153.
[84] Schrmann, E., Brauckmann, J. and Voss, H. J., Arch. Eisenhuettenw., 47 (1976) , 1.
[85] 江島彬夫,鈴木健一郎,原田信男,三本木貢沼,鉄と鋼,61(1975) ,2784.
[86] 井上博文,三本木貢沼,東北大学選鉱制錬研彙,29(1973) ,№ 2,193.
[87] #12
[88] Richerd, J., Mere. Sci. Rev. Met., 59 (1962) , 527.
[89] Sims, C. E., Trans. AIME, 215 (1959) , 367.
[90] Baker, T. J. and Charles, J. A., J. Iron Steel Inst., 300 (1972) , 702.
[91] Baker, T. J. and Charles, J. A., J. Iron Steel Inst., 301 (1973) , 187.
[92] Baker, T. J. and Charles, J. A., J. Iron Steel Inst., 300 (1972) , 680.
[93] Mohla, P. P. and Beech, J., J. Iron Steel Inst., 297 (1969) , 177.
[94] Davies, I. G., PB 218920, BSC-MG/39/72, (1972) .
[95] 别所 勇,鉄と鋼,61(1975) ,S.505.
[96] Baker, T. J. and Charles, J. A., Effect of Second-Phase Particles on the Mechanical Properties of Steel, Iron and Steel Inst., London, 1971, p. 79.
[97] 成田貴一,鉄と鋼,61(1975) ,S.506.
[98] Bennett, H. W. and Sandell, L. P. Jr., Elec. Furnace Conf. Proc., 31 (1973) , 167.
[99] Malm, S., Scand. J. Met., 5 (1976) , № 6, 248.
[100] Davies, I. G., Metals Technol., 1 (1974) , № 5, 241.
[101] 桜谷敏和,鉄と鋼,59(1973) ,S.449.
[102] 包头钢铁公司冶金研究所,包头钢铁公司机械总厂,在钢锭模中加稀土方法的探索,(1975年11月),
[103] 大日方逹一,鉄と鋼,6q(1976) ,S.128.
[104] Breyer, N. N. and Gordon, P., The Microstructure and Design of Alloys, Proc. 3rd Int. Conf. on the Strength of Metals and Alloys, Vol, 1, Cambridge, England, Aug. 1973, p. 493.
[105] Breyer, N. B., Park, H. and Mostovy, S., U. S. Pat. № 3, 726, 669 (1973) .
[106] Corradini, D., Australian. Pat. № 401, 335 (1965) .
[107] #12
[108] Wilson, W. G., Proc. 10th Rare Earth Res. Conf., Carefree, Arizona, U. S., 1(1973) , p. 34.
[109] 鞍山钢铁公司第二炼钢厂等,16Mn钢夹杂物、断口和机械性能,(1974年).
[110] 成田貴一,鉄と鋼,61(1975) ,S.80.
[111] 郡司好喜,鉄と鋼,62(1976) ,S.571.
[112] #12
[113] #12
[114] 包头钢铁公司冶金研究所,利用放射性同位素Ce~(141) 研究铈在纯铁中的扩散,(1975年).
[115] #12
[116] #12
[117] #12
[118] #12
[119] Roe, G. J. and Marsh, G. D., J. Metals, 27 (1975) , 15.
[120] 杭州钢铁厂转炉炼钢分厂,小型氧气顶吹转炉生产60#绳钢总结,(1973年).
[121] 由淼,杨继先,陈德源,物理学报,23(1974) ,292.
[122] 葛庭燧,容保粹,王业宁,物理学报,11(1955) ,№ 11,91.
[123] #12
[124] #12
[125] #12
[126] #12
[127] 包头钢铁公司冶金研究所,稀土对含磷钢断裂行为影响的研究,(1977年).
[128] Bingcl, J. and Scott, L. V., Elec. Furnace Conf. Proc., 31 (1973) , 171.
[129] Lyckx, L. and Jackman, J. R., Elec. Furnace Conf. Proc,, 31 (1973) , 175.
[130] #12
[131] #12
[132] Shigeyuki Okazaki,日本 特公昭36-12402(1961) .
[133] Hidetaro Nemoto, Takaho Kawawa, Hidekl Sato, Eiichi Sakamoto, Takayuki Koyano, Takanori Anzai, U. S. Pat. № 3, 871, 870 (1975) .
[134] #12
[135] 陕西钢[
No related articles found!
No Suggested Reading articles found!