STRESS-INTENSITY FACTORS CALCULATED BY DISLOCATION THEORY
Long Qi-wei (Lung Chi-wei) (Institute of Metal Research; Academia Sinica)
Cite this article: 

Long Qi-wei (Lung Chi-wei) (Institute of Metal Research; Academia Sinica). STRESS-INTENSITY FACTORS CALCULATED BY DISLOCATION THEORY. Acta Metall Sin, 1978, 14(2): 118-126.

Download:  PDF(476KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based upon dislocation theory the stress intensity factors can be calculated. The dislocation density distribution function (?) (x) is easily obtained by solving the integral equation with the Chebyshev polynomials. Some stress intensity factors thus calculated for practical cases have been found to agree fairly well with the results obtained by the conventional fracture mechanics.
Received:  18 February 1978     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1978/V14/I2/118

[1] Bilby, B. A. and Eshelby, J. D., in "Fracture", Vol. Ⅰ, edited by H. Liebowitze, Academic Press, New York, 1968, pp. 100-178.
[2] Eshelby, J. D., in "Solid State Physics", edited by F. Seitz and D. Turnbull, Vol. Ⅲ, Academic Press, New York, 1956, p. 79.
[3] Sih, G. C., Handbook of Stress Intensity Factors, (1) 1. 1-24; (2) 1. 3-1, Inst. of Fracture and Solid Mech., Lehigh Univ., Pennsylvania, 1973.
[4] 雷日克,和格拉德什坦,函数表与积分表,高等教育出版社,1959,p.283.
[5] Irving, J. and Mullineux, N., Mathematics in Physics and Engineering, Academic, New York, 1959, p. 633.
[6] 龙期威,待发表工作.
[7] 末发表资料(1977年).
[8] Hirth, J. P. and Lothe, J., Theory of Dislocations, McGraw-Hill, New York, 1968, p. 694.
[9] 梁昆淼,数学物理方法,人民教育出版社,1960,p.132.
No related articles found!
No Suggested Reading articles found!