ON THE CRITERION FOR CRACK EXTENSION
Chen Chih
Cite this article: 

Chen Chih. ON THE CRITERION FOR CRACK EXTENSION. Acta Metall Sin, 1977, 13(z1): 57-153.

Download:  PDF(1937KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the inevitable blunting of the crack-tip and the finiteness of stressand strain, it is shown that the basic criterion for crack extension is either themaximum shear stress criterion (for ductile fracture) or the maximum principalstress criterion (for cleavage fracture) after analyzing three series of experimentaldatum. Critical relations can be deduced under specific conditions. In the caseof plane strain and small scale yielding, this critical relation is just the well-known K_I=K_(Ic)=material constant; whereas, in the case of plane stress andsmall scale yielding, the critical relation deduced is K_c=(π/8kσ_Fε_F~2BE)~(1/2). Factorseffecting K_(Ic) were also discussed.

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1977/V13/Iz1/57

[1] 陈篪、姚蘅,切口尖度与断裂韧度,1974,待发表工作.
[2] Bridgman, P. W., Studies in Large Plastic Flow and Fracture, McGraw, New York, 1952.
[3] 陈篪,待发表工作.
[4] Rosenfield, A. R. and Hahn, G. T., ASM Trans. Quart., 59 (1966) , 962.
[5] 陈篪等,金属学报 11(1975) ,174.
[6] Kobayashi, A. S., Fracture, ed. by H. Liebowitz, Vol. Ⅲ, Academic Pr., New York, 1971, pp. 312--370.
[7] Marloff, R. H. et al., Exp. Mech., 11 (1971) , 529.
[8] Neuber, H., Kerbspannungslehre, Julius Springer, Berlin, 1937.
[9] Weiss, V., Fracture, ed. by H. Liebowitz, Vol. Ⅲ, Academic Pr., New York, 1971, pp. 228--266.
[10] McClintock, F. A. and Irwin, G. R., Amer. Soc. Test. Mater., Spec. Tech. Publ, № 381, pp. 84--113.
[11] 陈篪,力学,1975,№ 2,78.
[12] Neuber, H., J. Appl. Mech., 28 (1961) , 544.
[13] Rice, J. R., J. Appl. Mech., 34 (1971) , 287.
[14] Godwa, C. V. B. and Topper, T. H., J. Appl. Mech., 37 (1970) , 77.
[15] 陈篪、潘灏,待发表工作.
[16] 邓枝生、陈篪,待发表工作.
[17] Hahn, G. T. and Rosenfield, A. R., Amer. Soc. Tech. Mater., Spec. Tech. Publ., № 432, 1968, p. 5.
[18] Birkle, A. J. et al., ASM Trans. Quart., 59 (1966) , 59.
[19] Cox, T. B. and Low, J. R., Met. Trans., 5 (1974) , 1457
No related articles found!
No Suggested Reading articles found!