Please wait a minute...
Acta Metall Sin  1977, Vol. 13 Issue (4): 308-315    DOI:
Current Issue | Archive | Adv Search |
THE GENERAL TREATMENT OF DIFFRACTION GEOMETRY OF AMPLITUDE-MODULATED STRUCTURE
Li Po-tsang Peking Institute of Metallurgical Research
Cite this article: 

Li Po-tsang Peking Institute of Metallurgical Research. THE GENERAL TREATMENT OF DIFFRACTION GEOMETRY OF AMPLITUDE-MODULATED STRUCTURE. Acta Metall Sin, 1977, 13(4): 308-315.

Download:  PDF(578KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 April 1977     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1977/V13/I4/308

[1] Guinier, A., Theorie et Technique de la Radiocristallographie, Dunod, Paris, (1964) .
[2] 郭可信,X射线学及电子显微术的进展,全国第二届金属物理学术会议论文集编辑委员会编,上海科技出版社,(1966) ,27.
[3] Китайгородский, А. И., 结构分析理论, (中译本), 科学出版社, (1965) .
[4] Hoseman, R. and Bagchi, S. N., Direct Analysis of Diffraction by Matter, North-Holland, Amsterdam, (1962) .
[5] Lipson, H. and Taylor, C. A., Fourier Transforms and X-Ray Diffraction, Bell and Sons, London, (1958) .
[6] Jennison, R. C., Fourier Transforms and Covolutions for the Experimentalist, Pergamon, (1961) .C
No related articles found!
No Suggested Reading articles found!