IRON MAKING IN ANCIENT CHINA
LU TA
Cite this article: 

LU TA. IRON MAKING IN ANCIENT CHINA. Acta Metall Sin, 1966, 9(1): 1-3.

Download:  PDF(219KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Metallographic studies of antique iron utensils that had been unearthed in various parts of China revealed the structures of white cast iron, hammered low carbon steel, and black heart maleable iron, indicating that our ancestors in the 3rd or 4th Century B.C. had already mastered the art of making these materials.Brief descriptions are given of an excavated crucible furnace for iron smelting, of the possible ways of converting white cast iron into malleable metal, and of ancient methods of making swords.
Received:  18 January 1966     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1966/V9/I1/1

[1] 黄展岳:考古学报,1957,(3) ,93.
[2] 河南省文化局文物工作队:文物,1960,(1) ,158.
[3] 金槐:文物,1959,(2) ,16.
[4] 孙廷烈:考古学报,1956,(2) ,125.
[5] 华觉明、杨根、刘恩珠:考古学报,1960,(1) ,73.
[6] 中国古代冶金史资料(北京钢铁学院图书馆未刊稿).
[7] 张子高:中国化学史稿(古代之部),(科学出版社,1964) ,97页.
[8] 郑绍宗:考古通讯,1956,(1) ,29.
[9] 孔令坛:钢铁,1957,(5) ,85.
[10] 徐祖耀:金属学原理,(上海科学技术出版社,1964) ,1-2页.
[11] 北史,第89卷,艺术列传.
[12] 周志宏:科学通报,1955,(2) ,25.N
No related articles found!
No Suggested Reading articles found!