AN INVESTIGATION OF THERMO-STABILITY OF POTASSIUM FLUOTANTALATE IN VARIOUS ATMOSPHERES |
FANG CHIN-YING; SU HUNG-Y; SHêN TSING-NANG (Institute of Applied Chemistry; Academic Sinica) |
|
Cite this article:
FANG CHIN-YING; SU HUNG-Y; SHêN TSING-NANG (Institute of Applied Chemistry; Academic Sinica). AN INVESTIGATION OF THERMO-STABILITY OF POTASSIUM FLUOTANTALATE IN VARIOUS ATMOSPHERES. Acta Metall Sin, 1965, 8(4): 435-442.
|
Abstract The thermo-stability of K_2TaF_7 in air and argon atmosphere was investigated by means of thermo-differential, thermo-gravimetric and chemical analyses and also X-ray powder diffraction method. An obvious heat-absorbing effect was observed at 218°±3℃ with the appearance of break-up of larger crystals. The melting point of K_2TaF_7 was measured to be 730°±3℃. During the course of heating, by the action of moisture in air, K_2TaF_7 was hydrolyzed into K_2TaO_2F_3 which is soluble in molten K_2TaF_7 and thus affects its melting point. This might throw light on the disagreement of the melting points of K_2TaF_7 determined by the various authors. The end product of hydrolysis of K_2TaF_7 was identified to be KF and KTaO_3 (potassium meta-tantalate). Finally, the different stages of hydrolytic reaction of K_2TaF_7 and its relation with various temperatures were discussed.
|
Received: 18 April 1965
|
[1] Hahn, O., Putter, K. E.:Z. Anorg. Chem., 1923, 127, 153. [2] Drossbach, P., Petrick, P.:Z. Elektrochem., 1957, 61, 410. [3] #12 [4] 井內俊明、松岛知夫、小野建二:东北大学选矿制炼研究所汇报,1959,15,(2) ,87. [5] 井內俊明、小野建二:东北大学选矿制炼研究所汇报,1960,16,(2) ,133. [6] #12 [7] Quill, L. L.:Z. Anorg. Chem., 1932,208,257. [8] #12 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|