| THE EFFECT OF SURFACE ACTIVE MEDIA ON MACHINING |
| LIU MIN-CHIH;WANG KUI-CHIN Institute of Metal Research; Academia Sinica |
|
Cite this article:
LIU MIN-CHIH;WANG KUI-CHIN Institute of Metal Research; Academia Sinica. THE EFFECT OF SURFACE ACTIVE MEDIA ON MACHINING. Acta Metall Sin, 1965, 8(2): 274-276.
|
|
|
|
|
Received: 18 February 1965
|
[1] Ребиндр, П. А.: 1928. Ребиндер, П. А.: 1931, 72, 91. [2] Ошер, Р. Н.: 金属切削加工用润滑冷却液的制备与应用,(机械工业出版社, 1954年) 38--86页. [3] #12 [4] Machlin, E. S.: Strengthening Mechanisms in Solids, (ASM, 1962) , p. 381--89. |