Please wait a minute...
Acta Metall Sin  1965, Vol. 8 Issue (2): 177-186    DOI:
Current Issue | Archive | Adv Search |
AN EMPIRICAL RELATION BETWEEN THE DISTRIBUTION COEFFICIENT OF IMPURITIES IN BINARY ALLOYS AND THE PHASE DIAGRAM
WANG WEI-YUAN Institute of Metallurgy; Academia Sinica
Cite this article: 

WANG WEI-YUAN Institute of Metallurgy; Academia Sinica. AN EMPIRICAL RELATION BETWEEN THE DISTRIBUTION COEFFICIENT OF IMPURITIES IN BINARY ALLOYS AND THE PHASE DIAGRAM. Acta Metall Sin, 1965, 8(2): 177-186.

Download:  PDF(704KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A linear relation has been obtained between the logarithm of the distribution co-efficient of impurities logK_B and the square root of liquidus composition for componentA x_(A, L)~(1/2). in binary systems of Ge or Si with impurities. This relationship hasbeen found to be also applicable to Au-Bi, Au-Tl, Ag-Bi, Ag-Pb and Ag-Tl systems,where the second element represents the impurity. The distribution coefficients at themelting point (K_B~o) of impurities in Ge or Si obtained by extrapolating to zero concentra-tion are in reasonable agreement with the experimental values. Besides, the values K_B~oof certain impurities in Au, Ag, Cu (from group I), Mg (from group II) and Al (fromgroup III) have been calculated. It is shown that in these systems a simple correlationexists between K_B~o and the maximum molar solid solubility of impurities, just like thatfound earlier by Fischler in the binary systems of Ge or Si.
Received:  18 February 1965     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1965/V8/I2/177

[1] Trumbore, F. A.: Bell System Tech. J., 1960, 39, 205.
[2] Thurmond, C. D., Kowalchik, M.: Bell System Tech. J., 1960, 39, 169.
[3] Hansen, M.: Constitution of Binary Alloys, (McGraw-Hill, 1958) , 有关各图.
[4] Fischler, S.: J. Appl. Phys., 1962, 33, 1615.
[5] Thurmond, C. D., Struthers, J. D.: J. Phys. Chem., 1953, 57, 831.
[6] Hall, R. N.: J. Phys. Chem. Solids, 1957, 3, 63.
[7] Thurmond, C. D.: Semi-conductors, ed. N. B. Hanny, (Reinhold, 1959) , p. 145. [8] Thurmond, C. D.: Metallurgical Society Conferences, Properties of Elemental and Compound Semiconductors, ed. H. C. Gatos, (Interscience, 1960) , p. 121.
[9] Raub, E., Engel, A.: Metallforschung 1946, 1, 76.
[10] Trumbore, F. A., Isenberg, C. R., Porbansky, E. M.: J. Phys. Chem. Solids, 1959, 9, 60.
[11] Trumbore, F. A., Porbansky, E. M., Tartaglia, A. A.: J. Phys. Chem. Solids, 1959, 11, 239.
[12] Thurmond, C. D., Trumbore, F. A., Kowalchik, M.: J. Chem. Phys., 1956, 25, 799L.
[13] Tolmie, E. D., Robins, D. A.: J. Inst. Metals, 1956--57, 85, 171.
[14] Yue, A. S., Clark, J. B.: Trans. AIME, 1958, 212, 881.
[15] Yue, A. S., Clark, J. B.: Trans. AIME, 1960, 218, 55.
[16] #12
[17] Albert, P., Montariol, F., Reich, R. et al.: Radioisotope Conference, ed. J. E. Johnson, (Butterworths, 1954) , vol. 2, p. 75.
[18] Burton, J. A., Prim, R. C., Slichter, W. P.: J. Chem. Phys., 1953, 21, 1987. [19] Kubaschewski, O., Evans, E. LL.: Metallurgical Thermochemistry, 3rd ed., (Pergamon, 1958) , p. 286, 292.
No related articles found!
No Suggested Reading articles found!