FREE ENERGIES OF FORMATION OF Mg_2Si, Mg_2Pb AND Mg_2Sn
CHOU YUAN-HSI(Institute of Metallurgy; Academia Sinica)
Cite this article: 

CHOU YUAN-HSI(Institute of Metallurgy; Academia Sinica). FREE ENERGIES OF FORMATION OF Mg_2Si, Mg_2Pb AND Mg_2Sn. Acta Metall Sin, 1964, 7(3): 327-331.

Download:  PDF(333KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 March 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I3/327

[1] 邹元爔:金属学报,1964,7,217.
[2] Hanson, D., Gayler, M. L. V.: J. Inst. Metals, 1921, 26, 321.
[3] Phillips, H. W. L.: J. Inst. Metals, 1946, 72, 157.
[4] Hume-Rothery, W.: Phil. Mag., 1936, 22, 151.
[5] Phillips, H. W. L.: J. Inst. Metals, 1946, 72, 229.
[6] Kubaschewski, O., Catterall, J. A.: Thermochemical Data of Alloys, (Pergamon, 1956) , vol. 1, p. 31.
[7] Kubaschewski, O., Catterall, J. A.: Thermochemical Data of Alloys, (Pergamon, 1956) , vol. 1, p. 32.
[8] Kubaschewski, O., Catterall, J. A.: Thermochemical Data of Alloys, (Pergamon, 1956) , vol. 1, p. 33.
[9] Hansen, M., Anderko, K.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) , p. 912.
[10] Ashtakala, S., Pidgeon, L. M.: Can. J. Chem., 1962, 40, (4) , 718.
[11] Hansen, M., Anderko, K.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) , p. 919.
[12] Kubaschewski, O., Catterall, J. A.: Thermochemical Data of Alloys, (Pergamon, 1956) , Vol. 1, p. 32-34.
[13] Caulfield, H. J.: Dissertation Abstracts, 1962, 23, 1052.]
No related articles found!
No Suggested Reading articles found!