Please wait a minute...
Acta Metall Sin  1964, Vol. 7 Issue (3): 229-239    DOI:
Current Issue | Archive | Adv Search |
THE THEORETICAL REQUIREMENTS OF CARBON FOR REDUCTION AND HEAT SUPPLY IN BLAST-FURNACE SMELTING
CHEN TA-SHOU(Peking Institute of Ferrous Metallurgy)
Cite this article: 

CHEN TA-SHOU(Peking Institute of Ferrous Metallurgy). THE THEORETICAL REQUIREMENTS OF CARBON FOR REDUCTION AND HEAT SUPPLY IN BLAST-FURNACE SMELTING. Acta Metall Sin, 1964, 7(3): 229-239.

Download:  PDF(882KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A modified diagram of theoretical requirements of carbon in ore reduction and heat supply for iron smelting has been proposed. The carbon requirements for reduction of Fe_3O_4 and that of wustite under different degrees of direct reduction of wiistite are separately considered in the proposed diagram. It is evident that the heat requirement varies with the degree of direct reduction, and is different from that conventionally adopted by some workers.The proposed diagram indicates the possibility of reducing the coke ratio to about 450 kg/ton of pig-iron, by proper preparation of raw materials, by working with a moderate driving rate under a favourable distribution of ascending gas currents across the furnace cross section to improve the gas utilization and by lowering the starting temperature of reduction of wustite.In actual practice, a surplus of reducing agents above the equilibrium is required, in order to control a proper rate of reduction; and stronger peripheral and central gas currents are required for smoother operation. Thus, the lowest possible coke ratio and the degree of direct reduction are usually higher than that theoretically required for minimum carbon supply, and can only be attained with easily reducible sinters or pellets.
Received:  18 March 1964     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I3/229

[1] #12
[2] Jacob, W., Quade, G.: Stahl Eisen, 1959, 1058.
[3] Schenck, H.: Physikalische Chemie der Eisenhuttenprozesse, (Verlag von Julius Springer, Berlin, 1932) , S. 144.
[4] Schurmann, E., Bulter, D.: Journees Internationales de Siderurgie, (Luxembourg, 1-4 Oct. 1962) .
[5] Michard, J., Daucoisne, P., Chanty, G.: Blast Furnace, Coke Oven, Raw Mater. Comm. Proc., 1961, 329.
No related articles found!