THE MAGNETIC PROPERTIES AND THE DEGREE OF CRYSTAL ORIENTATION OF A 3% SILICON-IRON AFTER ROLLING AND ANNEALING
HO CHUNG-CHIH; CHANG HSIN-YU; CHOW TSUNG-CHUEN (Iron and Steel Research Institute; The Ministry of Metallurgical Industry)
Cite this article: 

HO CHUNG-CHIH; CHANG HSIN-YU; CHOW TSUNG-CHUEN (Iron and Steel Research Institute; The Ministry of Metallurgical Industry). THE MAGNETIC PROPERTIES AND THE DEGREE OF CRYSTAL ORIENTATION OF A 3% SILICON-IRON AFTER ROLLING AND ANNEALING. Acta Metall Sin, 1964, 7(2): 165-173.

Download:  PDF(963KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The magnetic properties and the degree of crystal orientation of a 3% silicon-iron have been investigated. The effects of rolling methods, the degree of cold deformation, and the intermediate and final annealing temperatures on the inhomogeneities in magnetic properties and the spread of preferred orientation have been considered.
Received:  18 February 1964     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1964/V7/I2/165

[1] Goss, N. P.: Trans. Am. Soc. Metals, 1935, 23, 511.
[2] Carpenter, V. W.: U. S. Patent, 1942, No. 2287466.
[3] #12
[4] Frey, A. A., Bitter, F.: U. S. Patent, 1938, No. 2112084.
[5] 勒斯曼G.:冶軋矽鋼片的热处理和性能,(冶金工业出版社,1959年),1頁.
[6] Morill, W.: Metal Progr., 1948, 54, 675.
[7] 米洛諾夫,冶軋矽鋼片的热处理和性能,(冶金工业出版社,1959年),48頁.
[8] Barrett, C. S.: Structure of Metals, (McGraw-Hill, 1953) , p. 485.
[9] 陈能寬、刘长祿:金属学报,1958,3,30.
[10] Wiener, G., Corcoran, R.: J. Metals, 1956, 8, 901.
[11] Dunn, C. G.: Acta Met., 1954, 2, 173.
[12] 张信鈺、孙学范:(110) [001] 取向多晶硅鋼片形变和再結晶織构,未发表.
[13]#12
[14] 鋼鉄研究院:矽鋼片,(冶金工业出版社,1959年),142-150頁.
[15] 格利高罗夫,勃洛欣,冶軋矽鋼片的热处理和性能,(冶金工业出版社,1959年),67頁.
[16] 潘孝順、王煥元:晶粒取向硅鋼片的試制,未发表.
[17] 特拉赫欽別尔格,热軋矽鋼片的热处理和性能,(冶金工业出版社,1959年),13頁,25頁.
[18] Fast, J. D.: Philips Res. Repts., 1956, 11, 490.
[19] May, J. E., Turnbull, D.: Trans. AIME, 1958, 212, 769.
[20] Fiedler, H. C.: Trans. AIME, 1961, 221, 1201.
[21] Markuszewicz, M. J.: J. Iron Steel Inst. (London), 1962, 200, 223.
No related articles found!
No Suggested Reading articles found!