THE EFFECT OF STRIP THICKNESS ON THE COLD-ROLLING AND RECRYSTALLIZATION TEXTURE OF ELECTROLYTIC COPPER
CHOU PANG-HSIN;YEN MING-KAO
Cite this article: 

CHOU PANG-HSIN;YEN MING-KAO. THE EFFECT OF STRIP THICKNESS ON THE COLD-ROLLING AND RECRYSTALLIZATION TEXTURE OF ELECTROLYTIC COPPER. Acta Metall Sin, 1963, 6(2): 163-175.

Download:  PDF(3922KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of thickness of specimen on the recrystallization texture of cold-rolledcopper strips under different percentage of reduction and with or without the surfacelayer has been investigated.The recrystallization texture of specimens of 0.84—0.02mmin thickness corresponding to a reduction of 88.7—99.7%,was found to have a nearlyperfect cubic texture.No concentrated cubic texture was observed in the specimens of0.01mm in thickness under a reduction of 99.8%.However,for specimens with cubi-cally aligned grains,cold-rolled to 0.01 mm in thickness(under a reduction of 98.6%),a rather concentrated cubic texture was developed after annealing at 900℃.The effect of strip thickness on the recrystallization texture has been found to bedifferent for different percentage of reduction.Under a smaller reduction of 88.7%,the specimens,less than 0.04mm in thickness,did not give a concentrated cubic texture.Whereas,for specimens under larger reduction(96—99.7%),no significant effect of stripthickness on the development of recrystallization texture was observed.The decreasing in thickness of specimens suppresses the occurrence of second re-crystallization but no pronounced effect on the grain orientation of the second recrystal-lization texture has been noticed.
Received:  18 February 1963     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1963/V6/I2/163

[1] Rostoker,W.,Spachner,S.:Trans.AIME,1955,203,921.
[2] #12
[3] Koh,P.K.(郭本坚):Trans.AIME,1961,221,50.
[4] 颜鸣皋、周邦新:物理学报,1958,14,121.
[5] Yen Ming-kao(颜鸣皋):Trans.AIME,1949,185,59.
[6] Baldwin,W.M.:Trans.AIME,1946,166,591.
[7] 颜鸣皋:“金属织构的测定”,全国第二次金属物理学术会议报告,1962年,11月,上海.
[8] 周邦新:“铁硅单晶体的冶轧及再结晶织构”,全国第二次金属物理学术会议报告,1962年,11月,上海.
[9] Duun,C.G.,Koh,P.K.(郭本坚):Trans.AIME,1958,212,80.
[10] 周邦新、王维敏、陈能宽:物理学报,1960,16,155.
[11] Burke,J.E.:Trans.AIME,1949,180,73.
[12] 陈能宽、周邦新、王维敏等,待发表.
[13] 周邦新、韩昌茂:“铁硅合金中立方织构的形成”,金属学会沈阳地区分会报告,1960年6月
No related articles found!
No Suggested Reading articles found!