ACTIVITY OF MnO IN LIQUID BLAST-FURNACE-TYPE SLAGS AND ITS RATE OF REDUCTION
WANG WEI-YUAN;CHOU YUAN-HSI Institute of Metallurgy;Academia Sinica
Cite this article: 

WANG WEI-YUAN;CHOU YUAN-HSI Institute of Metallurgy;Academia Sinica. ACTIVITY OF MnO IN LIQUID BLAST-FURNACE-TYPE SLAGS AND ITS RATE OF REDUCTION. Acta Metall Sin, 1963, 6(1): 40-50.

Download:  PDF(902KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The equilibrium represented by the reaction MnO(in slag)+C=Mn+COhas been investigated with a view to evaluating the activity of MnO in liquid blast-furnace-type slags.In two series of experiments,carbon-saturated iron and silver wereused respectively as the solvent metal.It has been shown that the use of silver insteadof the conventional iron as the metal phase has certain important advantages.Besides,some preliminary work has been done on the rate of reduction of MnO from liquid blast-furnace-type slags.The effect of various slag components on the activity of MnO has been explainedfrom the point of view of the ionic structure of slags.The mechanism of reduction ofMnO and the order of reaction are discussed on the basis of convectional diffusion.Thepractical application of the experimental data in blast-furnace operation is briefly dis-cussed.
Received:  18 January 1963     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1963/V6/I1/40

[1] Chou,Y.H.(邹元燨):Doctorate Thesis,Department of Metallurgy,Carnegie Institute of Technology,1947.
[2] Filer,E.W.,Darken,L.S.:Trans.AIME,1952,194,253.
[3] Stukel,J.E.,Cocubinsky,J.:J.Metals,1954,6,353.
[4] K(o|¨)rber,F.,Oelsen,W.:Mitt.K.W.Inst.Eisenf.,1932,14,181.
[5] 三本木贡治、大谷正康:铁(?)纲,1954,40,277。
[6] 王渭源、邹元燨:科学通报,1957,(9) ,287.
[7] Schenck,H.,Neumann,F.:Arch.Eisenhüttenw.,1958,263.
[8] Ohtani,M.:Sci.Rept.Res.Inst.Tohoku Univ.,1957,A9,426
[9] #12
[10] Chipman,J.,Fulton,J.C.,Caskey,G.R,:Acta Met.,1954,2,439.
[11] Chou,Y.H.(邹元燨):Freiberger Forschungsh.,1957,B15,18.
[12] Fulton,J.C.,Chipman,J.:Trans.AIME,1954. 200,1136.
[13] Schenck,H.,Neumann,F.:Arch.Eisenhüttenw.,1959,705;1960,83.
[14] Abraham,K.P.,Davis,M.W.,Richardson,F.D.:J.Iron Steel Inst.,1960,196,82.
[15] Chang,L.C.(张禄经),Goldman,K.M.:Trans.AIME,1948,176,309.
[16] McCoy,C.W.,Philbrook,W.O.:Trans.AIME,1958,212,226.
[17] Fulton,J.C.,Chipman,J.:The Physical Chemistry of Steelmaking,(Wiley,1958) ,p.113.
[18] #12
[19] Philbrook,W.O.,Kirkbride,L.D.:Trans.AIME,1956,206,351.
[20] Tarby,S.K.,Philbrook,W.O.:J.Metals,1961,13,442.
[21] 赵彭年、邹元燨:金属学报,1963,6,28。
[22] 邹元燨、赵彭年、曹兆民:待发表.
[23] Kozakevitch,P.:Rev.Met.,1954,51,559.
[24] Bockris,J.O'M.,Lowe,D.C.:Proc.Roy.Soc.,1954,A226,423.
[25] B(?)k,T.,(O|¨)lander,A.:Acta Chem.Scand.,1955,9,1350.
[26] #12
[27] Wagner,C.:The Physical Chemistry of Steelmaking,(Wiley,1958) ,p.237.
[28] 王渭源:待发表.
[29] 靳树梁等:现代炼铁学,(冶金工业出版社,1959年),273页.
[30] 邹元燨:金属学报,1956,1,325.x
No related articles found!
No Suggested Reading articles found!