A STATISTICAL INVESTIGATION OF FACTORS INFLUENCING FLOTATION OF WOLFRAMITE |
HU WEI-PEI;LOO TSU-HSI Midsouthern Institute of Mining and Metallurgy |
|
Cite this article:
HU WEI-PEI;LOO TSU-HSI Midsouthern Institute of Mining and Metallurgy. A STATISTICAL INVESTIGATION OF FACTORS INFLUENCING FLOTATION OF WOLFRAMITE. Acta Metall Sin, 1963, 6(1): 14-22.
|
Abstract An attempt was made to apply the method of statistical analysis to research in the flotation of wolframite.The statistically designed experiment studied the effects of six factors,i.e.,(A)grainsize,(B)mode of the generation of airbubbles,(C)pH value of the pulp,(D)acid treat-ment,(E)quantity of the frother used,and(F)temperature of the pulp.The analysis of variance showed that,in the case of wolframite flotation whensodium oleate was used as a collector,the grain size,pH value and temperature of thepulp are the significant variables.The analysis of the interactions between the variables led to best synthetic techno-logical conditions.
|
Received: 18 January 1963
|
[1] #12 [2] (a)胡为柏:国外钨锡选矿现状及动向,(冶金部矿冶研究院,1962年),32-38页.(b)胡为柏、卢祖禧:微细矿泥浮选的几个方向,(中南矿冶学院浮选教研室,1962年). [3] #12 [4] #12 [5] Schranz,H.:Z.Chemie Bergwesen,1961,21,(3) ,49-54. [6] #12 [7] 岩崎严:日本矿业会志,1961,9,639-645. [8] Bauer,E.L.:A Statistical Manual for Chemists,(Academic,1960) ,p.21-38. [9] Scheffé,H.:The Analysis of Variance,(Wiley,1959) ,p.68-79. [10] (a)Boyard,G.:Application du plan de travail factoriel á la recherche en flotation,Rev.Ind.Min.,1954,35,346-365,85,395-405. (b)Boyard,G.:Anwendung eines Faktoren-Arbeitesplanes bei untersuchungsarbeiten in der Aufbeveitung von Touissit,Z.Erzbergbau Metalluttenew.,1955,8,Beiheft,B 221.v |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|