BEHAVIOUR OF FLUORINE IN BLAST-FURNACE SMELTING Ⅴ. AN INVESTIGATION OF THE SLAG-FORMING PROCESSES IN A 11M~3 BLASTFURNACE SMELTING PAO-TOU IRON ORE
INSTITUTE OF METALLURGY AND CERAMICS; ACADEMIA SINICA
Cite this article: 

INSTITUTE OF METALLURGY AND CERAMICS; ACADEMIA SINICA. BEHAVIOUR OF FLUORINE IN BLAST-FURNACE SMELTING Ⅴ. AN INVESTIGATION OF THE SLAG-FORMING PROCESSES IN A 11M~3 BLASTFURNACE SMELTING PAO-TOU IRON ORE. Acta Metall Sin, 1959, 4(2): 107-113.

Download:  PDF(2470KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The results of investigation of the behaviour of fluorine in blast-furnace smelting have beenreported in a series of previous papers. The purpose of the present research is to investigatethe slag-forming processes in a 11 M~3 blast-furnace smelting Pao-Tou iron ore. Petrographical examinations supplemented by White test studies show that the chief mineralconstituents present in the primary slag are calcium oxide, fluorite and wustite. From a comparison of the slag-forming processes in a 11 M~3 blast-furnace smelting Pao-Touiron ore with that smelting an ordinary acid ore, a new mechanism for the formation of theprimary slag in smelting the former ore has been proposed. In addition, it has been found thatthe plastic region in smelting Pao-Tou iron ore is smaller than that in the usual case, thereby,considerably facilitating the driving of the blast-furnace by improving the penetrability of thecharge column.
Received:  18 February 1959     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1959/V4/I2/107

[1] И. П. Бардин, А. В. Руднева, Л. М. Цылев: № 4 (1952) .
[2] И. П. Бардин, А. В. Руднева, Л. М. Цылев: № 5 (1955) .
[3] Л. м. Цылев: (1953) .
[4] А. В. Руднева: (1953) .
[5] T. L. Ho: Note on Some Rare Earth Minerals from Beiyin Obo, Suiyuan. Bull. Geol. Soc. of China. 114, 219 (1935) .
[4] 周仁、邹元燨等,氟在高炉冶炼中的行为Ⅲ.氟在1W~3实验高炉冶炼包头铁矿过程中的变化,金属学报,4(1) ,(1959) .
[7] 中国科学院冶金陶瓷研究所,氟在高炉冶炼中的行为Ⅳ.氟在11M~3高炉冶炼包头铁矿过程中的变化及其挥发机理,金属学报,4(2) ,(1959) .
[8] 11M~3高炉冶炼庞家堡矿中的成渣过程,中国科学院冶金陶瓷研究所,内部资料(1958) .
[9] Oesare Brisi: Role of Cuspidine 3CaO·2SiO_2·CaF_2 in the System CaF_2-SiO_2-CaO. Jour. Cerm. Soc., 40, 174 (1957)
No related articles found!
No Suggested Reading articles found!