Please wait a minute...
Acta Metall Sin  1959, Vol. 4 Issue (1): 75-80    DOI:
Current Issue | Archive | Adv Search |
DETERMINATION OF BORON IN STEEL AND IRON BY THE ALUMINUM SPARK METHOD
WANG HONG-JANG Institute of Metal Research; Anademia Sinica
Cite this article: 

WANG HONG-JANG Institute of Metal Research; Anademia Sinica. DETERMINATION OF BORON IN STEEL AND IRON BY THE ALUMINUM SPARK METHOD. Acta Metall Sin, 1959, 4(1): 75-80.

Download:  PDF(489KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Determination of boron in steel and iron by the aluminum spark method possesses highersensitivity and precision. It is not necessary to separate iron from the sample. The sample isdissolved with perchloric acid, and into the perchlorate solution is added a certain amount ofNaOH solution. The standards are prepared from synthetic solutions with different proportionsof boric acid added. Electrodes are made from pure aluminum 8 mm in diameter and 5-10 cm in length. Theends of the electrodes should be machined flat and the sharp edges should be removed by light cham-fering to reduce the tendency of sparks to strike these sharp edges. Drops of solutions are placed onthe surface of the electrode by means of a micropipet calibrated to deliver 0.05 ml. With a con-trol spark source and medium spectrograph we can analyze boron in the range from 0.005% to1.0% by the line B 2496.778A.
Received:  18 January 1959     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1959/V4/I1/75

[1] E. F. Runge, L. S. Brooks and F. R. Bryan., Anal chem, 27, 1543, (1955) .
[2] Soichiro Musha., Science Repts. Research Insts., Tohoku Univ. Ser. A. 2, 437, (1950) .
[3] 曹思启.,钢铁工厂实验室,8, 22,(1957) .
[4] B. I. S. R. A., J. Iron Steel, Inst. 189, 227, (1958) .
[5] 村木勇夫,日色和夫.,化学译报,4,407,(1958) .
[6] Everett C. Cogbill and John H. Yoe., Anal Chem, 29, 1251, (1957) .
[7] W. G. Kirchgessner and N. A. Finkelstein., Anal Chem, 25, 1024, (1953) .
[8] Ralph H. Steinberg., Applied Spectroscopy, 7, 176, (1953) .
[9] О. В. Фалькова., ДАН, 48, 189. (1945) .
[10] Naoichi Ota., Japan. Analyst, 2, 205, (1953) .
[11] Fred M., J. O. S. A. 37, 279, (1947) .
[12] Norman H. Nachtrieb: Principles and Practice of Spectrochemical Analysis. 261~277, (1950) ."
No related articles found!
No Suggested Reading articles found!