LAMINATION DEFECTS IN RIMMING STEEL SLABS
SHAO HSIANG-HUA Anshan Iron and Steel Corporation
Cite this article: 

SHAO HSIANG-HUA Anshan Iron and Steel Corporation. LAMINATION DEFECTS IN RIMMING STEEL SLABS. Acta Metall Sin, 1959, 4(1): 16-21.

Download:  PDF(1248KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An extraordinarily large gas pocket formed during the rolling of a rimming steel slab wasstudied. Results of investigation indicated that the serious lamination defects that often occurredin such slabs were due to the presence in large rimming steel ingots of central cavities that (1) con-tained gases at high pressure, (2) were surrounded by heavily segregated metal, and (3) wereloaded at their surfaces with non-metallic substances. During the rolling operation these cavitiesfailed to weld up. On the contrary, the solid walls dividing neighbouring cavities were pushedopen and, as a result, a large discontinuity remained in the rolled slab. It was found that aftershearing the slab and thus exposing the discontinuity to atmosphere, in most cases such discon-tinuities could weld up during subsequent rolling into plates. Lower tapping temperature and lower pouring temperature (speed) were found effective tolessen lamination rejects.
Received:  18 January 1959     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1959/V4/I1/16

[1] 56的附钢锭模设计使用总结,鞍钢中央试验室资料,1957年.
[2] S. Marshall, J. Chipman, Trans. ASM, 1942, Vol. 30, No.3, P. 695.
[3] H. Schenck, Physikalische Chemie der Eisenhuttenprozesse, Julius Springer, Berlin, 1934, Band II, S. 246.
[4] Г. Н. Ойкс, 1955, 191.
[5] K. C. McCutcheon, J. Chipman, Trans. AIME, 1938, Vol. 131, Iron and Steel Division, pp. 206--226.
[6] А. М. Самарир, 1953, 94.
[7] 二炼钢沸腾钢3气囊缺陷第二次生产试验小结,鞍钢中央试验室资料,1957年.(
No related articles found!
No Suggested Reading articles found!