PROPERTIES OF IRON-GRAPHITE POROUS BEARINGS
HUANG YUNG-SHU AND WU TZU-LIANG Institute of Metallurgy and Ceramics;Academia Sinica
Cite this article: 

HUANG YUNG-SHU AND WU TZU-LIANG Institute of Metallurgy and Ceramics;Academia Sinica. PROPERTIES OF IRON-GRAPHITE POROUS BEARINGS. Acta Metall Sin, 1958, 3(4): 300-305.

Download:  PDF(1314KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The antiseizure property of the iron-graphite porous bearings can be improved by using purer grades of iron powder.A grade of iron powder of>98% Fe,processed by the reduction of rimmedsteel mill scale with charcoal,is found to be suitable for this purpose.Bearings made of a coarsegrade iron powder(~80%>0.06mm)and containing~1.5% graphite give a good combinationof mechanical strength and antifriction properties.When the graphite content is lower than 0.5%,excessive free ferrite in the matrix results seizure between the rubbings surfaces.On the other hand,with the graphite content in excess of 3.0%,voluminous free carbide in the matrix induces heavymechanical wear.In comparison with the bronze-graphite porous bearings of the same hardness,an iron-graphite porous bearing possesses a higher strength,a larger oil content,a smaller coefficientof friction and less wear loss.
Received:  18 April 1958     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1958/V3/I4/300

[1] 吴自良等,青铜-石墨含油轴承的压制及烧结,金属研究工作报告会会刊,第三卷(1954) 151。
[2] #12
[3] #12
[4] #12
[5] 卢肇基、沈邦儒、金大康、吴自良:(a)氧化铁还原的速率,金属学报,第3卷第2期(1958. 6. )111。(b)用木炭还原法从沸腾钢铁鳞制取铁粉(已送钢铁杂志发表)。
No related articles found!
No Suggested Reading articles found!