Please wait a minute...
Acta Metall Sin  1958, Vol. 3 Issue (3): 181-196    DOI:
Current Issue | Archive | Adv Search |
BEHAVIOUR OF FLUORINE IN BLAST-FURNACE SMELTING Ⅱ.SMELTING PAO-TOU IRON ORE IN AN EXPERIMENTAL BLAST-FURNACE
CHOW JEN;CHOU YUAN-HSI;SUN TSUNG-LI;HSU YUAN-SUN;CHOW SHENG-HSIANG;WANG WEI-YUAN;MOW PEI-KEN;PENG HSUI-WU;TSUNG CHIA-TING Institute of Metallurgy and Ceramics;Academia Sinica
Cite this article: 

CHOW JEN;CHOU YUAN-HSI;SUN TSUNG-LI;HSU YUAN-SUN;CHOW SHENG-HSIANG;WANG WEI-YUAN;MOW PEI-KEN;PENG HSUI-WU;TSUNG CHIA-TING Institute of Metallurgy and Ceramics;Academia Sinica. BEHAVIOUR OF FLUORINE IN BLAST-FURNACE SMELTING Ⅱ.SMELTING PAO-TOU IRON ORE IN AN EXPERIMENTAL BLAST-FURNACE. Acta Metall Sin, 1958, 3(3): 181-196.

Download:  PDF(1505KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  For the investigation of a series of problems in connection with the behaviour of fluorine inblast-furnace smelting,an experimental blast-furnace of an effective volume of about 1 m~3 wasbuilt at our Institute by November 1955 together with the necessary auxiliary equipment.Pao-Tou iron ore,which contains fluorite as one of its chief gangues,was smelted in our experimentalblast-furnace with and without previous sintering,and the planned experiments were completed intwo campaigns which lasted for 22 and 36 days respectively.The smelting characteristics ofour experimental blast-furnace are herewith reported together with data on material balance of allthe constituents including fluorine.It was found that nearly all the fluorine went into the slag,while the fluorine content of tht blast-furnace gas was exceedingly low despite the rather highpercentage of fluorite in the charge.
Received:  18 March 1958     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1958/V3/I3/181

[1] 周仁等,金属学报,3(1) ,15(1958) .
[2] #12
[3] 杨行简等,未发表资料,包头钢铁公司(1954) .
[4] H.L.Saunders,G.B.Butler and J.M.Tweedy,J.Iron Steel Inst.,163,173(1949) .
[5] 金森九郎等,日本东京大学生产技术研究所报告,4(4) ,(1955) .
[6] #12Y
No related articles found!
No Suggested Reading articles found!