    					| THE LOSS OF NON-METALLIC INCLUSIONS IN STEEL DURING ELECTROLYTIC SEPARATION | 
  					 
  					  										
						| SHIH CHANG-HSU;LEE TAI-CHUNG;CHAO SHU-HSI Institute of Metal Research; Academia Sinica | 
					 
															
						 | 
					 
				 
				
				Cite this article: 
				
					
			      SHIH CHANG-HSU;LEE TAI-CHUNG;CHAO SHU-HSI Institute of Metal Research; Academia Sinica. THE LOSS OF NON-METALLIC INCLUSIONS IN STEEL DURING ELECTROLYTIC SEPARATION. Acta Metall Sin, 1957, 2(3): 297-300.	
				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									               
																												  