Please wait a minute...
Acta Metall Sin  1956, Vol. 1 Issue (4): 337-421    DOI:
Current Issue | Archive | Adv Search |
THE DECOMPOSITION OF δ-FERRITE IN A Cr-Ni-Mo-Ti STAINLESS STEEL
CHUANG YU-CHIH AND LIU CHIA-LO Institute of Metal Research;Academia Sinica
Cite this article: 

CHUANG YU-CHIH AND LIU CHIA-LO Institute of Metal Research;Academia Sinica. THE DECOMPOSITION OF δ-FERRITE IN A Cr-Ni-Mo-Ti STAINLESS STEEL. Acta Metall Sin, 1956, 1(4): 337-421.

Download:  PDF(6166KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The decomposition of δ-ferrite at 750°,850° and 950℃ in quenched 18/8/3/1Cr-Ni-Mo-Ti stainless steel specimens has been studied microscopically,thetransformation products being electrolytically extracted and identified by X-raydiffraction method.At early stages of decomposition accicular austenite forms along certaincrystallographic planes of δ-ferrite.As a result,the remaining ferrite becomesenriched in Cr,Mo and impoverished in C,Ni,Mn,and was found to transformsubsequently to sigma which begins after heating for 5-6 minutes at 850℃.Precipitation of titanium carbide first occurs in the ferrite grains,later itmakes appearance along the ferrite-austenite interphase boundaries and along thetwinning planes within the austenite grain.The precipitation of titanium carbideseems to have no appreciable effect on the sequence of decomposition of δ-ferrite.The impact value of the steel was found to decrease very markedly before thecommencement of the δ→σ transformation and it is considered that this mightbe associated with the titanium carbide precipitation.
Received:  18 April 1956     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1956/V1/I4/337

[1] Gilman,J.J.,Koh,P.K.and Zmeskal,O.,Trans.Amer.Soc.Metals,41(1949) ,1371.
[2] Kirkby,H.W.and Morley,J.I.,J.Iron Steel Institute,158(1948) ,289.
[3] Smith,L.and Bowen,K.W.J.,J.Iron Steel Institute,148(1948) ,295.
[4] Hoar,T.P.and Bowen,K.W.J.,Trans.Amer.Soc.Metals,45(1953) ,443.
[5] Bindari,A.E.,Kow,P.K.and Zmeskal,O.,Trans.Amer.Soc.Metals,43(1951) ,226.
[6] #12
[7] Shirley,H.T.,J.Iron Steel Institute,174(1953) ,242.
[8] 庄育智、李有柯,物理学报,10卷,4期(1954) ,321.
[9] Kuo,K.(郭可信),J.Iron Steel Institute,181(1955) ,213.
[10] Franks,R.,Binder,W.O.and Bishop,C.R.,Trans.Amer.Soc.Metals,29(1941) ,33.
[11] #12
[12] Dulis,E.J.and Smith,G.V.,Symposium on the Nature,Occurrence,and Effects of Sigma Phase(Amer.Soc.for Testing Materials,Philadelphia,1951) ,3.
[13] Barrett,C.S.,Structure of Metals(McGraw-Hill London,1953) ,249.
[14] Barnett,W.I.and Troiano,A.R.,Metal Progress,53(1948) .
[15] Vacher,H.C.and Bechtoldt,C.J.,J.Res.Nat.Bur.Stand.53(1954) ,67.