| AN INVESTIGATION OF CHEMICAL EQUILIBRIA IN THE BLAST-FURNACE HEARTH Ⅰ.THE MANGANESE-SULFUR EQUILIBRIUM |
| CHOU YUAN-HSI Institute of Metallurgy and Ceramics;Academia Sinica |
|
Cite this article:
CHOU YUAN-HSI Institute of Metallurgy and Ceramics;Academia Sinica. AN INVESTIGATION OF CHEMICAL EQUILIBRIA IN THE BLAST-FURNACE HEARTH Ⅰ.THE MANGANESE-SULFUR EQUILIBRIUM. Acta Metall Sin, 1956, 1(4): 325-335.
|
|
|
Abstract This paper presents an analysis of slag-metal data of 122 tests collected fromthree blast-furnace plants in China by plotting[Mn][S]against(MnO)(S).Itis shown that the manganese-sulfur equilibrium is approached in the blast-furnacehearth in agreement with the conclusions of some recent publications.The threesets of data may be represented by straight lines of different slopes obtained bythe least square method.The manganese-sulfur equilibrium constant is shown to be related to theactivities of CaO,MnO and CaS.By using the activity values derived previouslyby the author,some preliminary results have been obtained concerning the effectof basicity and(S)on the manganese-sulfur equilibrium.The temperature-depen-dence of the manganese-sulfur equilibrium constant has been recalculated fromFiler and Darken's data on the distribution of manganese and sulfur betweenblast-furnace metal and slags.The blast-furnace practice of the three different plants is discussed in the lightof the present calculations.
|
|
Received: 18 April 1956
|
[1] Oelsen,W.und Maetz,H.,Stahl und Eisen,69,147(1949) . [2] Weilandt,B.,Maetz,H.und Oelsen,W.,Arch.Eisenhüttenwesen,23,163(1952) . [3] Grant,N.J.,Dowding,J.W.and Murphy,R.J.,Trans.Am.Min.Met.Engrs.,197,1451(1953) . [4] Turkdogan,E.T.,J.Iron and Steel Inst.,179,147(1955) . [5] Filer,E.W.and Darken,L.S.,Trans.Am.Inst.Min.Met.Engrs.,194,253(1952) . [6] 邹元爔,金属学报,1(2) ,127(1956) . [7] 邹元爔,金属学报,1(2) ,143(1956) . [8] 邹元爔,金属学报,1(3) ,233(1956) . [9] Rosenqvist,T.,Trans.Am.Inst.Min.Met.Engrs.,191,535(1951) . [10] Basic Open Hearth Steelmaking,Am.Inst.Min.Met.Engrs.,New York(1951) . [11] Osborn,E.F.,DeVries,R.C.,Gee,K.H.,Kraner,H.M.,Trans.Amer.Inst.Min.Met.Engrs.,200,33(1954) . [12]#12 [13] 李薰.陈(?)志,李捷报,严铄,徐曾基,吴汶海,金属学报,1(1) ,15(1956) . |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|