Abstract It was found that the addition of a minute amount of boron(0.0005-0.005%)as an alloying element can greatly increase the hardenability of steel.So it wasrecognised that boron can be used as a substitute for the more expensive alloyingelements such as nickel,chromium and molybdenum,and greatly lowering the costof steel production.The aim of this investigation was to find a substitute for steel 18 ХΓТ,in orderto save the expenditure of the alloying element chromium.By comparison of hardenability properties and core properties of the carburizedboron steel and the carburized 18 ХΓТ,a carburizing grade boron steel was finallychosen,which contained less than 0.30% chromium,0.30% nickel and 0.15%molybdenum.The boron hardenability factor decreases with increase of carbon content;itwas found in the present investigation that a linear relationship exists betweencarbon content and boron hardenability factor,expressed asF_B=1+1.88(0.97-C%).In order to obtain the best properties of the carburized boron steel,the maxi-mum carbon content of the carburized surface should be maintained below 1%.
|
|
Received: 18 March 1956
|
[1] 李薰,对冶金科学长远计划以及建立我国合金钢系统的一些初步意见,科学通报,12(1955) ,第46页. [2] Grange,R.A.and Garvey,T.M.,Factors Affecting the Hardenability of Boron Treated Steels,Trans.ASM,37(1946) ,p.136. [3] Rahrer,C.D.and Armstrong,C.D.,Effect of C-content on Hardenability of Boron Steels,Trans.ASM,40(1948) ,p.1099. [4] Jatczak,C.F.,and Rowland,E.S.,The Influence of Boron on Case Hardenability in Alloy Carburizing Steels,Trans.ASM,45(1953) ,p.771. [5] Grange,R.A.and Mitchell,J.B.,Effect of Carbon and Boron on the Hardenability of a Casecarburized Steel,Trans.ASM,46(1954) ,p.446. [6] Gurry,R.W.,The Relative Deoxidizing Power of Boron in Liquid Steel and the Elimination of Boron in the Open-hearth Process,Metal Technology,Dec.1943. [7] Speight,G.E.,Addition of Boron to Steel by Reduction from Oxide.J.I.S.I.,171(1952) . [8] Asimow,M.,Graig,W.F.and Grossmann,M.A.,Correlation between the Jominy Test and Quenched round Bars.,Journal SAE,49 No.1 July 1941,p.283. [9] Grossmann,M.A.,Hardenability Calculated from Chemical Composition,Metals Technology,June,1942. [10] Grossmann,M.A.,Elements of Hardenability,ASM,1952. [11] #12 [12] #1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|