| BATH REACTIONS OF ELECTRIC-FURNACE STEELMAKING WITH OXYGEN INJECTION |
| FANG BING;WANG CHING-TANG;HOO CHWANG-CHI;LIU CHENG-CHI AND HSING CHUNG-SHU Institute of Metal Research;Academia Sinica |
|
Cite this article:
FANG BING;WANG CHING-TANG;HOO CHWANG-CHI;LIU CHENG-CHI AND HSING CHUNG-SHU Institute of Metal Research;Academia Sinica. BATH REACTIONS OF ELECTRIC-FURNACE STEELMAKING WITH OXYGEN INJECTION. Acta Metall Sin, 1956, 1(3): 243-254.
|
|
|
Abstract Bath reactions during the oxidizing period of electric-furnace steelmaking withinjection were studied. It is found that,under favourable conditions,a rate of carbon removal ofabout 0.015—0.020%C per minute(that of the normal smelting with ore beingaround 0.005% C per minute only)may be obtained;(FeO)and[O]decreasesignificantly and approach to equilibrium with[C]during the oxidizing period,andthe decrement of[O]increases proportionately with the increase of the rate ofcarbon removal.Dephosphorization during the oxidizing period is found to be rather ineffective,the average[P]removed amounts to about 0.004% only.With a supplementaryoperation of dephosphorization during the melting period,[P]can be reduced toless than 0.015% at the end of oxidizing period.However,the dephosphorizationmechanism in the case of the oxygen smelting is still not yet clear.
|
|
Received: 18 March 1956
|
[1] #12 [2] #12 [3] #12 [4] #12 [5] Schenk,H.,Physical Chemistry of Steel-making(English edition),1945,148. [6] #12 [7] 高桥俊雄,铁与钢,昭和28年(1953) 2月,97. [8] 同文献[4] ,512-513. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|