A RESEARCH ON THE WORKABILITY OF CAST IRON WITH SPHEROIDAL GRAPHITE
CHANG TSO-MEI;SH(U
Cite this article: 

CHANG TSO-MEI;SH(U. A RESEARCH ON THE WORKABILITY OF CAST IRON WITH SPHEROIDAL GRAPHITE. Acta Metall Sin, 1956, 1(2): 165-188.

Download:  PDF(2361KB) 
Export:  BibTeX | EndNote (RIS)      
Received:  18 February 1956     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1956/V1/I2/165

[1] #12
[2] #12
[3] #12
[4] #12
[5] Cook,M.& Davis,D.,The Hot-working of Copper and Copper Alloys,Symposium on Hotworking,The Institute of Metals,pp,108-114,London,1951.
[6] #12
[7] 张作梅、郭胜泉,球墨铸铁的锻造、压延和机械性能的研究,机械工程学报,3(1) ,45-74(1955) .
[8] 张作梅、徐有容,在不同温度下球墨铸铁的冲击性能,物理学报,10(4) ,333-345(1954) .
[9] 中国科学院金属研究所,球墨铸铁锻压初步试验总结报告,铸工,6(1953) ,5-15页.
[10] Siebel,E.und Pomp,A.,Die Ermittlung der Form(a|¨)inderungs Festigkeit von Metallen durch den Stauchversuch,Mitt.aus.d.k.w.Inst.F.Eisenforsch,Di(u|¨)sseldorf,9(1927) ,p.157.
[11] Manjoine,M.J.and Nadai,A.,High Speed Tension Tests at Elevated Temperatures,part I,Proc.A.S.T.M.,40(1940) ,pp.822-837.
[12] Nadai,A.and Manjoine,M.J.,High Speed Tension Tests at Elevated Temperatures,parts II and III,Jour.Applied Mechanics,No.6,1941,pp.77-91.
No related articles found!
No Suggested Reading articles found!