含硅的低合金超高强度贝氏体钢的晶粒细化与冲击能提高
高宽; 王六定; 朱明; 陈景东; 施易军; 陈国栋
Refinement of Grain and Enhancement of Impact Energy Absorption for Low-Alloy Ultra-High Strength Bainite Steels Containing Silicon
金属学报 . 2007, (3): 315 -320 .