高容量镁基储氢合金材料研究与应用进展
邹建新, 张嘉祺, 赵颖燕, 林羲, 丁文江
Progress in the Research and Application of High-Capacity Mg-Based Hydrogen Storage Alloy Materials
ZOU Jianxin, ZHANG Jiaqi, ZHAO Yingyan, LIN Xi, DING Wenjiang
金属学报
.
2025, (3): 420
-436
.
DOI: 10.11900/0412.1961.2024.00344