基于晶体塑性的6XXX铝合金力学性能多尺度计算
郑潇禹, 陈辛, 何美玲, 黄奇, 李亚, 孔毅, 杜勇
Multi-Scale Simulation of Mechanical Properties of 6XXX Aluminum Alloy Based on Crystal Plasticity
ZHENG Xiaoyu, CHEN Xin, HE Meiling, HUANG Qi, LI Ya, KONG Yi, DU Yong
金属学报 . 2025, (11): 1758 -1768 .  DOI: 10.11900/0412.1961.2024.00083