间隙元素O对 β 型Ti-15Mo合金超低温力学性能的影响
戴进财, 闵小华, 辛社伟, 刘凤金
Effect of Interstitial Element O on Cryogenic Mechanical Properties in β-Type Ti-15Mo Alloy
DAI Jincai, MIN Xiaohua, XIN Shewei, LIU Fengjin
金属学报
.
2025, (2): 243
-252
.
DOI: 10.11900/0412.1961.2023.00268