研究论文

冷丝辅助旋转/摇动电弧窄间隙MAG焊缝成形特性及接头组织性能演变机制

  • 李红 ,
  • 姜玉清 ,
  • 曹玉鹏 ,
  • 王加友 ,
  • 刘澍彬
展开
  • 1 江苏科技大学 材料科学与工程学院 镇江 212100
    2 沙洲职业工学院 智能制造学院 张家港 215699
李 红,女,1984年生,博士生
第一联系人:姜玉清(共同第一作者),男,1992年生,博士
王加友,jywang@just.edu.cn,主要从事高效电弧焊接技术及装备研究
刘澍彬,shubin_l18@just.edu.cn,主要从事高效焊接工艺及接头组织性能研究

收稿日期: 2025-08-13

  修回日期: 2025-09-28

  网络出版日期: 2026-01-06

基金资助

国家自然科学基金项目(52275340);国家自然科学基金项目(51875268)

Weld Formation Characteristics and the Evolution Mechanisms of Joint Microstructure and Mechanical Properties for Rotating/Swing Arc Narrow Gap MAG Welding Assisted by Cold Wire

  • LI Hong ,
  • JIANG Yuqing ,
  • CAO Yupeng ,
  • WANG Jiayou ,
  • LIU Shubin
Expand
  • 1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212100, China
    2 School of Intelligent Manufacturing, Shazhou Professional Institute of Technology, Zhangjiagang 215699, China

Received date: 2025-08-13

  Revised date: 2025-09-28

  Online published: 2026-01-06

Supported by

National Natural Science Foundation of China(52275340)

摘要

为解决深坡口焊接中坡口间隙对冷丝摆幅限制的问题,并通过优化窄间隙焊接工艺改善接头组织和性能,提高实用性,本工作提出了可变幅摆动冷丝辅助的旋转/摇动电弧窄间隙熔化极活性气体保护焊接方法,研究了电弧旋转频率、冷丝送进速率以及冷丝与摇动电弧的横向摆动协同率(η)对焊缝成形和焊接效率的影响规律,阐明了窄间隙焊接接头组织和力学性能的演变机制。结果表明,在小摆幅(η ≤ 0.5)冷丝辅助下,旋转/摇动电弧焊缝成形稳定,焊接效率可分别提高25.7%和44.2%;与旋转电弧焊相比,摇动电弧对熔池后方无重复加热作用,缩窄粗晶热影响区,冷丝吸热作用可进一步加快熔池冷却,显著细化焊缝晶粒、韧化粗晶热影响区,在相应的组织类型和晶粒尺寸因素主导下,焊缝强度可增大6.0%、熔合线区冲击功可显著提高53.8%,协同提升了窄间隙焊接效率和性能,从而促进高质高效窄间隙焊接工艺的应用。

本文引用格式

李红 , 姜玉清 , 曹玉鹏 , 王加友 , 刘澍彬 . 冷丝辅助旋转/摇动电弧窄间隙MAG焊缝成形特性及接头组织性能演变机制[J]. 金属学报, 2026 , 62(1) : 235 -252 . DOI: 10.11900/0412.1961.2025.00231

Abstract

Narrow gap gas metal arc welding (GMAW) is increasingly applied in the manufacturing of thick-walled structures, such as large ships, offshore equipment, and pressure pipelines. Previous research focused on the improving weld formation and welding efficiency in this process but seldom addressed the correlations among the welding process, joint microstructure, and mechanical properties. The study aims to modify the microstructure and properties of the joint while overcoming the limitations of groove gap on cold wire swaying amplitude in deep-groove welding, thereby enhancing the practicality of the process. A rotating/swing arc narrow gap metal active gas welding assisted by a cold wire with variable swaying amplitude is proposed. Effects of arc rotation frequency, cold wire feeding speed, and the horizontal oscillation cooperative rate between the cold wire and the swing arc (η) on weld formation and welding efficiency are then investigated. Additionally, the evolution mechanisms of the microstructure and mechanical properties of cold wire-assisted rotating/swing arc narrow gap welding joints are clarified. Experimental results show that the cold wire-assisted rotating/swing arc processes yield stable weld formation and increase the welding efficiency by 25.7% and 44.2% at η ≤ 0.5, respectively. Compared to the rotating arc process, the swing arc process achieves greater penetrations into the groove sidewalls and weld bottom even at smaller swaying amplitudes of the cold wire; the swing arc has no the reheating effect on the rear of the molten pool, thereby narrowing the coarse-grain heat-affected zone (CGHAZ). This nonreheating effect, combined with the heat absorption effect of the cold wire, accelerates the molten pool cooling, substantially refining the weld grain size and toughening the CGHAZ. Owing to the dominant factors of the microstructure type and grain size, impact energy near the fusion line increases by 53.8% while weld strength rises by 6.0%. Consequently, the two cold wire-assisted processes concurrently improve welding efficiency and joint performance, advancing the application of high-quality, high-efficiency methods in narrow gap welding.

参考文献

[1] Zhang F J, Guo J L, Zhang G D. Comparison of technical and economic characteristics of common arc welding process for heavy plate [J]. Electr. Weld. Mach., 2017, 47(5): 144
  张富巨, 郭嘉琳, 张国栋. 厚板常用弧焊工艺的技术和经济特性比较 [J]. 电焊机, 2017, 47(5): 144
[2] Wu Y J, Wang J Y, Xu G X, et al. Numerical analysis of residual stress in swing-arc narrow-gap gas metal arc welding [J]. Materials, 2025, 18: 803
[3] Liu H S, Xue R L, Zhou J P, et al. Implementation of a two-stage algorithm for NG-GMAW seam tracking and oscillation width adaptation in pipeline welding [J]. Sci. Technol. Weld. Joinning, 2023, 28: 992
[4] Teng B, Fan C L, Xu K, et al. Research status and application progress of narrow gap welding technology for thick plates [J]. Trans. China Weld. Inst., 2024, 45(1): 116
  滕 彬, 范成磊, 徐 锴 等. 厚板窄间隙焊接技术研究现状与应用进展 [J]. 焊接学报, 2024, 45(1): 116
[5] Xu W H, Yang Q F, Xiao Y F. Research status of sidewall fusion control technology in narrow gap welding [J]. J. Netshape Form. Eng., 2020, 12(4): 47
  徐望辉, 杨清福, 肖逸峰. 窄间隙焊接侧壁熔合控制技术的研究现状 [J]. 精密成形工程, 2020, 12(4): 47
[6] Kang Y H, Na S J. Characteristics of welding and arc signal in narrow groove gas metal arc welding using electromagnetic arc oscillation [J]. Weld. J., 2003, 82: 93
[7] Wang J Y, Zhu J, Fu P, et al. A swing arc system for narrow gap GMA welding [J]. ISIJ Int., 2012, 52: 110
[8] Li W H, He C F, Chang J S, et al. Modeling of weld formation in variable groove narrow gap welding by rotating GMAW [J]. J. Manuf. Process., 2020, 57: 163
[9] Murayama M, Oazamoto D, Ooe K. Narrow gap gas metal arc (GMA) welding technologies [J]. JFE Technol. Rep., 2015, 20: 147
[10] Cheng Y X, Jiang X X, Gou N N, et al. Research status of ultra-narrow gap arc welding with flux band confinement [J]. Electr. Weld. Mach., 2025, 1-11 [2025-11-10].
  程雨潇,蒋小霞,苟宁年,等.焊剂带约束电弧超窄间隙焊接研究现状[J/OL].电焊机, 2025, 1-11 [2025-11-10].
[11] Sugitani Y, Kobayashi Y, Murayama M. Development and application of automatic high speed rotation arc welding [J]. Weld. Int., 1991, 5: 577
[12] Wang J Y, Ren Y S, Yang F, et al. Novel rotation arc system for narrow gap MAG welding [J]. Sci. Technol. Weld. Joinning, 2007, 12: 505
[13] Yang C L, Guo N, Lin S B, et al. Application of rotating arc system to horizontal narrow gap welding [J]. Sci. Technol. Weld. Joinning, 2009, 14: 172
[14] Guo N, Lin S B, Gao C, et al. Study on elimination of interlayer defects in horizontal joints made by rotating arc narrow gap welding [J]. Sci. Technol. Weld. Joinning, 2009, 14: 584
[15] Costa J F M, Filho W A S, Jorge J C F, et al. Investigation on the ASTM A516 Grade 70 narrow gap welded joints obtained by the GMAW process with rotating electrode [J]. Int. J. Adv. Manuf. Technol., 2024, 134: 3452
[16] Wang J Y, Zhu J, Zhang C, et al. Effect of arc swing parameters on narrow gap vertical GMA weld formation [J]. ISIJ Int., 2016, 56: 844
[17] Cui H C, Jiang Z D, Tang X H, et al. Research on narrow-gap GMAW with swing arc system in horizontal position [J]. Int. J. Adv. Manuf. Technol., 2014, 74: 297
[18] Bao Y, Xue R L, Zhou J P, et al. The influence of oscillation parameters on the formation of overhead welding seams in the narrow-gap GMAW process [J]. Appl. Sci., 2023, 13: 5519
[19] Xu W H, Lin S B, Fan C L, et al. Prediction and optimization of weld bead geometry in oscillating arc narrow gap all-position GMA welding [J]. Int. J. Adv. Manuf. Technol., 2015, 79: 183
[20] Yang Z D, Chen Y T, Zhang Z W, et al. Research on the sidewall penetration mechanisms of cable-type welding wire narrow gap GMAW process [J]. Int. J. Adv. Manuf. Technol., 2022, 120: 2443
[21] Fang C F, Chen Z W, Xu G X, et al. Study on the process of CTWW CO2 gas shielded welding [J]. Acta Metall. Sin., 2012, 48: 1299
  方臣富, 陈志伟, 胥国祥 等. 缆式焊丝CO2气体保护焊工艺研究 [J]. 金属学报, 2012, 48: 1299
[22] Zhu Z Y, Wang J Y, Liu S B, et al. Thick-wire swing arc narrow gap GMA welding assisted by pre-embedding cold wires [J]. Int. J. Adv. Manuf. Technol., 2024, 131: 301
[23] Cai X Y, Lin S B, Fan C L, et al. Molten pool behaviour and weld forming mechanism of tandem narrow gap vertical GMAW [J]. Sci. Technol. Weld. Joinning, 2016, 21: 124
[24] Fang D S, Liu L M. Analysis of process parameter effects during narrow-gap triple-wire gas indirect arc welding [J]. Int. J. Adv. Manuf. Technol., 2017, 88: 2717
[25] Marques L F N, Santos E B F, Gerlich A P, et al. Fatigue life assessment of weld joints manufactured by GMAW and CW-GMAW processes [J]. Sci. Technol. Weld. Joinning, 2017, 22: 87
[26] Wang C, Wang J, Bento J, et al. A novel cold wire gas metal arc (CW-GMA) process for high productivity additive manufacturing [J]. Addit. Manuf., 2023, 73: 103681
[27] Ribeiro R A, Assun??o P D C, Dos Santos E B F, et al. Application of cold wire gas metal arc welding for narrow gap welding (NGW) of high strength low alloy steel [J]. Materials, 2019, 12: 335
[28] Suwannatee N, Yamamoto M. Single-pass process of square butt joints without edge preparation using hot-wire gas metal arc welding [J]. Metals, 2023, 13: 1014
[29] Jiang Y Q, Li H, Zhu J, et al. A swing arc narrow gap gas metal arc welding process assisted by direct-current hot wire [J]. Sci. Technol. Weld. Joinning, 2025, 30: 231
[30] Wang J Y, Jiang Y Q, Zhu J, et al. Development of swing arc narrow gap GMAW process assisted by swaying wire [J]. J. Mater. Process. Technol., 2023, 318: 118004
[31] Li Y, Jiang P, Li Y T, et al. Microstructure evolution and mechanical properties in the depth direction of ultra-high power laser-arc hybrid weld joint of 316L stainless steel [J]. Opt. Laser Technol., 2023, 160: 109093
[32] Zhang M, Jia F, Cheng K K, et al. Influence of quenching and tempering on microstructure and properties of welded joints of G520 martensitic steel [J]. Acta Metall. Sin., 2019, 55: 1379
  张 敏, 贾 芳, 程康康 等. 调质处理对G520钢焊接接头组织及性能的影响 [J]. 金属学报, 2019, 55: 1379
[33] Kang Y, Park G, Jeong S, et al. Correlation between microstructure and low-temperature impact toughness of simulated reheated zones in the multi-pass weld metal of high-strength steel [J]. Metall. Mater. Trans., 2018, 49A: 177
[34] Xie X, Wan Y B, Zhong M, et al. Optimizing microstructures and mechanical properties of electro-gas welded metals for EH36 shipbuilding steel treated by CaF2-TiO2 fluxes [J]. Acta Metall. Sin., 2025, 61: 998
  谢 旭, 万一博, 钟 明 等. CaF2-TiO2焊剂作用下EH36船板钢气电立焊焊缝金属组织优化及力学性能调控 [J]. 金属学报, 2025, 61: 998
[35] Jiao J J, Cao R, Li Y M, et al. Effect of post-welding heat treatment on impact toughness of Q690 high strength steel welded metal [J]. Mater. Rep., 2025, 39: 24010076
  焦继军, 曹 睿, 李义民 等. 焊后热处理对Q690高强钢焊缝金属冲击韧性的影响 [J]. 材料导报, 2025, 39: 24010076
文章导航

/