铝合金搅拌摩擦焊热-力-流耦合仿真及材料迁移轨迹解析
收稿日期: 2025-08-20
修回日期: 2025-09-22
网络出版日期: 2025-11-05
基金资助
国家自然科学基金项目(52175334);清洁高效透平动力装备全国重点实验室课题项目(DEC8300CG202428557A-1228215)
Coupled Thermal-Mechanical-Fluid Simulation and Material Migration Trajectory Analysis for Friction Stir Welding of Aluminum Alloy
Received date: 2025-08-20
Revised date: 2025-09-22
Online published: 2025-11-05
Supported by
National Natural Science Foundation of China(52175334);State Key Laboratory of Clean and Efficient Turbomachinery Power Equipment Project(DEC8300CG202428557A-1228215)
搅拌摩擦焊(FSW)过程中,材料在数秒时间内迅速完成材料流动-沉积过程。为解析材料流经搅拌头附近的完整轨迹,本工作以2219-T87铝合金FSW过程为研究对象,构建了FSW过程热-力-流全耦合仿真模型,并运用轨迹追踪算法,着重分析了FSW过程中材料流动-沉积的轨迹。结果表明,焊接过程中材料流动-沉积行为受其所处位置影响:靠近轴肩的材料流经搅拌头附近的轨迹呈多圈绕流模式,材料在流动过程中,绕行半径由大变小,并在搅拌针附近发生显著的向下迁移,沉积位置均位于前进侧;远离轴肩的材料呈现出直通流动模式,材料未完成整圈流动后便沉积在搅拌针后方,前进侧材料焊后沉积在前进侧,后退侧材料焊后沉积在后退侧。
韩鸿华 , 史清宇 , 杨诚乐 , 孔德帅 , 陈高强 . 铝合金搅拌摩擦焊热-力-流耦合仿真及材料迁移轨迹解析[J]. 金属学报, 2026 , 62(1) : 148 -158 . DOI: 10.11900/0412.1961.2025.00240
Although friction stir welding (FSW) is widely employed in aerospace and other engineering fields owing to its ability to produce high-quality joints and low residual stresses, the understanding of its physical mechanisms remains limited by the intense material flow during welding, which lags behind engineering practice. This gap motivates researchers to develop thermo-mechanical coupling models to elucidate the underlying physics, aiming to expand its application boundaries. During FSW, the material undergoes a highly rapid flow-deposition process that is completed within a few seconds. In this study, we present a fully coupled thermo-mechanical-fluid model for friction-stir-welded 2219-T87 aluminum alloy to demonstrate the complete material transport path in the vicinity of the tool. A particle-tracking algorithm was employed to quantitatively analyze the flow and subsequent refilling trajectory of the tracer material. The predicted temperature history and flow-zone geometry showed close agreement with experimental data. At the axis Z = 7 mm, the peak downward vertical velocity of the material reached 16.57 mm/s at the advancing side of the pin, whereas the peak upward vertical velocity reached 10.47 mm/s at the retreating side. The analysis revealed that the flow-deposition behavior of the material was highly position dependent. The material adjacent to the shoulder followed a multi-loop spiral trajectory around the tool, during which the loop radius gradually decreased and the material migrated markedly downward in the vicinity of the pin. Ultimately, all deposits accumulated on the advancing side. In contrast, the material far from the shoulder exhibited a through-flow pattern, depositing behind the pin without completing a full revolution. Post-weld deposits originating from the advancing side remained on the advancing side, whereas those from the retreating side settled on the retreating side.
Key words: friction stir welding; aluminum alloy; material flow; numerical simulation
| [1] | Schmidt H, Hattel J, Wert J. An analytical model for the heat generation in friction stir welding [J]. Modell. Simul. Mater. Sci. Eng., 2004, 12: 143 |
| [2] | Colligan K J, Mishra R S. A conceptual model for the process variables related to heat generation in friction stir welding of aluminum [J]. Scr. Mater., 2008, 58: 327 |
| [3] | Chen G Q, Shi Q Y, Li Y J, et al. Computational fluid dynamics studies on heat generation during friction stir welding of aluminum alloy [J]. Comput. Mater. Sci., 2013, 79: 540 |
| [4] | Su H, Wu C S, Pittner A, et al. Thermal energy generation and distribution in friction stir welding of aluminum alloys [J]. Energy, 2014, 77: 720 |
| [5] | Fratini L, Buffa G, Palmeri D, et al. Material flow in FSW of AA7075-T6 butt joints: Continuous dynamic recrystallization phenomena [J]. J. Eng. Mater. Technol., 2006, 128: 428 |
| [6] | Nie L, Wu Y X, Gong H. Prediction of temperature and residual stress distributions in friction stir welding of aluminum alloy [J]. Int. J. Adv. Manuf. Technol., 2020, 106: 3301 |
| [7] | Heidarzadeh A, Mironov S, Kaibyshev R, et al. Friction stir welding/processing of metals and alloys: A comprehensive review on microstructural evolution [J]. Prog. Mater. Sci., 2021, 117: 100752 |
| [8] | Wu C S, Su H, Shi L. Numerical simulation of heat generation, heat transfer and material flow in friction stir welding [J]. Acta Metall. Sin., 2018, 54: 265 |
| 武传松, 宿 浩, 石 磊. 搅拌摩擦焊接产热传热过程与材料流动的数值模拟 [J]. 金属学报, 2018, 54: 265 | |
| [9] | Schmidt H N B, Dickerson T L, Hattel J H. Material flow in butt friction stir welds in AA2024-T3 [J]. Acta Mater., 2006, 54: 1199 |
| [10] | Morisada Y, Imaizumi T, Fujii H, et al. Three-dimensional visualization of material flow during friction stir welding of steel and aluminum [J]. J. Mater. Eng. Perform., 2014, 23: 4143 |
| [11] | Morisada Y, Imaizumi T, Fujii H. Determination of strain rate in Friction Stir Welding by three-dimensional visualization of material flow using X-ray radiography [J]. Scr. Mater., 2015, 106: 57 |
| [12] | Huang Y X, Wang Y B, Wan D, et al. Material-flow behavior during friction-stir welding of 6082-T6 aluminum alloy [J]. Int. J. Adv. Manuf. Technol., 2016, 87: 1115 |
| [13] | Zeng X H, Xue P, Wang L, et al. Material flow and void defect formation in friction stir welding of aluminium alloys [J]. Sci. Technol. Weld. Joining, 2018, 23: 677 |
| [14] | Chen S J, Han Y, Jiang X Q, et al. Study on in-situ material flow behaviour during friction stir welding via a novel material tracing technology [J]. J. Mater. Process. Technol., 2021, 297: 117205 |
| [15] | Kumar R, Lal A K, Bharti R P, et al. Experimental and computational analyses of material flow characteristics in friction stir welding [J]. Int. J. Adv. Manuf. Technol., 2021, 115: 3011 |
| [16] | Colegrove P A, Shercliff H R. 3-dimensional CFD modelling of flow round a threaded friction stir welding tool profile [J]. J. Mater. Process. Technol., 2005, 169: 320 |
| [17] | Bastier A, Maitournam M H, Dang Van K, et al. Steady state thermomechanical modelling of friction stir welding [J]. Sci. Technol. Weld. Joining, 2006, 11: 278 |
| [18] | Liechty B C, Webb B W. Modeling the frictional boundary condition in friction stir welding [J]. Int. J. Mach. Tools Manuf., 2008, 48: 1474 |
| [19] | Atharifar H, Lin D C, Kovacevic R. Numerical and experimental investigations on the loads carried by the tool during friction stir welding [J]. J. Mater. Eng. Perform., 2009, 18: 339 |
| [20] | Yu Z Z, Zhang W, Choo H, et al. Transient heat and material flow modeling of friction stir processing of magnesium alloy using threaded tool [J]. Metall. Mater. Trans., 2012, 43A: 724 |
| [21] | Chen G Q, Feng Z L, Zhu Y C, et al. An alternative frictional boundary condition for computational fluid dynamics simulation of friction stir welding [J]. J. Mater. Eng. Perform., 2016, 25: 4016 |
| [22] | Yang C L, Chen G Q, Qiao J N, et al. Material flow during dissimilar friction stir welding of Al/Mg alloys [J]. Int. J. Mech. Sci., 2024, 272: 109173 |
| [23] | Tamadon A, Pons D J, Chakradhar K, et al. 3D-printed tool shoulder design for the analogue modelling of bobbin friction stir weld joint quality [J]. Adv. Mater. Sci., 2021, 21: 27 |
| [24] | Schneider J A, Nunes Jr A C. Characterization of plastic flow and resulting microtextures in a friction stir weld [J]. Metall. Mater. Trans., 2004, 35B: 777 |
| [25] | Liu F C, Hovanski Y, Miles M P, et al. A review of friction stir welding of steels: Tool, material flow, microstructure, and properties [J]. J. Mater. Sci. Technol., 2018, 34: 39 |
| [26] | Liu X C, Sun Y F, Nagira T, et al. Experimental evaluation of strain and strain rate during rapid cooling friction stir welding of pure copper [J]. Sci. Technol. Weld. Joining, 2019, 24: 352 |
| [27] | Wu C S, Wang T, Su H. Material flow velocity, strain and strain rate in ultrasonic vibration enhanced friction stir welding of dissimilar Al/Mg alloys [J]. J. Manuf. Process., 2022, 75: 13 |
| [28] | Qiao J N, Shi Q Y, Chen S J, et al. Modeling and simulation of interface friction and material flow behavior during friction stir welding [J]. Electr. Weld. Mach., 2023, 53(3): 15 |
| 乔俊楠, 史清宇, 陈树君 等. 搅拌摩擦焊界面摩擦及材料流动行为仿真 [J]. 电焊机, 2023, 53(3): 15 | |
| [29] | Zhen Y Q, Liu X C, Shen Z K, et al. State-of-art of experimental characterization of material flow in friction stir welding [J]. J. Mech. Eng., 2020, 56(6): 184 |
| 甄云乾, 刘小超, 申志康 等. 搅拌摩擦焊材料流动的试验表征研究现状 [J]. 机械工程学报, 2020, 56(6): 184 | |
| [30] | Wang X, Gao Y F, Liu X, et al. Tool-workpiece stick-slip conditions and their effects on torque and heat generation rate in the friction stir welding [J]. Acta Mater., 2021, 213: 116969 |
| [31] | Yang C L, Dai Q L, Shi Q Y, et al. Flow-coupled thermo-mechanical analysis of frictional behaviors at the tool-workpiece interface during friction stir welding [J]. J. Manuf. Process., 2022, 79: 394 |
| [32] | Xue W, Xiao L Y, Tao T, et al. A novel method of lateral tool-tilt for optimizing material flow and temperature distribution in friction stir welding [J]. Mater. Today Commun., 2024, 40: 109962 |
| [33] | Qiao J N, Shi Q Y, Wu C S, et al. Elucidation of solid-state metal flow behaviors during friction stir welding: Numerical and experimental investigation [J]. Phys. Fluids, 2023, 35: 123105 |
| [34] | Yu M, Li W Y, Li J L, et al. Modelling of entire friction stir welding process by explicit finite element method [J]. Mater. Sci. Technol., 2012, 28: 812 |
| [35] | Sahu M, Paul A, Ganguly S. Influence of frictional heat spread pattern on the formation of intermetallic layers at the dissimilar FSW joint interface between AA 5083 and HSLA steel [J]. J. Manuf. Process., 2022, 83: 555 |
| [36] | Xu W F, Liu J H, Zhu H Q. Numerical simulation of thermal field of friction stir welded 2219 aluminum alloy thick plate [J]. Trans. China Weld. Inst., 2010, 31(2): 63 |
| 徐韦锋, 刘金合, 朱宏强. 2219铝合金厚板搅拌摩擦焊接温度场数值模拟 [J]. 焊接学报, 2010, 31(2): 63 | |
| [37] | Wan S Q, Wu Y X, Gong H, et al. Thermal mechanical coupling simulation of temperature and residual stress in friction stir welding of 2219 aluminum alloy [J]. Hot Work. Technol., 2019, 48(13): 159 |
| 万胜强, 吴运新, 龚 海 等. 2219铝合金搅拌摩擦焊温度与残余应力热力耦合模拟 [J]. 热加工工艺, 2019, 48(13): 159 | |
| [38] | Ke L M, Pan J L, Xing L, et al. Sucking-extruding theory for the material flow in friction stir welds [J]. J. Mech. Eng., 2009, 45(4): 89 |
| 柯黎明, 潘际銮, 邢 丽 等. 搅拌摩擦焊焊缝金属塑性流动的抽吸-挤压理论 [J]. 机械工程学报, 2009, 45(4): 89 | |
| [39] | He C S, Qie M F, Zhang Z Q, et al. Effect of axial ultrasonic vibration on metal flow behavior during friction stir welding [J]. Acta Metall. Sin., 2021, 57: 1614 |
| 何长树, 郄默繁, 张志强 等. 轴向超声振动对搅拌摩擦焊过程中金属流动行为的影响 [J]. 金属学报, 2021, 57: 1614 | |
| [40] | Jain R, Pal S K, Singh S B. A study on the variation of forces and temperature in a friction stir welding process: A finite element approach [J]. J. Manuf. Process., 2016, 23: 278 |
| [41] | Ou L, Sun B, Wang Z. Flow stress of 2219 aluminium alloy during hot compression deformation [J]. Hot Work. Technol., 2008, 37(2): 42 |
| 欧 玲, 孙 斌, 王 智. 2219铝合金热压缩变形流变应力 [J]. 热加工工艺, 2008, 37(2): 42 | |
| [42] | Wang Z T, Tian R Z. Handbook of Aluminum and Aluminum Alloys [M]. 2nd Ed., Changsha: Central South University Press, 2000: 188 |
| 王祝堂, 田荣璋. 铝合金及其加工手册 [M]. 第2版. 长沙: 中南大学出版社, 2000: 188 | |
| [43] | Davis J R. Aluminum and Aluminum Alloys [M]. Materials Park: ASM International, 1993: 68 |
| [44] | Colegrove P A, Shercliff H R. CFD modelling of friction stir welding of thick plate 7449 aluminium alloy [J]. Sci. Technol. Weld. Joining, 2006, 11: 429 |
| [45] | Su H, Wu C S, Bachmann M, et al. Numerical modeling for the effect of pin profiles on thermal and material flow characteristics in friction stir welding [J]. Mater. Des., 2015, 77: 114 |
| [46] | Chen G Q, Wang G Q, Shi Q Y, et al. Three-dimensional thermal-mechanical analysis of retractable pin tool friction stir welding process [J]. J. Manuf. Process., 2019, 41: 1 |
| [47] | Chen G Q, Liu X, Qiao J N, et al. Improved analytical model for thermal softening in aluminum alloys form room temperature to solidus [J]. Materials, 2023, 16: 7358 |
/
| 〈 |
|
〉 |