表层多孔Ti6Al4V/TiC梯度材料的构筑、组织和性能
收稿日期: 2025-02-27
修回日期: 2025-07-05
网络出版日期: 2025-07-16
基金资助
河南省重点研发专项项目(241111231300)
Construction, Microstructure, and Properties of Ti6Al4V/TiC Functionally Graded Material with Porous Surface
Received date: 2025-02-27
Revised date: 2025-07-05
Online published: 2025-07-16
Supported by
Key Research and Development Project of Henan Province(241111231300)
均质钛基复合材料因组织和性能单一而导致抗冲击性能不足,本工作旨在构筑一种兼具表层多孔和功能梯度特征的高吸能、高抗冲击钛基复合材料。通过ZrO2空心球占位法和热压烧结法制备了含表层多孔钛层和五个梯度层的Ti6Al4V/TiC梯度材料,多孔钛层孔隙率为40%,梯度层致密度不低于98.8%,梯度层由底层向多孔钛方向,TiC加入量0~8%递增,TiC粒径由3~5 μm增加至15~53 μm。研究了表层多孔Ti6Al4V/TiC梯度材料的显微组织和性能,结果表明,相邻梯度层的连接形式为冶金结合,基体由层片状α-Ti相和β-Ti相构成,TiC颗粒主要分布在原始β-Ti晶界位置,强化机制为细晶强化、位错强化和弥散强化;与Ti6Al4V层相比,加入TiC颗粒后,原始β-Ti晶粒及其内部的α-Ti相、β-Ti相得到明显细化,加入尺寸为15~53 μm、含量为8%的TiC颗粒后,该梯度层材料硬度最高;加入尺寸为3~5 μm、含量为4%和6%的TiC颗粒后,两个梯度层材料的抗拉强度和韧性均提升,其中前者韧性最好,后者抗拉强度最高;在压缩实验过程中,表面多孔钛层能在较低压缩载荷下持续坍塌变形,具有显著的吸能特性。表层多孔Ti6Al4V/TiC梯度材料通过高吸能表层多孔钛的削弱冲击作用、高硬度迎弹面的抗穿透作用和高强高韧背弹面的抗冲击作用,来实现防护性能提升。
邵星海 , 王文焱 , 谢敬佩 , 秦文栋 , 王爱琴 , 马窦琴 , 毛志平 , 柳培 , 郭清远 . 表层多孔Ti6Al4V/TiC梯度材料的构筑、组织和性能[J]. 金属学报, 2026 , 62(4) : 636 -648 . DOI: 10.11900/0412.1961.2025.00058
Homogeneous titanium matrix composites (TMCs), despite their unique microstructure and properties, often exhibit inadequate impact resistance. To overcome this limitation, this study presents a high-energy-absorbing and impact-resistant TMC by incorporating a dual design strategy: a porous surface layer and a functionally graded internal structure. A Ti6Al4V/TiC graded material, consisting of one porous titanium surface layer and five gradient layers, was fabricated using the ZrO2 hollow sphere placeholder method combined with hot pressing sintering. The porous titanium layer exhibited a porosity of 40%, while each of the five gradient layers achieved a relative density of 98.8%. Moving from the bottom layer towards the porous surface, the TiC content was systematically increased from 0 to 8%, and the TiC particle size was enlarged from 3-5 μm to 15-53 μm. The microstructure and properties of the fabricated material were comprehensively characterized. The gradient layers were metallurgically bonded, ensuring structural integrity. The matrix microstructure comprised lamellar α-Ti and β-Ti phases, with TiC particles predominantly distributed along prior β-Ti grain boundaries. The identified strengthening mechanisms included grain refinement, dislocation strengthening, and dispersion strengthening. Compared with the monolithic Ti6Al4V layer, the incorporation of TiC particles effectively refined the prior β-Ti grains along with the α-Ti and β-Ti phases. The gradient layer containing 8%TiC particles (15-53 μm) achieved the highest hardness. In contrast, the layers containing 4% and 6%TiC particles (3-5 μm) demonstrated enhanced tensile strength and toughness. Notably, the layer with 4%TiC showed superior toughness, while the layer with 6%TiC achieved the maximum tensile strength. Compression tests revealed that the porous titanium surface layer possessed remarkable energy absorption capacity, undergoing progressive collapse deformation under relatively low compressive loads before reaching densification. The Ti6Al4V/TiC functionally graded material with a porous surface effectively enhanced protective performance through a synergistic mechanism: the highly energy-absorbing porous surface mitigated initial impact forces, the high-hardness impact-facing layers provided superior penetration resistance, and the high-strength, high-toughness backing layers contributed to excellent residual load-bearing capacity and overall impact resistance.
| [1] | Hayat D M, Singh H, He Z, et al. Titanium metal matrix composites: An overview [J]. Composites, 2019, 121A: 418 |
| [2] | Zhao Y H, Jing J H, Chen L W, et al. Current research status of interface of ceramic-metal laminated composite material for armor protection [J]. Acta Metall. Sin., 2021, 57: 1107 |
| 赵宇宏, 景舰辉, 陈利文 等. 装甲防护陶瓷-金属叠层复合材料界面研究进展 [J]. 金属学报, 2021, 57: 1107 | |
| [3] | Xia X C, Zhang E K, Ding J, et al. Research progress on laser cladding of refractory high-entropy alloy coatings [J]. Acta Metall. Sin., 2025, 61: 59 |
| 夏兴川, 张恩宽, 丁 俭 等. 激光熔覆难熔高熵合金涂层研究进展 [J]. 金属学报, 2025, 61: 59 | |
| [4] | Dong L L, Wang Y M, Cui W F, et al. Research progress on interface structure and performance optimization of carbonaceous nanomaterial reinforced titanium matrix composites [J]. Mater. China, 2023, 42: 942 |
| 董龙龙, 王圆梦, 崔文芳 等. 纳米碳强化钛基复合材料界面结构与性能优化研究进展 [J]. 中国材料进展, 2023, 42: 942 | |
| [5] | Ghazlan A, Ngo T, Tan P, et al. Inspiration from Nature's body armours—A review of biological and bioinspired composites [J]. Composites, 2021, 205B: 108513 |
| [6] | Zhang C, Cao J W, Guo J B, et al. The research on transparent armor material technology [J]. J. Phys.: Conf. Ser., 2020, 1507: 102014 |
| [7] | Savio S G, Madhu V, Gogia A K. Ballistic performance of alumina and zirconia-toughened alumina against 7.62 armour piercing projectile [J]. Def. Sci. J., 2014, 64: 477 |
| [8] | B?rvik T, Langseth M, Hopperstad O S, et al. Perforation of 12 mm thick steel plates by 20 mm diameter projectiles with flat, hemispherical and conical noses: Part I: experimental study [J]. Int. J. Impact Eng., 2002, 27: 19 |
| [9] | Hazell P J, Fellows N A, Hetherington J G, et al. A note on the behind armour effects from perforated alumina/aluminium targets [J]. Int. J. Impact Eng., 1998, 21: 589 |
| [10] | Tan C W, Su J H, Liu Y F, et al. Enhanced interfacial bonding strength of laser bonded titanium alloy/CFRTP joint via hydrogen bonds interaction [J]. Composites, 2022, 239B: 109966 |
| [11] | Gupta N, Basu B, Prasad V, et al. Ballistic studies on TiB2-Ti functionally graded armor ceramics [J]. Def. Sci. J., 2012, 62: 382 |
| [12] | Shojaei P, Trabia M, O'Toole B, et al. Enhancing hypervelocity impact resistance of titanium substrate using Ti/SiC metal matrix nanocomposite coating [J]. Composites, 2020, 194B: 108068 |
| [13] | Medvedovski E. Ballistic performance of armour ceramics: Influence of design and structure. Part 2 [J]. Ceram. Int., 2010, 36: 2117 |
| [14] | Prestat M, Thierry D. Corrosion of titanium under simulated inflammation conditions: Clinical context and in vitro investigations [J]. Acta Biomater., 2021, 136: 72 |
| [15] | Wang W R, Xie H F, Xie L, et al. Anti-penetration performance of high entropy alloy-ceramic gradient composites [J]. Int. J. Min. Met. Mater., 2018, 25: 1320 |
| [16] | Wang J X, Yang J J, Liu K, et al. Study on damage characteristics of metal sandwich plate under combined actions of shock wave and randomly distributed fragments [J]. Shipbuild. China, 2023, 64(6): 60 |
| 王加夏, 杨俊杰, 刘 昆 等. 冲击波与随机分布破片联合作用下金属夹层板损伤特性研究 [J]. 中国造船, 2023, 64(6): 60 | |
| [17] | Hao F, Xin S W, Mao Y C, et al. Review on application of titanium alloy in armor [J]. Mater. Rep., 2020, 34(suppl.1): 293 |
| 郝 芳, 辛社伟, 毛友川 等. 钛合金在装甲领域的应用综述 [J]. 材料导报, 2020, 34(): 293 | |
| [18] | Zhang J B. Analysis of armor titanium alloy technology for new generation ground combat platforms [J]. Tank Armoured Vehicle, 2023, (21): 42 |
| 张久宝. 新一代地面作战平台装甲钛合金技术探析 [J]. 坦克装甲车辆, 2023, (21): 42 | |
| [19] | Zhang L H, Gour G, Petrinic N, et al. Rate dependent behaviour and dynamic strain localisation of three novel impact resilient titanium alloys: Experiments and modelling [J]. Mater. Sci. Eng., 2020, A771: 138552 |
| [20] | Banerjee D, Williams J C. Perspectives on titanium science and technology [J]. Acta Mater., 2013, 61: 844 |
| [21] | Liu X, Zhou Y, Zhu X J, et al. The failure mechanism at adiabatic shear bands of titanium alloy: High-precision survey using precession electron diffraction and geometrically necessary dislocation density calculation [J]. Mater. Sci. Eng., 2019, A746: 322 |
| [22] | Zhang R, Han B, Lu T J. Confinement effects on compressive and ballistic performance of ceramics: A review [J]. Int. Mater. Rev., 2021, 66: 287 |
| [23] | Zhang C J, Kong F T, Xiao S L, et al. Evolution of microstructure and tensile properties of in situ titanium matrix composites with volume fraction of (TiB + TiC) reinforcements [J]. Mater. Sci. Eng., 2012, A548: 152 |
| [24] | Ji W M, Zhou R H, Vivegananthan P, et al. Recent progress in gradient-structured metals and alloys [J]. Prog. Mater. Sci., 2023, 140: 101194 |
| [25] | Mehara M, Goswami C, Kumar S R, et al. Performance evaluation of advanced armor materials [J]. Mater. Today: Proc., 2021, 47: 6039 |
| [26] | Yang Q Q, Shao X H, Liu Y, et al. Preparation and analysis of ceramic hollow spheres/titanium alloy composite foam materials [J]. Foundry, 2020, 69: 115 |
| 杨倩倩, 邵星海, 刘 源 等. 陶瓷空心球/钛合金复合泡沫材料的制备与分析 [J]. 铸造, 2020, 69: 115 | |
| [27] | Wang Y Q, Liu P S, Hou H L, et al. Pore structure and mechanical properties of titanium foam [J]. Rare Met. Mater. Eng., 2017, 46(suppl.1): 134 |
| 王耀奇, 刘培生, 侯红亮 等. 泡沫钛孔隙结构及力学性能 [J]. 稀有金属材料与工程, 2017, 46(): 134 |
/
| 〈 |
|
〉 |