集成电路芯片锡基微凸点电迁移:从物理本质到可靠性提升
收稿日期: 2024-08-20
修回日期: 2025-03-05
网络出版日期: 2025-03-17
基金资助
国家自然科学基金项目(52350321);国家自然科学基金项目(U1837208);中国博士后科学基金项目(2024M750313)
Electromigration of Sn-Based Microbumps in Chip Interconnections of Integrated Circuits: From Physical Nature to Reliability Improvement
Received date: 2024-08-20
Revised date: 2025-03-05
Online published: 2025-03-17
Supported by
National Natural Science Foundation of China(52350321);National Natural Science Foundation of China(U1837208);China Postdoctoral Science Foundation(2024M750313)
随着先进封装技术向微型化、高性能方向发展,集成电路芯片锡基微凸点的直径持续减小至微米尺度,通过单个凸点的电流密度随直径减小呈平方增加,其电迁移行为与机理研究对集成电路芯片互连可靠性评估与设计具有重要价值。本文归纳分析了芯片互连微凸点(焊点)电迁移现象的物理本质、主要影响因素和研究方法;系统综述了微焊点固-固电迁移过程中的极性效应、反极性效应和两相分离等电迁移行为特征与液-固电迁移过程中原子迁移、相析出和相溶解等电迁移行为特征;梳理评价了电迁移寿命的评估模型及修正模型;最后阐明了微焊点电迁移可靠性提升的方法,并展望了集成电路芯片互连锡基微凸点电迁移未来的研究方向和可靠性分析方法。
黄明亮 , 王胜博 , 尤海潮 , 刘厚麟 , 任婧 , 黄斐斐 . 集成电路芯片锡基微凸点电迁移:从物理本质到可靠性提升[J]. 金属学报, 2025 , 61(7) : 979 -997 . DOI: 10.11900/0412.1961.2024.00290
With advancements in miniaturization and performance in advanced packaging technology, the diameter of Sn-based microbumps continues to shrink to the micrometer scale. Consequently, the current density passing through each solder bump increases exponentially as the radius reduces. This emphasizes the critical need to understand the behaviors and mechanisms of electromigration (EM) for the reliability evaluation and design of chip interconnects in integrated circuits. This study systematically summarizes and analyzes the physical nature, key influencing factors and research methods related to the electromigration of Sn-based microbumps. The EM characteristics during the solid-solid EM, including the polarity effect, reverse polarity effect and two-phase separation are reviewed. Similarly, the EM behaviors during the liquid-solid EM, including atomic migration, phase segregation, and phase dissolution, are systematically reviewed. The EM lifetime assessment models and their modifications are evaluated. Furthermore, this study summarizes methods to improve the EM reliability of Sn-based microbumps and outlines prospective research directions and analytical approaches to further improve their reliability in advanced electronic applications.
| 1 | Gerardin M. De l'action de la pile sur les sels de potasse st de soude st sur les alliages soumis à la fusion ingée [J]. Comptes Rendus, 1861, 53: 727 |
| 2 | Blech I A, Meieran E S. Direct transmission electron microscope observation of electrotransport in aluminum thin films [J]. Appl. Phys. Lett., 1967, 11: 263 |
| 3 | Clement J J, Thompson C V. Modeling electromigration-induced stress evolution in confined metal lines [J]. J. Appl. Phys., 1995, 78: 900 |
| 4 | Brandenburg S, Yeh S. Electromigration studies of flip chip bump solder joints [A]. Surface Mount International Conference and Exposition [C]. San Jose, CA: SMTA, 1998: 337 |
| 5 | Tu K N. Recent advances on electromigration in very-large-scale-integration of interconnects [J]. J. Appl. Phys., 2003, 94: 5451 |
| 6 | Tammaro M. Investigation of the temperature dependence in Black's equation using microscopic electromigration modeling [J]. J. Appl. Phys., 1999, 86: 3612 |
| 7 | Yang D S, Huang Y L. Interfacial intermetallic compound modification to extend the electromigration lifetime of copper pillar joints [J]. Front. Mater., 2023, 9: 1080848 |
| 8 | Li X M, Liu Z H, Li C, et al. Effects of trace elements Ag, Bi and Ni on solid-liquid electromigration interface diffusion in solder joints [J]. J. Electron. Mater., 2021, 50: 5312 |
| 9 | Liu Y, Xu X, Xue Y X, et al. An in-situ experimental and simulation study on the electromigration behavior of SAC305 solder joints [J]. J. Adhes. Sci. Technol., 2024, 38: 3348 |
| 10 | Ye S, Huang M L, Chen L D, et al. Failure mechanisms of Ni/Sn-3.0Ag-0.5Cu/OSP flip chip solder under high current stressing [A]. 12th International Conference on Electronic Packaging Technology and High Density Packaging [C]. Shanghai: IEEE, 2011: 1 |
| 11 | Chen L D, Huang M L. Effect of electromigration on intermetallic compound formation in Cu/Sn/Cu interconnect [A]. 2009 International Conference on Electronic Packaging Technology & High Density Packaging [C]. Beijing: IEEE, 2009: 666 |
| 12 | Wang F J, Liu L T, Li D Y, et al. Electromigration behaviors in Sn-58Bi solder joints under different current densities and temperatures [J]. J. Mater. Sci.: Mater. Electron., 2018, 29: 21157 |
| 13 | Huang M L, Zhang Z J, Zhao N, et al. In situ study on reverse polarity effect in Cu/Sn-9Zn/Ni interconnect undergoing liquid-solid electromigration [J]. J. Alloys Compd., 2015, 619: 667 |
| 14 | Huang M L, Zhang Z J, Zhao N, et al. A synchrotron radiation real-time in situ imaging study on the reverse polarity effect in Cu/Sn-9Zn/Cu interconnect during liquid-solid electromigration [J]. Scr. Mater., 2013, 68: 853 |
| 15 | Huang M L, Zhang Z J, Zhao N, et al. Study on liquid-solid electromigration in Cu/Sn-9Zn/Cu interconnect using synchrotron radiation real-time in situ imaging technology [A]. 14th International Conference on Electronic Packaging Technology [C]. Dalian: IEEE, 2013: 126 |
| 16 | Huang M L, Zhou Q, Zhao N, et al. Reverse polarity effect and cross-solder interaction in Cu/Sn-9Zn/Ni interconnect during liquid-solid electromigration [J]. J. Mater. Sci., 2014, 49: 1755 |
| 17 | Huang M L, Feng X F, Zhao J F, et al. Cu-Ni cross-solder interaction in Cu/Sn-58Bi/Ni interconnect undergoing liquid-solid electromigration [J]. Chin. J. Nonferrous Met., 2015, 25: 967 |
| 黄明亮, 冯晓飞, 赵建飞 等. Cu/Sn-58Bi/Ni焊点液-固电迁移下Cu和Ni的交互作用 [J]. 中国有色金属学报, 2015, 25: 967 | |
| 18 | Zhang Z J, Huang M L. Abnormal migration behavior and segregation mechanism of Bi atoms undergoing liquid-solid electromigration [J]. J. Mater. Sci., 2019, 54: 7975 |
| 19 | Zhang Z J, Huang M L. In situ observation of electromigration-induced anomalous precipitation of Ag3Sn phase in Ag-containing solder joints [J]. J. Electron. Mater., 2021, 50: 2111 |
| 20 | Chen L D, Huang M L, Zhou S M. Effect of electromigration on intermetallic compound formation in line-type Cu/Sn/Cu and Cu/Sn/Ni interconnects [A]. 2010 Proceedings 60th Electronic Components and Technology Conference (ECTC) [C]. Las Vegas: IEEE, 2010: 176 |
| 21 | Zhang Z J. Liquid-solid electromigration behavior and mechanism of micro interconnect [D]. Dalian: Dalian University of Technology, 2016 |
| 张志杰. 微互连焊点液-固电迁移行为与机理研究 [D]. 大连: 大连理工大学, 2016 | |
| 22 | Huang M L, Zhao J F, Zhang Z J, et al. Role of diffusion anisotropy in β-Sn in microstructural evolution of Sn-3.0Ag-0.5Cu flip chip bumps undergoing electromigration [J]. Acta Mater., 2015, 100: 98 |
| 23 | Huang M L, Sun H Y. Interaction between β-Sn grain orientation and electromigration behavior in flip-chip lead-free solder bumps [J]. Acta Metall. Sin., 2018, 54: 1077 |
| 黄明亮, 孙洪羽. 倒装芯片无铅凸点β-Sn晶粒取向与电迁移交互作用 [J]. 金属学报, 2018, 54: 1077 | |
| 24 | Huang M L, Zhao J F, Zhang Z J, et al. Dominant effect of high anisotropy in β-Sn grain on electromigration-induced failure mechanism in Sn-3.0Ag-0.5Cu interconnect [J]. J. Alloys Compd., 2016, 678: 370 |
| 25 | Xu K X, Fu X, Wang X J, et al. The effect of grain orientation of β-Sn on copper pillar solder joints during electromigration [J]. Materials, 2022, 15: 108 |
| 26 | Li X, Gao L Y, Tao J L, et al. Detrimental angle range between c axis of Sn crystal and electron flow for the electromigration reliability of ball grid array devices [J]. J. Mater. Sci.: Mater. Electron., 2022, 33: 17877 |
| 27 | Wang Y, Wang Y S, Ma L M, et al. Effect of Sn grain c-axis on Cu atomic motion in Cu reinforced composite solder joints under electromigration [J]. J. Electron. Mater., 2020, 49: 2159 |
| 28 | Bashir M N, Butt S U, Mansoor M A, et al. Role of crystallographic orientation of β-Sn grain on electromigration failures in lead-free solder joint: An overview [J]. Coatings, 2022, 12: 1752 |
| 29 | Shen Y A, Wu J A. Effect of Sn grain orientation on reliability issues of Sn-rich solder joints [J]. Materials, 2022, 15: 5086 |
| 30 | Yuan H Y, Li C, Zhang H Z, et al. Revealing evolutions of intermetallics in a solder joint under electromigration: A quasi-in situ study combining 3D microstructural characterization and numerical simulation [J]. Appl. Phys. Lett., 2023, 123: 231904 |
| 31 | Mohanram H, Kim Y, Ni G, et al. Control of solder microstructure stimulated by interface condition of the UBM/solder and enhancement of electromigration reliability [A]. 2023 IEEE 73rd Electronic Components and Technology Conference (ECTC) [C]. Orlando: IEEE, 2023: 1060 |
| 32 | Tsai C P, Chiu C Y, Huang W C, et al. Single-grain Sn-rich micro-bump by reducing Sn undercooling with heterogeneous nucleation [J]. Mater. Lett., 2024, 357: 135729 |
| 33 | Yuan H Y, Li C, Ma Z L, et al. A case study of intermetallic evolutions in a solder joint under electromigration using a novel experiment-simulation combined approach [A]. 24th International Conference on Electronic Packaging Technology (ICEPT) [C]. Shihezi City: IEEE, 2023: 1 |
| 34 | Wang S B, Liu P, Cong S, et al. The Evolution of micro-voids in Sn37Pb solder joints under electromechanical coupling loading [J]. J. Electron. Mater., 2024, 53: 6448 |
| 35 | Zhang Q K, An C W, Song Z L. Thermal cycling-electric current coupling damage mechanisms of SnAgCu/Cu solder joints under different temperature ranges [J]. J. Electron. Mater., 2024, 53: 2544 |
| 36 | Li S L, Hang C J, Zhang W, et al. Current-induced solder evolution and mechanical property of Sn-3.0Ag-0.5Cu solder joints under thermal shock condition [J]. J. Alloys Compd., 2024, 970: 172519 |
| 37 | Huang M L, Zhou S M, Chen L D, et al. Effect of electroless Ni-P consumption on the failure mechanism of solder joints during electromigration [J]. Acta Metall. Sin., 2013, 49: 81 |
| 黄明亮, 周少明, 陈雷达 等. Ni-P消耗对焊点电迁移失效机理的影响 [J]. 金属学报, 2013, 49: 81 | |
| 38 | Fu Z W, Wei Q R, Guo X T, et al. Influence of temperature and current stressing on Cu-Sn intermetallic compound growth characteristics of lead-free microbump [J]. Adv. Theory Simul., 2023, 6: 2200881 |
| 39 | Huang J Q, Zhu Y H, Pan K H, et al. Polarity effect of interfacial intermetallic compounds of BGA structure Cu/Sn-52In/Cu solder joints during electromigration [J]. Intermetallics, 2024, 168: 108252 |
| 40 | Chen L D, Huang M L, Zhou S M. Effect of electromigration on intermetallic compound formation in line-type Cu/Sn/Cu interconnect [J]. J. Alloys Compd., 2010, 504: 535 |
| 41 | Zhang X F, Guo J D, Shang J K. Reverse polarity effect from effective charge disparity during electromigration in eutectic Sn-Zn solder interconnect [J]. J. Mater. Res., 2008, 23: 3370 |
| 42 | Tu K N. Solder Joint Technology: Materials, Properties, and Reliability [M]. New York: Springer, 2007: 1 |
| 43 | Liang S B, Jiang H, Huang J Q. Study on phase electromigration and segregation behavior of Cu-cored Sn-58Bi solder interconnects under electric current stressing [J]. J. Electron. Mater., 2024, 53: 1192 |
| 44 | Chen W M, Zhang K K, Fan Y C, et al. Effect of electromigration on microstructure and properties of CeO2 nanopartical-reinforced Sn58Bi/Cu solder joints [J]. Sci. Rep., 2024, 14: 15693 |
| 45 | Daghfal J P, Shang J K. Current-induced phase partitioning in eutectic indium-tin Pb-free solder interconnect [J]. J. Electron. Mater., 2007, 36: 1372 |
| 46 | Huang M L, Zhang Z J, Zhao N, et al. Migration behavior of indium atoms in Cu/Sn-52In/Cu interconnects during electromigration [J]. J. Mater. Res., 2015, 30: 3316 |
| 47 | Zhang Z J, Huang M L. Liquid-solid electromigration behavior of Cu/Sn-52In/Cu micro-interconnect [J]. Acta Metall. Sin., 2017, 53: 592 |
| 张志杰, 黄明亮. Cu/Sn-52In/Cu微焊点液-固电迁移行为研究 [J]. 金属学报, 2017, 53: 592 | |
| 48 | Zhang Z J, Huang M L. In situ study on liquid-solid electromigration behavior in Cu/Sn-37Pb/Cu micro-interconnect [J]. Acta Metall. Sin., 2020, 56: 1386 |
| 张志杰, 黄明亮. 原位研究Cu/Sn-37Pb/Cu微焊点液-固电迁移行为 [J]. 金属学报, 2020, 56: 1386 | |
| 49 | Huang M L, Zhang Z J, Yang F, et al. Novel growth of whole preferred orientation intermetallic compound interconnects for 3D IC packaging [A]. 2016 IEEE 66th Electronic Components and Technology Conference (ECTC) [C]. Las Vegas: IEEE, 2016: 1216 |
| 50 | Huang M L, Zou L, Yin S Q. Electromigration behavior and mechanical properties of the whole preferred orientation intermetallic compound interconnects for 3D packaging [A]. 2018 IEEE 68th Electronic Components and Technology Conference (ECTC) [C]. San Diego: IEEE, 2018: 2041 |
| 51 | Huang M L, Zou L. Effects of electromigration on microstructural evolution and mechanical properties of preferential growth intermetallic compound interconnects for 3D packaging [A]. 2019 IEEE 69th Electronic Components and Technology Conference (ECTC) [C]. Las Vegas: IEEE, 2019: 1774 |
| 52 | Huang M L, Zhao N, Zhang Z J, et al. A preparation method and structure of full intermetallic compound (IMC) interconnects [P]. Chin Pat, 201510069883.6, 2016 |
| 黄明亮, 赵 宁, 张志杰 等. 一种全金属间化合物互连焊点的制备方法及结构 [P]. 中国专利, 201510069883.6, 2016) | |
| 53 | Huang M L, Wu Y, Zhang S N, et al. A method to control crystal orientation and microstructure of full intermetallic compound (IMC) interconnects [P]. Chin Pat, 202010964080.8, 2020 |
| 黄明亮, 武 洋, 张诗楠 等. 一种控制全金属间化合物微互连焊点晶体取向及微观组织的方法 [P]. 中国专利, 202010964080.8, 2020) | |
| 54 | Black J R. Electromigration failure modes in aluminum metallization for semiconductor devices [J]. Proc. IEEE, 1969, 57: 1587 |
| 55 | Yao Y F, Gusak A M, Chen C, et al. Influence of Sn grain orientation on mean-time-to-failure equation for microbumps in 3D IC technology [J]. Scr. Mater., 2024, 250: 116175 |
| 56 | Flores J, Panta S, Hadian F, et al. Changes in the microstructure and electrical resistance of SnBi-based solder joints during current stressing [J]. J. Electron. Mater., 2024, 53: 1299 |
| 57 | Chen S, Wu Q S, Fu Z W, et al. Black equation of the electromigration lifetime for ceramic package with lead bumps and plastic package with lead-free bump [A]. 2020 21st International Conference on Electronic Packaging Technology (ICEPT) [C]. Guangzhou: IEEE, 2020: 1 |
| 58 | Li Y R Y, Fu G C, Wan B, et al. A study on the effects of electrical and thermal stresses on void formation and migration lifetime of Sn3.0Ag0.5Cu solder joints [J]. Soldering Surf. Mount Technol., 2021, 34: 162 |
| 59 | Ting L M, May J S, Hunter W R, et al. AC electromigration characterization and modeling of multilayered interconnects [A]. 31st Annual Proceedings Reliability Physics 1993 [C]. Atlanta: IEEE, 1993: 311 |
| 60 | Liang S B, Kunwar A, Wei C, et al. Insight into the preferential grain growth of intermetallics under electric current stressing—A phase field modeling [J]. Scr. Mater., 2021, 203: 114071 |
| 61 | Liang S B, Wei C, Kunwar A, et al. Phase field modelling combined with data-driven approach to unravel the orientation influenced growth of interfacial Cu6Sn5 intermetallics under electric current stressing [J]. Surf. Interfaces, 2023, 37: 102728 |
| 62 | Zhao Z P, Zhang X M, Wu Z Z, et al. Competitive failure mechanism and load tolerance of solder joint under thermo-mechano-electrical coupling [J]. Mech. Mater., 2021, 163: 104104 |
| 63 | Guo F, Wen T Y, Ma L M, et al. Electromigration damage analysis of BGA solder joint under high temperature and high current density [J]. J. Beijing Univ. Technol., 2021, 47: 1264 |
| 郭 福, 文廷玉, 马立民 等. 高温高电流密度下BGA焊点电迁移损伤 [J]. 北京工业大学学报, 2021, 47: 1264 | |
| 64 | Hu S H, Lin T C, Kao C L, et al. Effects of bismuth additions on mechanical property and microstructure of SAC-Bi solder joint under current stressing [J]. Microelectron. Reliab., 2021, 117: 114041 |
| 65 | Mokhtar N Z M, Salleh M A A M, Zhang G M, et al. Tin whiskers formation in Sn0.7Cu0.05Ni1.5Bi under electro-migration stressing [J]. Acta Phys. Pol., 2020, 138A: 261 |
| 66 | Lin Y X, Wang J Y, Chen C Y, et al. Effect of Ag additives on the consumption of a cathode Cu pad in a Cu/Sn3.5Ag/Cu flip-chip structure under electromigration [J]. J. Electron. Mater., 2021, 50: 6584 |
| 67 | Liu H Y, Zhu Q S, Wang Z G, et al. Effects of Zn addition on electromigration behavior of Sn-1Ag-0.5Cu solder interconnect [J]. J. Mater. Sci.: Mater. Electron., 2013, 24: 211 |
| 68 | Li M Y, Han J, Guo F, et al. Electromigration behavior of low-silver Sn-0.3Ag-0.7Cu-1.6Bi-0.2In solder joints [J]. J. Electron. Mater., 2020, 49: 4237 |
| 69 | Kelly M B, Antoniswamy A, Mahajan R, et al. Effect of trace addition of In on Sn-Cu solder joint microstructure under electromigration [J]. J. Electron. Mater., 2021, 50: 893 |
| 70 | Liu S F, Liu Z Y, Liu L, et al. Electromigration behavior of Cu/Sn-58Bi-1Ag/Cu solder joints by ultrasonic soldering process [J]. J. Mater. Sci.: Mater. Electron., 2020, 31: 11997 |
| 71 | Zhao X, Saka M, Muraoka M, et al. Electromigration behaviors and effects of addition elements on the formation of a Bi-rich layer in Sn58Bi-based solders [J]. J. Electron. Mater., 2014, 43: 4179 |
| 72 | Wu X F, Hou Z Z, Xie X C, et al. Microstructural evolution of joints with and without Sb, Ni in Sn58Bi solder under electro-thermal-force coupling [J]. J. Mater. Res. Technol., 2023, 26: 1382 |
| 73 | Wu X F, Hou Z Z, Xie X C, et al. Mechanical properties and microstructure evolution of Sn-Bi-based solder joints by microalloying regulation mechanism [J]. J. Mater. Res. Technol., 2024, 31: 3226 |
| 74 | Bashir M N, Khan N B, Bashir S, et al. Effect of Zn nanoparticle-doped flux on mechanical properties of SAC305 solder joint after electromigration [J]. J. Mater. Sci.: Mater. Electron., 2023, 34: 321 |
| 75 | Bashir M N, Haseeb A S M A. Grain size stability of interfacial intermetallic compound in Ni and Co nanoparticle-doped SAC305 solder joints under electromigration [J]. J. Mater. Sci.: Mater. Electron., 2022, 33: 14240 |
| 76 | Bashir M N, Haseeb A S M A, Rahman A Z M S, et al. Effect of cobalt doping on the microstructure and tensile properties of lead free solder joint subjected to electromigration [J]. J. Mater. Sci. Technol., 2016, 32: 1129 |
| 77 | Li Y, Luo K M, Lim A B Y, et al. Improving the mechanical performance of Sn57.6Bi0.4Ag solder joints on Au/Ni/Cu pads during aging and electromigration through the addition of tungsten (W) nanoparticle reinforcement [J]. Mater. Sci. Eng., 2016, A669: 291 |
| 78 | Shafiq I, Chan Y C, Xu S, et al. Electro-migration study of nano Al doped lead-free Sn-58Bi on Cu and Au/Ni/Cu ball grid array (BGA) packages [A]. 18th European Microelectronics & Packaging Conference [C]. Brighton: IEEE, 2011: 1 |
| 79 | Shafiq I, Chan Y C. Improved electro-migration resistance in nano Ag modified Sn-58Bi solder joints under current stressing [A]. 2011 International Conference on Quality, Reliability, Risk, Maintenance, and Safety Engineering [C]. Xi'an: IEEE, 2011: 374 |
| 80 | Kim Y, Nagao S, Sugahara T, et al. Refinement of the microstructure of Sn-Ag-Bi-In solder, by addition of SiC nanoparticles, to reduce electromigration damage under high electric current [J]. J. Electron. Mater., 2014, 43: 4428 |
| 81 | Yang L, Ge J G, Zhang Y C, et al. Electromigration reliability for Al2O3-reinforced Cu/Sn-58Bi/Cu composite solder joints [J]. J. Mater. Sci.: Mater. Electron., 2017, 28: 3004 |
| 82 | Xu S, Chan Y C, Zhang K L, et al. Interfacial intermetallic growth and mechanical properties of carbon nanotubes reinforced Sn3.5Ag0.5Cu solder joint under current stressing [J]. J. Alloys Compd., 2014, 595: 92 |
| 83 | Chen G, Li J Q, Kuang X W, et al. The study on reliability of Ni-coated graphene doped SAC305 lead-free composite solders under high current-density stressing [J]. Soldering Surf. Mount Technol., 2019, 31: 261 |
| 84 | Kim J, Jung K H, Kim J H, et al. Electromigration behaviors of Sn58%Bi solder containing Ag-coated MWCNTs with OSP surface finished PCB [J]. J. Alloys Compd., 2019, 775: 581 |
| 85 | Dai J J, Zhang Y X, Li Z K, et al. Research on reliability of Ni/Sn/Cu(Ni) copper pillar bump under thermoelectric loading [J]. J. Electron. Packag., 2022, 144: 031014 |
| 86 | Chiu M C, Tsai M Y, Wang S B, et al. Applications of Ni and Ag metallizations at the solder/Cu interfaces in advanced high-power automobile interconnects: An electromigration study [J]. Surf. Coat. Technol., 2024, 484: 130828 |
| 87 | Kim J, Jung S B, Yoon J W. Effect of Ni(P) thickness in Au/Pd/Ni(P) surface finish on the electrical reliability of Sn-3.0Ag-0.5Cu solder joints during current-stressing [J]. J. Alloys Compd., 2021, 850: 156729 |
| 88 | Huang M L, Chen L D, Zhou S M, et al. Effect of surface finish (OSP and ENEPIG) on failure mechanism induced by electromigration in Sn-3.0Ag-0.5Cu flip chip solder interconnect [A]. 2011 International Symposium on Advanced Packaging Materials (APM) [C]. Xiamen: IEEE, 2011: 297 |
| 89 | Wang F J, Liu L T, Zhou L L, et al. Microstructural evolution of Sn-58Bi/Cu joints through minor Zn alloying substrate during electromigration [J]. Mater. Trans., 2017, 58: 1593 |
| 90 | Zhang S N, Ren J, Huang F F, et al. In-situ observation on liquid-solid electromigration behavior of (111) nt-Cu/Sn/Cu interconnects [A]. 25th International Conference on Electronic Packaging Technology (ICEPT) [C]. Tianjin: IEEE, 2024: 1 |
| 91 | Zhang J Q, Huang X M, Wang X J, et al. Effect of (111) oriented nanotwinned Cu substrate on the electromigration of Sn58Bi solder joint at high current density [J]. J. Mater. Sci.: Mater. Electron., 2024, 35: 1293 |
| 92 | Chen C N, Chen B Z, Wu W H, et al. Correlation between Ag content and Cu pad consumption in lead-free solder joints under electron current stressing [A]. 12th International Conference on Electronic Packaging Technology and High Density Packaging [C]. Shanghai: IEEE, 2011: 1 |
| 93 | Yamanaka K, Nishikawa H, Taguchi H, et al. Effect of magnetic flux density on Sn crystallographic orientation in a solder joint system [J]. J. Mater. Sci.: Mater. Electron., 2016, 27: 3710 |
| 94 | Chen J Q, Guo J D, Ma H C, et al. Magnetic-field induced anisotropy in electromigration behavior of Sn-Ag-Cu solder interconnects [J]. J. Mater. Res., 2015, 30: 1065 |
| 95 | Ma Z L, Belyakov S A, Sweatman K, et al. Harnessing heterogeneous nucleation to control tin orientations in electronic interconnections [J]. Nat. Commun., 2017, 8: 1916 |
| 96 | Huang M L, Yang F. Size effect model on kinetics of interfacial reaction between Sn-xAg-yCu solders and Cu substrate [J]. Sci. Rep., 2014, 4: 7117 |
| 97 | Liu Y X, Chu Y C, Tu K N. Scaling effect of interfacial reaction on intermetallic compound formation in Sn/Cu pillar down to 1 μm diameter [J]. Acta Mater., 2016, 117: 146 |
| 98 | Ouyang F Y, Hsu H, Su Y P, et al. Electromigration induced failure on lead-free micro bumps in three-dimensional integrated circuits packaging [J]. J. Appl. Phys., 2012, 112: 023505 |
| 99 | Shen Y A, Chen C. Effect of Sn grain orientation on formation of Cu6Sn5 intermetallic compounds during electromigration [J]. Scr. Mater., 2017, 128: 6 |
| 100 | Chang Y W, Hu C C, Peng H Y, et al. A new failure mechanism of electromigration by surface diffusion of Sn on Ni and Cu metallization in microbumps [J]. Sci. Rep., 2018, 8: 5935 |
/
| 〈 |
|
〉 |