累积叠轧焊Cu/Nb多层材料中的滑移传递
收稿日期: 2024-09-27
修回日期: 2024-11-21
网络出版日期: 2024-12-17
基金资助
国家自然科学基金项目(52474424);国家自然科学基金项目(52431002);凝固技术国家重点实验室自主课题项目(2022-TS-01)
Slip Transfer in Accumulative Roll Bonding Cu/Nb Multilayer Composites
Received date: 2024-09-27
Revised date: 2024-11-21
Online published: 2024-12-17
Supported by
National Natural Science Foundation of China(52474424);National Natural Science Foundation of China(52431002);Research Fund of the State Key Laboratory of Solidi?cation Processing(2022-TS-01)
为探明累积叠轧焊Cu/Nb多层材料中的滑移传递机制,本工作利用SEM和EBSD观察原位拉伸实验过程中滑移迹线的对齐状况和表面形貌的连续程度,系统研究了晶界和相界处的滑移传递和阻塞行为;并通过统计Luster-Morris参数(m′)和残余Burgers矢量(Δb),分析Cu/Nb多层材料中的滑移传递规律。结果表明,Cu层相比Nb层更易发生晶界处的滑移传递,Cu晶界发生滑移传递时所需的最小m′ (
关键词: 滑移传递; Cu/Nb多层复合材料; 非均匀变形; 原位拉伸实验
杨然 , 宋韶杰 , 刘飞龙 , 申熙美 , 宋克兴 , 刘峰 . 累积叠轧焊Cu/Nb多层材料中的滑移传递[J]. 金属学报, 2026 , 62(8) : 1443 -1453 . DOI: 10.11900/0412.1961.2024.00337
Niobium-based alloys are commonly used as superconductors in particle accelerators and fusion Tokamaks. However, magnets made of these alloys experience considerable radiation damage, particularly from helium transmutation products in nuclear reactors, which tend to aggregate at grain boundaries (GBs) and phase boundaries (PBs). This aggregation severely degrades the material's performance. Furthermore, niobium is highly prone to oxidation at high temperatures, further restricting its applications in extreme environments. Recent studies have demonstrated that Cu/Nb multilayer composites fabricated through accumulative roll bonding (ARB) exhibit high yield strength, acceptable ductility, and excellent radiation resistance, making them highly promising for nuclear industry applications. In Cu/Nb multilayer composites with fcc/bcc structures prepared via ARB, interfacial instability and strain concentration can occur during deformation due to the high three-dimensional incompatibility of heterophase interfaces. In this study, Cu/Nb polycrystalline multilayer composites were prepared using ARB. In situ tensile tests were conducted using SEM to investigate the slip transfer and blocking behaviors at the GBs and PBs. These behaviors were studied by observing the slip trace alignment and surface morphology continuity. Slip transfer behavior in Cu/Nb multilayer materials was elucidated through statistical analysis of the Luster-Morris parameter (m' = cosψcosκ,where ψ and κ represent the angles between the two slip plane normal directions and the two slip directions, respectively) and residual Burgers vector (Δb = | bs2-bs1|, where bs2and bs1 are the two unit Burgers vectors of the slip systems in sample coordinate system). In the Cu layer, slip transfer occurs at the GBs when m′ exceeds 0.77 and Δb is less than 0.029. In the Nb layer, slip transfer occurs when m′ exceeds 0.81 and Δb is less than 0.250. For the Cu/Nb PBs, slip transfer occurs when m′ exceeds 0.93 and Δb is less than 0.173. Notably, the minimum m′(
| [1] | Chee S W, Stumphy B, Vo N Q, et al. Dynamic self-organization in Cu alloys under ion irradiation [J]. Acta Mater., 2010, 58: 4088 |
| [2] | Fu E G, Misra A, Wang H, et al. Interface enabled defects reduction in helium ion irradiated Cu/V nanolayers [J]. J. Nucl. Mater., 2010, 407: 178 |
| [3] | Zhang X, Li N, Anderoglu O, et al. Nanostructured Cu/Nb multilayers subjected to helium ion-irradiation [J]. Nucl. Instrum. Methods Phys. Res., 2007, 261B: 1129 |
| [4] | Saito Y, Utsunomiya H, Tsuji N, et al. Novel ultra-high straining process for bulk materials—Development of the accumulative roll-bonding (ARB) process [J]. Acta Mater., 1999, 47: 579 |
| [5] | Gao R, Jin M M, Han F, et al. Superconducting Cu/Nb nanolaminate by coded accumulative roll bonding and its helium damage characteristics [J]. Acta Mater., 2020, 197: 212 |
| [6] | Dong S J, Chen T J, Huang S X, et al. Thickness-dependent shear localization in Cu/Nb metallic nanolayered composites [J]. Scr. Mater., 2020, 187: 323 |
| [7] | Jia N, Roters F, Eisenlohr P, et al. Simulation of shear banding in heterophase co-deformation: Example of plane strain compressed Cu-Ag and Cu-Nb metal matrix composites [J]. Acta Mater., 2013, 61: 4591 |
| [8] | Bayerschen E, McBride A T, Reddy B D, et al. Review on slip transmission criteria in experiments and crystal plasticity models [J]. J. Mater. Sci., 2016, 51: 2243 |
| [9] | Zhang Y B, Song S J, Liu F. Thermo-kinetic orientation study on interface behavior of polycrystalline Cu-Nb composite by crystal plasticity finite element method [J]. Mater. Des., 2022, 223: 111215 |
| [10] | Zhou H, Wang P, Lu S P. Investigation on the effects of grain boundary on deformation behavior of bicrystalline pillar by crystal plasticity finite element method [J]. Crystals, 2021, 11: 923 |
| [11] | Patriarca L, Abuzaid W, Sehitoglu H, et al. Slip transmission in bcc FeCr polycrystal [J]. Mater. Sci. Eng., 2013, A588: 308 |
| [12] | Luster J, Morris M A. Compatibility of deformation in two-phase Ti-Al alloys: Dependence on microstructure and orientation relationships [J]. Metall. Mater. Trans., 1995, 26A: 1745 |
| [13] | Xu Y S, Zhang W G, Xu L C, et al. Simulation of deformation coordination and hardening behavior in ferrite-ferrite grain boundary [J]. Acta Metall. Sin., 2023, 59: 1042 |
| 徐永生, 张卫刚, 徐凌超 等. 铁素体晶间变形协调与硬化行为模拟研究 [J]. 金属学报, 2023, 59: 1042 | |
| [14] | Alizadeh R, Pe?a-Ortega M, Bieler T R, et al. A criterion for slip transfer at grain boundaries in Al [J]. Scr. Mater., 2020, 178: 408 |
| [15] | Palomares-García A J, Pérez-Prado M T, Molina-Aldareguia J M. Slip transfer across γ-TiAl lamellae in tension [J]. Mater. Des., 2018, 146: 81 |
| [16] | Abuzaid W, Sangid M D, Sehitoglu H, et al. The role of slip transmission on plastic strain accumulation across grain boundaries [J]. Procedia IUTAM, 2012, 4: 169 |
| [17] | Ding C G, Xu J, Li X W, et al. Microstructural evolution and mechanical behavior of Cu/Nb multilayer composites processed by accumulative roll bonding [J]. Adv. Eng. Mater., 2020, 22: 1900702 |
| [18] | You X J, Yang J, Dan C Y, et al. Statistical analysis of slip transfer in Al alloy based on in-situ tensile test and high-throughput computing method [J]. Int. J. Plast., 2023, 166: 103649 |
| [19] | Wang H, Boehlert C J, Wang Q D, et al. In-situ analysis of the slip activity during tensile deformation of cast and extruded Mg-10Gd-3Y-0.5 Zr (wt.%) at 250 oC [J]. Mater. Charact., 2016, 116: 8 |
| [20] | Dash S S, Li D J, Zeng X Q, et al. On the origin of deformation mechanisms in a heterostructured aluminum alloy via slip trace and lattice rotation analyses [J]. Mater. Sci. Eng., 2023, A867: 144723 |
| [21] | Zhang Y B, Song S J, Liu F. Thermo-kinetic characteristics on stabilizing hetero-phase interface of metal matrix composites by crystal plasticity finite element method [J]. J. Mater. Sci. Technol., 2024, 169: 53 |
| [22] | Chen J T, Lu J X, Cheng X P, et al. In-situ study of the effect of grain boundary misorientation on plastic deformation of Inconel 718 at high temperature [J]. J. Mater. Sci., 2024, 59: 7473 |
| [23] | Zheng S J, Yan Z, Kong X F, et al. Interface modifications on strength and plasticity of nanolayered metallic composites [J]. Acta Metall. Sin., 2022, 58: 709 |
| 郑士建, 闫 哲, 孔祥飞 等. 纳米金属层状材料强塑性的界面调控 [J]. 金属学报, 2022, 58: 709 | |
| [24] | Zha M, Ma X, Jia H L, et al. Dynamic precipitation and deformation behaviors of a bimodal-grained WE43 alloy with enhanced mechanical properties [J]. Int. J. Plast., 2023, 167: 103682 |
| [25] | Mara N A, Beyerlein I J. Review: Effect of bimetal interface structure on the mechanical behavior of Cu-Nb fcc-bcc nanolayered composites [J]. J. Mater. Sci., 2014, 49: 6497-6516 |
| [26] | Hunter A, Leu B, Beyerlein I J. A review of slip transfer: Applications of mesoscale techniques [J]. J. Mater. Sci., 2018, 53: 5584 |
| [27] | Wang J, Misra A, Hoagland R G, et al. Slip transmission across fcc/bcc interfaces with varying interface shear strengths [J]. Acta Mater., 2012, 60: 1503 |
| [28] | Wang J, Hoagland R G, Liu X Y, et al. The influence of interface shear strength on the glide dislocation-interface interactions [J]. Acta Mater., 2011, 59: 3164 |
| [29] | Sangid M D, Ezaz T, Sehitoglu H, et al. Energy of slip transmission and nucleation at grain boundaries [J]. Acta Mater., 2011, 59: 283 |
| [30] | Huang Z X, Jiang Y H, Lai C M, et al. Analysis of the correlation between the energy and crystallographic orientation of grain boundaries in Fe based on atomistic simulations [J]. Acta Metall. Sin., 2024, 60: 1289 |
| 黄曾鑫, 蒋逸航, 赖春明 等. 基于原子模拟的金属Fe晶界能与晶界取向相关性分析 [J]. 金属学报, 2024, 60: 1289 |
/
| 〈 |
|
〉 |