O含量对Ti2448合金时效析出行为及力学性能的影响
收稿日期: 2024-04-15
修回日期: 2024-06-12
网络出版日期: 2024-08-29
基金资助
国家自然科学基金项目(U2341259)
Effect of O Content on the Aging Precipitation Behavior and Mechanical Properties of Ti2448 Alloy
Received date: 2024-04-15
Revised date: 2024-06-12
Online published: 2024-08-29
Supported by
National Natural Science Foundation of China(U2341259)
为探究O含量对经双步热处理后Ti2448合金时效析出行为及力学性能的影响,选取2种不同O含量的Ti2448合金(LO:0.08%和HO:0.33%,质量分数)为研究对象,分别采用873和923 K退火10 min + 773 K时效1~4 h的热处理工艺,通过XRD、SEM、TEM和拉伸性能测试等方法,研究合金的组织演化行为和力学性能变化。结果表明,O含量对热处理前合金的相组成与晶粒尺寸影响较小,但提高O含量能抑制合金的双屈服特征并提升合金强度与弹性模量。经双步热处理后,2种O含量合金均析出致密的片层状析出相,伴有模量硬化与时效强化;O含量对析出相的初始厚度影响较小,但影响析出相在后续时效过程的粗化行为。相同热处理制度下,Ti2448-HO合金析出相的体积分数更高,进而贡献更强的模量硬化与时效强化,因此时效态Ti2448-HO合金具有更高的弹性模量与强度。
李丹 , 宫得伦 , 郝玉琳 . O含量对Ti2448合金时效析出行为及力学性能的影响[J]. 金属学报, 2025 , 61(12) : 1790 -1802 . DOI: 10.11900/0412.1961.2024.00107
Metastable β-titanium alloys are widely used in advanced biomedical applications because of their high strength and low modulus. Strength improvements in these alloys are mainly achieved through α-phase precipitation. Interestingly, a novel α″ + β dual-phase microstructure has been discovered in a multifunctional Ti2448 alloy after aging treatments, which effectively enhanced the strength while maintaining decent ductility. Since O plays a crucial role in regulating the decomposition and mechanical properties of titanium alloys, understanding its effects on the microstructural evolution and mechanical behavior of Ti2448 alloys is of great importance. However, the effect of O on the decomposition behavior of the Ti2448 alloy remains unclear. To investigate the influence of O content on the microstructure evolution and mechanical properties of the Ti2448 alloy, two Ti2448 alloys with different oxygen contents were selected: low oxygen (LO: 0.08%, mass fraction) and high oxygen (HO: 0.33%, mass fraction). This study employed a two-step heat treatment (annealing at 873/923 K for 10 min, followed by aging at 773 K for 1-4 h) on Ti2448-LO and Ti2448-HO alloys, focusing on the evolution of their microstructure and mechanical properties. Results indicated that O content minimally influenced the phase composition and grain size of the alloys before heat treatment. However, increasing the O content considerably suppressed the double yield phenomenon and enhanced the strength and elastic modulus of the alloy. After the two-step heat treatment, both alloys exhibited the precipitation of dense lamellar phases, resulting in remarkable modulus hardening and aging strengthening. Although the initial thickness of the precipitated phase was relatively unaffected by the O content, its subsequent coarsening behavior during aging was influenced. Under the same heat treatment conditions, the Ti2448-HO alloy exhibited a higher volume fraction of precipitates, leading to stronger modulus hardening and aging strengthening. Consequently, the aged Ti2448-HO alloy exhibited higher elastic modulus and strength than the Ti2448-LO alloy.
| [1] | Li S J, Hou W T, Hao Y L, et al. Research progress on the mechanical properties of the biomedical titanium alloy porous structures fabricated by 3D printing technique [J]. Acta Metall. Sin., 2023, 59: 478 |
| 李述军, 侯文韬, 郝玉琳 等. 3D打印医用钛合金多孔材料力学性能研究进展 [J]. 金属学报, 2023, 59: 478 | |
| [2] | Lütjering G, Williams J C. Titanium [M]. 2nd Ed., Berlin, Heidelberg: Springer, 2007: 8 |
| [3] | Zhu Y M, Zhang K, Meng Z C, et al. Ultrastrong nanotwinned titanium alloys through additive manufacturing [J]. Nat. Mater., 2022, 21: 1258 |
| [4] | Gong D L, Wang H L, Hao S H, et al. Ordering-induced Elinvar effect over a wide temperature range in a spinodal decomposition titanium alloy [J]. J. Mater. Sci. Technol., 2023, 150: 245 |
| [5] | Wang W J, Gong D L, Wang H L, et al. Spinodal decomposition coupled with a continuous crystal ordering in a titanium alloy [J]. Acta Mater., 2022, 233: 117969 |
| [6] | Wang H L, Hao Y L, He S Y, et al. Tracing the coupled atomic shear and shuffle for a cubic to a hexagonal crystal transition [J]. Scr. Mater., 2017, 133: 70 |
| [7] | Yu Q, Qi L, Tsuru T, et al. Origin of dramatic oxygen solute strengthening effect in titanium [J]. Science, 2015, 347: 635 |
| [8] | Liu Z, Welsch G. Effects of oxygen and heat treatment on the mechanical properties of alpha and beta titanium alloys [J]. Metall. Trans., 1988, 19A: 527 |
| [9] | Biesiekierski A, Wang J, Abdel-Hady Gepreel M, et al. A new look at biomedical Ti-based shape memory alloys [J]. Acta Biomater., 2012, 8: 1661 |
| [10] | Saito T, Furuta T, Hwang J H, et al. Multifunctional alloys obtained via a dislocation-free plastic deformation mechanism [J]. Science, 2003, 300: 464 |
| [11] | Tahara M, Kim H Y, Inamura T, et al. Lattice modulation and superelasticity in oxygen-added β-Ti alloys [J]. Acta Mater., 2011, 59: 6208 |
| [12] | Paton N E, Williams J C. The influence of oxygen content on the athermal β-ω transformation [J]. Scr. Metall., 1973, 7: 647 |
| [13] | Niu J G, Ping D H, Ohno T, et al. Suppression effect of oxygen on the β to ω transformation in a β-type Ti alloy: Insights from first-principles [J]. Model. Simul. Mater. Sci. Eng., 2014, 22: 015007 |
| [14] | Williams J C, Hickman B S, Leslie D H. The effect of ternary additions on the decompositon of metastable beta-phase titanium alloys [J]. Metall. Trans., 1971, 2: 477 |
| [15] | Tane M, Nakano T, Kuramoto S, et al. Low Young's modulus in Ti-Nb-Ta-Zr-O alloys: Cold working and oxygen effects [J]. Acta Mater., 2011, 59: 6975 |
| [16] | Niinomi M, Nakai M, Hendrickson M, et al. Influence of oxygen on omega phase stability in the Ti-29Nb-13Ta-4.6Zr alloy [J]. Scr. Mater., 2016, 123: 144 |
| [17] | Homma T, Arafah A, Haley D, et al. Effect of alloying elements on microstructural evolution in oxygen content controlled Ti-29Nb-13Ta-4.6Zr (wt%) alloys for biomedical applications during aging [J]. Mater. Sci. Eng., 2018, A709: 312 |
| [18] | Yang R, Ma Y J, Lei J F, et al. Toughening high strength titanium alloys through fine tuning phase composition and refining microstructure [J]. Acta Metall. Sin., 2021, 57: 1455 |
| 杨 锐, 马英杰, 雷家峰 等. 高强韧钛合金组成相成分和形态的精细调控 [J]. 金属学报, 2021, 57: 1455 | |
| [19] | Chong Y, Gholizadeh R, Guo B Q, et al. Oxygen interstitials make metastable β titanium alloys strong and ductile [J]. Acta Mater., 2023, 257: 119165 |
| [20] | Geng F, Niinomi M, Nakai M. Observation of yielding and strain hardening in a titanium alloy having high oxygen content [J]. Mater. Sci. Eng., 2011, A528 : 5435 |
| [21] | Fu Y, Xiao W L, Zhao S T, et al. Substantially strengthening a dual-phase titanium alloy by moderate oxygen doping [J]. Scr. Mater., 2023, 226: 115236 |
| [22] | Xiang W, Wang T, Miao R j, et al. Influence of oxygen on microstructures and tensile properties of hot-rolled Ti-4Zr-xO alloys [J]. Mater. Charact., 2021, 171: 110681 |
| [23] | dos Santos L U, Campo K N, Caram R, et al. Oxygen addition in biomedical Ti-Nb alloys with low Nb contents: Effect on the microstructure and mechanical properties [J]. Mater. Sci. Eng., 2021, A823: 141750 |
| [24] | Li S J, Jia M T, Prima F, et al. Improvements in nonlinear elasticity and strength by grain refinement in a titanium alloy with high oxygen content [J]. Scr. Mater., 2011, 64: 1015 |
| [25] | Sosa J M, Huber D E, Welk B A, et al. Mipar?: 2D and 3D image analysis software designed by materials scientists, for all scientists [J]. Microsc. Microanal., 2017, 23(suppl.1): 230 |
| [26] | Sharma A, Soni V, Dasari S, et al. Fine scale alpha precipitation in Ti-19at.%V in the absence of influence from omega precipitates [J]. Scr. Mater., 2021, 196: 113766 |
| [27] | Zheng Y F, Williams R E A, Sosa J M, et al. The indirect influence of the ω phase on the degree of refinement of distributions of the α phase in metastable β-Titanium alloys [J]. Acta Mater., 2016, 103: 165 |
| [28] | Cui J P, Hao Y L, Li S J, et al. Reversible movement of homogenously nucleated dislocations in a β-titanium alloy [J]. Phys. Rev. Lett., 2009, 102: 045503 |
| [29] | Wei L S, Kim H Y, Koyano T, et al. Effects of oxygen concentration and temperature on deformation behavior of Ti-Nb-Zr-Ta-O alloys [J]. Scr. Mater., 2016, 123: 55 |
| [30] | Chou K, Marquis E A. Oxygen effects on ω and α phase transformations in a metastable β Ti-Nb alloy [J]. Acta Mater., 2019, 181: 367 |
| [31] | Hao Y L, Li S J, Sun S Y, et al. Effect of Zr and Sn on Young's modulus and superelasticity of Ti-Nb-based alloys [J]. Mater. Sci. Eng., 2006, A441 : 112 |
| [32] | Pang E L, Pickering E J, Baik S I, et al. The effect of zirconium on the omega phase in Ti-24Nb-[0-8]Zr (at.%) alloys [J]. Acta Mater., 2018, 153: 62 |
| [33] | Okamoto N L, Brumbauer F, Luckabauer M, et al. Why is neutral tin addition necessary for biocompatible β-titanium alloys?—Synergistic effects of suppressing ω transformations [J]. Acta Mater., 2024, 273: 119968 |
| [34] | Hu Q M, Li S J, Hao Y L, et al. Phase stability and elastic modulus of Ti alloys containing Nb, Zr, and/or Sn from first-principles calculations [J]. Appl. Phys. Lett., 2008, 93: 121902 |
| [35] | Mott N F, Nabarro F R N. An attempt to estimate the degree of precipitation hardening, with a simple model [J]. Proc. Phys. Soc., 1940, 52: 86 |
| [36] | Villain J, Lavagna M, Bruno P. Jacques Friedel and the physics of metals and alloys [J]. C. R. Phys., 2016, 17: 276 |
| [37] | Gurney C. Report of a conference on the strength solids (1947) [J]. Nature, 1949, 163: 117 |
| [38] | Labusch R. A statistical theory of solid solution hardening [J]. Phys. Status Solidi, 1970, 41B: 659 |
| [39] | Conrad H, de Meester B, D?ner M, et al. Strengthening of alpha titanium by the interstitial solutes C, N, and O [A]. Physics of Solid Solution Strengthening [M]. New York: Springer, 1975: 1 |
| [40] | de Meester B, D?ner M, Conrad H. Deformation kinetics of the Ti-6Al-4V alloy at low temperatures [J]. Metall. Trans., 1975, 6A: 65 |
| [41] | Wang W J. Spinodal decomposition and its effect on mechanical properties of Ti2448 alloy [D]. Hefei: University of Science and Technology of China, 2022 |
| 王伟杰. Ti2448合金的成分分解和组织性能研究 [D]. 合肥: 中国科学技术大学, 2022 | |
| [42] | Mantri S A, Choudhuri D, Alam T, et al. Tuning the scale of α precipitates in β-titanium alloys for achieving high strength [J]. Scr. Mater., 2018, 154: 139 |
| [43] | Nembach E. Precipitation hardening caused by a difference in shear modulus between particle and matrix [J]. Phys. Status Solidi, 1983, 78A: 571 |
| [44] | Kato M. Hardening by spinodally modulated structure in b.c.c. alloys [J]. Acta Metall., 1981, 29: 79 |
| [45] | Wei Q Q, Wang L Q, Fu Y F, et al. Influence of oxygen content on microstructure and mechanical properties of Ti-Nb-Ta-Zr alloy [J]. Mater. Des., 2011, 32: 2934 |
| [46] | Chong Y, Gholizadeh R, Tsuru T, et al. Grain refinement in titanium prevents low temperature oxygen embrittlement [J]. Nat. Commun., 2023, 14: 404 |
/
| 〈 |
|
〉 |