横向弱磁场对镍基高温合金发散双晶竞争生长行为的影响
收稿日期: 2023-11-06
修回日期: 2024-01-03
网络出版日期: 2024-02-29
基金资助
国家重点研发计划项目(2019YFA0705300);国家重大科研仪器研制项目(52127807)
Effect of Weak Transverse Magnetic Field on the Competitive Grain Growth of Ni-Based Superalloy with Divergent Bi-Crystals
Received date: 2023-11-06
Revised date: 2024-01-03
Online published: 2024-02-29
Supported by
National Key Research and Development Program of China(2019YFA0705300);National Major Research Instrument Development Project of China(52127807)
静磁场作为外加物理场,可以有效调控材料成形过程,为调控镍基高温合金的凝固组织和晶体定向生长提供了新的思路。本工作研究了DD483镍基高温合金发散双晶在横向弱磁场下(0.1和0.7 T)的定向竞争生长规律和组织形貌演变特征。结果表明,未施加磁场时,发散双晶中择优取向晶粒(晶粒A)淘汰非择优取向晶粒(晶粒B),且晶粒淘汰速率与抽拉速率无关。磁场能显著影响发散双晶的竞争生长速率,且其受到双晶在磁场下的摆放方式和抽拉速率的影响。当发散双晶在磁场下按A-to-B方式摆放时,施加磁场抑制了晶粒A在晶界处的分枝,减缓了晶粒A的淘汰速率。当发散双晶按B-to-A方式摆放时,施加磁场进一步促进了晶粒A在晶界处的分枝,加速了晶粒A的淘汰速率。随着抽拉速率的提高,磁场对减缓或加速晶粒的竞争淘汰作用逐渐减弱。磁场在枝晶间产生的热电磁对流效应改变了发散双晶晶界处的溶质分布,从而影响枝晶在晶界处的侧枝生长,这是导致晶粒竞争生长行为发生变化的主要原因。随着抽拉速率的增加,磁场作用时间变短,热电磁对流对晶界处分枝作用的影响减弱。
谢信亮 , 周丽萍 , 余建波 , 玄伟东 , 陈超越 , 王江 , 任忠鸣 . 横向弱磁场对镍基高温合金发散双晶竞争生长行为的影响[J]. 金属学报, 2025 , 61(8) : 1203 -1216 . DOI: 10.11900/0412.1961.2023.00438
Ni-based single-crystal superalloys have excellent high-temperature mechanical properties and creep properties, rendering them as preferred turbine blade materials in advanced aerospace and gas engines. Controlling competitive grain growth during directional solidification is of great substantial importance for achieving high-quality single-crystal blades. As an external physical field, a static magnetic field can be used to effectively control material forming. The use of static magnetic fields during directional solidification has evolved as an effective method for controlling microstructures and grain growth. However, the influence of static magnetic fields on competitive grain growth during the directional solidification of Ni-based superalloys requires further investigation. Therefore, this study explored the competitive growth behavior of divergent grains during the directional solidification of Ni-based superalloy using bi-crystal seeds at various withdrawal rates under a weak transverse magnetic field (0.1 and 0.7 T). Results showed that the favorably oriented grain (grain A) overgrew the unfavorably oriented grain (grain B) without the application of a magnetic field, and the overgrowth rate was independent of the withdrawal rate. The application of a magnetic field substantially changed the overgrowth rate of divergent bi-crystals, and the overgrowth rate was affected by the placed patterns of the divergent bi-crystals and the withdrawal rate. When the divergent bi-crystal seeds were placed under the magnetic field in an A-to-B pattern, with the favorably oriented grain A positioned on the left side and the unfavorably oriented grain B on the right side, the side branching of favorably oriented grain was suppressed at the grain boundary (GB), decreasing the overgrowth rate of divergent bi-crystals. However, when the divergent bi-crystal seeds were placed under the magnetic field in a B-to-A pattern, with the unfavorably oriented grain B on the left side and the favorably oriented grain A on the right side, branching from the favorably oriented grain at the GB was enhanced, increasing the overgrowth rate of divergent bi-crystals. With increasing the withdrawal rate, the effect of the magnetic field on slowing down or accelerating the grain overgrowth rate gradually diminished. In addition, a tilted interface and refined dendrites were observed under a transverse magnetic field, especially at a low withdrawal rate. The application of a magnetic field produces a thermomagnetic convective effect at the interdendrite that changes the solute distribution at the divergent bi-crystal GBs, thereby affecting the side branching behavior of dendrites at GBs. With increasing withdrawal rate, the effect of thermoelectric magnetic convection on dendrite side branching at GBs is weakened.
| [1] | Wagner A, Shollock B A, McLean M. Grain structure development in directional solidification of nickel-base superalloys [J]. Mater. Sci. Eng., 2004, A374: 270 |
| [2] | D'souza N, Ardakani M G, Wagner A, et al. Morphological aspects of competitive grain growth during directional solidification of a nickel-base superalloy, CMSX4 [J]. J. Mater. Sci., 2002, 37: 481 |
| [3] | Yan X W, Guo X, Liu Y L, et al. Numerical simulation of dendrite growth in Ni-based superalloy casting during directional solidification process [J]. Trans. Nonferrous Met. Soc. China, 2019, 29: 338 |
| [4] | Stanford N, Djakovic A, Shollock B A, et al. Seeding of single crystal superalloys—Role of seed melt-back on casting defects [J]. Scr. Mater., 2004, 50: 159 |
| [5] | Stanford N, Djakovic A, Shollock B, et al. Defect grains in the melt-back region of CMSX-4 single crystal seeds [A]. 10th International Symposium on Superalloys [C]. Warrendale: TMS, 2004, 719 |
| [6] | Su Z Q, Zhang C J, Yuan X T, et al. Formation and evolution of stray grains on remelted interface in the seed crystal during the directional solidification of single-crystal superalloys assisted by vertical static magnetic field [J]. Acta Metall. Sin., 2023, 59: 1568 |
| 苏震奇, 张丛江, 袁笑坦 等. 纵向静磁场下单晶高温合金定向凝固籽晶回熔界面杂晶的形成与演化 [J]. 金属学报, 2023, 59: 1568 | |
| [7] | Xu W L, Wang F, Ma D X, et al. Sliver defect formation in single crystal Ni-based superalloy castings [J]. Mater. Des., 2020, 196: 109138 |
| [8] | Hu S S, Yang W C, Li Z R, et al. Formation mechanisms and control method for stray grains at melt-back region of Ni-based single crystal seed [J]. Prog. Nat. Sci. Mater. Int., 2021, 31: 624 |
| [9] | Lei Z L, Lu N N, Yu X F. Epitaxy and new stray grain formation mechanism during epitaxial laser melting deposition of Inconel 718 on directionally solidified nickel-based superalloys [J]. J. Manuf. Processes, 2019, 42: 11 |
| [10] | Walton D, Chalmers B. The origin of the preferred orientation in the columnar zone of ingots [J]. Trans. Am. Inst. Min. Metall. Eng., 1959, 215: 447 |
| [11] | Rappaz M, Gandin C A, Desbiolles J L, et al. Prediction of grain structures in various solidification processes [J]. Metall. Mater. Trans., 1996, 27A: 695 |
| [12] | Gandin C A, Rappaz M. A 3D cellular automaton algorithm for the prediction of dendritic grain growth [J]. Acta Mater., 1997, 45: 2187 |
| [13] | Zhou Y Z, Volek A, Green N R. Mechanism of competitive grain growth in directional solidification of a nickel-base superalloy [J]. Acta Mater., 2008, 56: 2631 |
| [14] | Zhou Y Z, Jin T, Sun X F. Structure evolution in directionally solidified bicrystals of nickel base superalloys [J]. Acta Metall. Sin., 2010, 46: 1327 |
| 周亦胄, 金 涛, 孙晓峰. 双晶镍基高温合金定向凝固过程的结构演化 [J]. 金属学报, 2010, 46: 1327 | |
| [15] | Yu H L, Lin X, Li J J, et al. Research on diverged bi-crystal competitive growth in directional solidification [J]. Acta Metall. Sin., 2013, 49: 58 |
| 宇红雷, 林 鑫, 李俊杰 等. 定向凝固发散双晶的竞争生长研究 [J]. 金属学报, 2013, 49: 58 | |
| [16] | Tourret D, Karma A. Growth competition of columnar dendritic grains: A phase-field study [J]. Acta Mater., 2015, 82: 64 |
| [17] | Meng X B, Lu Q, Zhang X L, et al. Mechanism of competitive growth during directional solidification of a nickel-base superalloy in a three-dimensional reference frame [J]. Acta Mater., 2012, 60: 3965 |
| [18] | Guo C W, Li J J, Yu H L, et al. Branching-induced grain boundary evolution during directional solidification of columnar dendritic grains [J]. Acta Mater., 2017, 136: 148 |
| [19] | Guo C W, Weng K R, Wang J C, et al. Competitive growth of diverging columnar grains during directional solidification: A three-dimensional phase-field study [J]. Comput. Mater. Sci., 2022, 210: 111061 |
| [20] | Zhang X L, Feng L, Yang Y H, et al. Influence of secondary orientation on competitive grain growth of nickel-based superalloys [J]. Acta Metall. Sin., 2020, 56: 969 |
| 张小丽, 冯 丽, 杨彦红 等. 二次枝晶取向对镍基高温合金晶粒竞争生长行为的影响 [J]. 金属学报, 2020, 56: 969 | |
| [21] | Li J J, Wang Z J, Wang Y Q, et al. Phase-field study of competitive dendritic growth of converging grains during directional solidification [J]. Acta Mater., 2012, 60: 1478 |
| [22] | Takaki T, Ohno M, Shimokawabe T, et al. Two-dimensional phase-field simulations of dendrite competitive growth during the directional solidification of a binary alloy bicrystal [J]. Acta Mater., 2014, 81: 272 |
| [23] | Yu H L, Li J J, Lin X, et al. Anomalous overgrowth of converging dendrites during directional solidification [J]. J. Cryst. Growth, 2014, 402: 210 |
| [24] | Yang W C, Hu S S, Huo M, et al. Orientation controlling of Ni-based single-crystal superalloy by a novel method: Grain selection assisted by un-melted reused seed [J]. J. Mater. Res. Technol., 2019, 8: 1347 |
| [25] | Huo M, Liu L, Yang W C, et al. Dendrite growth and defects formation with increasing withdrawal rates in the rejoined platforms of Ni-based single crystal superalloys [J]. Vacuum, 2019, 161: 29 |
| [26] | Li X, Fautrelle Y, Ren Z M, et al. Effect of a high magnetic field on the morphological instability and irregularity of the interface of a binary alloy during directional solidification [J]. Acta Mater., 2009, 57: 1689 |
| [27] | Li X, Fautrelle Y, Gagnoud A, et al. Effect of a weak transverse magnetic field on solidification structure during directional solidification [J]. Acta Mater., 2014, 64: 367 |
| [28] | Wang J, Ren Z M, Fautrelle Y, et al. Modification of liquid/solid interface shape in directionally solidifying Al-Cu alloys by a transverse magnetic field [J]. J. Mater. Sci., 2013, 48: 213 |
| [29] | Xuan W D, Ren Z M, Li C J. Effect of a high magnetic field on microstructures of Ni-based superalloy during directional solidification [J]. J. Alloys Compd., 2015, 620: 10 |
| [30] | Li X, Gagnoud A, Ren Z M, et al. Investigation of thermoelectric magnetic convection and its effect on solidification structure during directional solidification under a low axial magnetic field [J]. Acta Mater., 2009, 57: 2180 |
| [31] | Liu X, Wang Y H, Zhang X X, et al. Influence of longitudinal static magnetic field on microstructure and microsegregation during directional solidification of DD98M alloy [J]. Acta Metall. Sin., 2024, 60: 1595 |
| 刘 翔, 王英豪, 张小新 等. 纵向静磁场对DD98M合金定向凝固微观组织与偏析的影响 [J]. 金属学报, 2024, 60: 1595 | |
| [32] | Zhu R, Wang J J, Zhang Y H, et al. Flow and solidification microstructure in metal melts driven by a combined magnetic field [J]. Acta Metall. Sin., 2024, 60: 231 |
| 朱 锐, 王俊杰, 张云虎 等. 复合磁场对金属熔体流动及凝固组织影响研究 [J]. 金属学报, 2024, 60: 231 | |
| [33] | Zhao Y, Su H J, Fan G R, et al. Tailoring microstructure and microsegregation in a directionally solidified Ni-based SX superalloy by a weak transverse static magnetic field [J]. Acta Metall. Sin. (Engl. Lett.), 2022, 35: 1164 |
| [34] | Zhou Y Z, Sun X F. Effect of solidification rate on competitive grain growth in directional solidification of a nickel-base superalloy [J]. Sci. China Technol. Sci., 2012, 55: 1327 |
| [35] | Lehmann P, Moreau R, Camel D, et al. Modification of interdendritic convection in directional solidification by a uniform magnetic field [J]. Acta Mater., 1998, 46: 4067 |
| [36] | Li X, Ren Z M, Gagnoud A, et al. Effects of thermoelectric magnetic convection on the solidification structure during directional solidification under lower transverse magnetic field [J]. Metall. Mater. Trans., 2011, 42A: 3459 |
| [37] | Wang J, Fautrelle Y, Ren Z M, et al. Thermoelectric magnetic flows in melt during directional solidification [J]. Appl. Phys. Lett., 2014, 104: 121916 |
| [38] | Dong J W, Ren Z M, Ren W L, et al. Effect of horizontal magnetic field on the microstructure of directionally solidified Ni-based superalloy [J]. Acta Metall. Sin., 2010, 46: 71 |
| 董建文, 任忠鸣, 任维丽 等. 横向磁场对镍基高温合金定向凝固组织的影响 [J]. 金属学报, 2010, 46: 71 | |
| [39] | Tong X, Beckermann C, Karma A, et al. Phase-field simulations of dendritic crystal growth in a forced flow [J]. Phys. Rev., 2001, 63E: 061601 |
| [40] | Yuan X T, Zhou T, Ren W L, et al. Nondestructive effect of the cusp magnetic field on the dendritic microstructure during the directional solidification of nickel-based single crystal superalloy [J]. J. Mater. Sci. Technol., 2021, 62: 52 |
| [41] | Zhong H, Li C J, Ren Z M, et al. Effect of interdendritic thermoelectric magnetic convection on evolution of tertiary dendrite during directional solidification [J]. J. Cryst. Growth, 2016, 439: 66 |
/
| 〈 |
|
〉 |