激光束空域形态对激光定向能量沉积316L不锈钢热输运影响的数值模拟
收稿日期: 2022-10-12
修回日期: 2022-11-04
网络出版日期: 2023-03-28
基金资助
国家自然科学基金项目(51975205);贵州省科学技术基金项目([2021]265);贵州省科学技术基金项目([2023]017);贵州大学自然科学基金项目((2021)15);贵州大学研究生创新人才计划项目(202203)
Numerical Simulation on Effects of Spatial Laser Beam Profiles on Heat Transport During Laser Directed Energy Deposition of 316L Stainless Steel
Received date: 2022-10-12
Revised date: 2022-11-04
Online published: 2023-03-28
Supported by
National Natural Science Foundation of China(51975205);Guizhou Provincial Science and Technology Projects([2021]265);Guizhou Provincial Science and Technology Projects([2023]017);Natural Science Foundation of Guizhou University((2021)15);Guizhou University Graduate Innovative Talent Program Project(202203)
激光整形是调控微观结构以改善增材制件性能的重要手段,但是激光整形定向能量沉积过程中的基本热输运行为仍需阐明。本工作建立了激光定向能量沉积三维热输运模型,对比研究了Gaussian形态(GP)、超Gaussian形态(SGP1、SGP2)和完全平顶形态(FTP) 4种激光束空域形态对316L不锈钢熔池传热和流体流动特征的影响。结果表明:GP、SGP1、SGP2和FTP下熔池的峰值温度依次降低,凝固界面上的温度梯度从熔池顶部到熔池底部逐渐上升;凝固界面的温度梯度与其到熔池表面光束中心的距离负相关,与凝固界面的法方向和激光扫描方向的夹角正相关;在GP、SGP1、SGP2和FTP作用下,靠近熔池后部的相同凝固界面处的温度梯度依次增大,但熔池底部的温度梯度却依次减小,熔池的平均流速依次减小;4种激光束空域形态下的熔池流动由Marangoni剪切应力主导,传热由Marangoni对流传热和热传导共同主导。
任松 , 吴家柱 , 张屹 , 张大斌 , 曹阳 , 尹存宏 . 激光束空域形态对激光定向能量沉积316L不锈钢热输运影响的数值模拟[J]. 金属学报, 2024 , 60(12) : 1678 -1690 . DOI: 10.11900/0412.1961.2022.00509
The distribution characteristics and magnitude of energy density on the cross section of a laser beam are determined by its spatial profile, which directly impacts heat transport during laser material processing. Hence, it is essential to understand the influence of spatial profiles on heat transport during laser directed energy deposition with synchronous material delivery. Herein, a three-dimensional heat transport model that takes into account important physical events such as laser-powder-pool coupling, thermal-fluid coupling, solid-liquid phase change, and multiple heat transfer was established. The model was validated using single-track single-layer deposition experiments. The effects of four spatial laser beam profiles, including Gaussian (GP), super-Gaussian (SGP1 and SGP2), and pure flat-topped (FTP) profiles, on the heat transport and fluid flow within the molten pool were investigated. Simulated results show that peak temperatures of the molten pool decrease sequentially under GP, SGP1, SGP2 and FTP, and the temperature gradients on the solidification interface increase gradually from the top to the bottom of the molten pool. Temperature gradients on the solidification interface positively correlate with the angle between the normal direction of the solidification interface and the laser scanning direction, and negatively correlate with the distances from the beam center on the molten pool surface. Under all four spatial laser beam profiles, temperature gradients at the same positions on the solidification interface near the rear of the molten pool increase, while those at the bottom of the molten pool decrease. The molten pool exhibits an outward annular flow pattern under all four spatial laser beam profiles with fluid flows mainly driven by Marangoni shear stress. Heat transfer within the molten pool is dominated by Marangoni convection and heat conduction. Average fluid velocities within the molten pool decrease successively according to the following order: Gaussian, super-Gaussian, and pure flat-topped profiles.
| 1 | Gu D D, Zhang H M, Chen H Y, et al. Laser additive manufacturing of high-performance metallic aerospace components [J]. Chin. J. Lasers, 2020, 47: 0500002 |
| 顾冬冬, 张红梅, 陈洪宇 等. 航空航天高性能金属材料构件激光增材制造 [J]. 中国激光, 2020, 47: 0500002 | |
| 2 | Li D C, He J K, Tian X Y, et al. Additive manufacturing: Integrated fabrication of macro/microstructures [J]. J. Mech. Eng., 2013, 49(6): 129 |
| 李涤尘, 贺健康, 田小永 等. 增材制造: 实现宏微结构一体化制造 [J]. 机械工程学报, 2013, 49(6): 129 | |
| 3 | Gong G H, Ye J J, Chi Y M, et al. Research status of laser additive manufacturing for metal: A review [J]. J. Mater. Res. Technol., 2021, 15: 855 |
| 4 | Roehling T T, Wu S S Q, Khairallah S A, et al. Modulating laser intensity profile ellipticity for microstructural control during metal additive manufacturing [J]. Acta Mater., 2017, 128: 197 |
| 5 | Tumkur T U, Voisin T, Shi R P, et al. Nondiffractive beam shaping for enhanced optothermal control in metal additive manufacturing [J]. Sci. Adv., 2021, 7: eabg9358 |
| 6 | Kubiak M, Piekarska W, Stano S. Modelling of laser beam heat source based on experimental research of Yb:YAG laser power distribution [J]. Int. J. Heat Mass Transfer, 2015, 83: 679 |
| 7 | Sundqvist J, Kaplan A F H, Shachaf L, et al. Analytical heat conduction modelling for shaped laser beams [J]. J. Mater. Process. Technol., 2017, 247: 48 |
| 8 | Ya W, Pathiraj B, Liu S J. 2D modelling of clad geometry and resulting thermal cycles during laser cladding [J]. J. Mater. Process. Technol., 2016, 230: 217 |
| 9 | Song M J, Wu L S, Liu J M, et al. Effects of laser cladding on crack resistance improvement for aluminum alloy used in aircraft skin [J]. Opt. Laser Technol., 2021, 133: 106531 |
| 10 | Gao W Y, Zhao S S, Wang Y B, et al. Numerical simulation of thermal field and Fe-based coating doped Ti [J]. Int. J. Heat Mass Transfer, 2016, 92: 83 |
| 11 | Manvatkar V, De A, DebRoy T. Heat transfer and material flow during laser assisted multi-layer additive manufacturing [J]. J. Appl. Phys., 2014, 116: 124905 |
| 12 | Li C, Zhang D C, Gao X, et al. Numerical simulation method of the multi-field coupling mechanism for laser cladding 316L powder [J]. Weld. World, 2022, 66: 423 |
| 13 | Wang L P, Zhang D C, Chen C Z, et al. Multi-physics field coupling and microstructure numerical simulation of laser cladding for engine crankshaft based on CA-FE method and experimental study [J]. Surf. Coat. Technol., 2022, 438: 128396 |
| 14 | He X, Mazumder J. Transport phenomena during direct metal deposition [J]. J. Appl. Phys., 2007, 101: 053113 |
| 15 | Qi H, Mazumder J, Ki H. Numerical simulation of heat transfer and fluid flow in coaxial laser cladding process for direct metal deposition [J]. J. Appl. Phys., 2006, 100: 024903 |
| 16 | Wirth F, Wegener K. A physical modeling and predictive simulation of the laser cladding process [J]. Addit. Manuf., 2018, 22: 307 |
| 17 | Li C, Yu Z B, Gao J X, et al. Numerical simulation and experimental study of cladding Fe60 on an ASTM 1045 substrate by laser cladding [J]. Surf. Coat. Technol., 2019, 357: 965 |
| 18 | Gan Z T, Yu G, He X L, et al. Numerical simulation of thermal behavior and multicomponent mass transfer in direct laser deposition of Co-base alloy on steel [J]. Int. J. Heat Mass Transfer, 2017, 104: 28 |
| 19 | Zhang T, Li H, Liu S, et al. Evolution of molten pool during selective laser melting of Ti-6Al-4V [J]. J. Phys., 2019, 52D: 055302 |
| 20 | Han L, Phatak K M, Liou F W. Modeling of laser cladding with powder injection [J]. Metall. Mater. Trans., 2004, 35B: 11390 |
| 21 | Tovar A A. Propagation of flat-topped multi-Gaussian laser beams [J]. J. Opt. Soc. Am., 2001, 18A: 18974 |
| 22 | Kaplan A F H. Analysis and modeling of a high-power Yb:fiber laser beam profile [J]. Opt. Eng., 2011, 50: 054201 |
| 23 | Wu J Z, Zhao P H, Wei H Y, et al. Development of powder distribution model of discontinuous coaxial powder stream in laser direct metal deposition [J]. Powder Technol., 2018, 340: 449 |
| 24 | Wu J Z, Liu T W, Chen H Y, et al. Simulation of laser attenuation and heat transport during direct metal deposition considering beam profile [J]. J. Mater. Process. Technol., 2019, 270: 92 |
| 25 | Wu J Z, Ren S, Zhang Y, et al. Influence of spatial laser beam profiles on thermal-fluid transport during laser-based directed energy deposition [J]. Virtual Phys. Prototy., 2021, 16: 444 |
| 26 | Gan Z T, Yu G, He X L, et al. Surface-active element transport and its effect on liquid metal flow in laser-assisted additive manufacturing [J]. Int. Commun. Heat Mass Transfer, 2017, 86: 206 |
| 27 | He X L, Song L J, Yu G, et al. Solute transport and composition profile during direct metal deposition with coaxial powder injection [J]. Appl. Surf. Sci., 2011, 258: 898 |
| 28 | Morville S, Carin M, Peyre P, et al. 2D longitudinal modeling of heat transfer and fluid flow during multilayered direct laser metal deposition process [J]. J. Laser Appl., 2012, 24: 032008 |
| 29 | Wen S Y, Shin Y C. Modeling of transport phenomena during the coaxial laser direct deposition process [J]. J. Appl. Phys., 2010, 108: 044908 |
| 30 | Ai Y W, Jiang P, Shao X Y, et al. A three-dimensional numerical simulation model for weld characteristics analysis in fiber laser keyhole welding [J]. Int. J. Heat Mass Transfer, 2017, 108: 614 |
| 31 | Knapp G L, Mukherjee T, Zuback J S, et al. Building blocks for a digital twin of additive manufacturing [J]. Acta Mater., 2017, 135: 390 |
| 32 | Wu J Z, Zheng X Q, Zhang Y, et al. Modeling of whole-phase heat transport in laser-based directed energy deposition with multichannel coaxial powder feeding [J]. Addit. Manuf., 2022, 59: 103161 |
| 33 | Promoppatum P, Yao S C, Pistorius P C, et al. A comprehensive comparison of the analytical and numerical prediction of the thermal history and solidification microstructure of Inconel 718 products made by laser powder-bed fusion [J]. Engineering, 2017, 3: 685 |
| 34 | Wei H L, Mukherjee T, Zhang W, et al. Mechanistic models for additive manufacturing of metallic components [J]. Prog. Mater. Sci., 2021, 116: 100703 |
| 35 | Debroy T, Wei H L, Zuback J S, et al. Additive manufacturing of metallic components—Process, structure and properties [J]. Prog. Mater. Sci., 2018, 92: 112 |
/
| 〈 |
|
〉 |