综述

Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展

  • 吴欣强 ,
  • 戎利建 ,
  • 谭季波 ,
  • 陈胜虎 ,
  • 胡小锋 ,
  • 张洋鹏 ,
  • 张兹瑜
展开
  • 中国科学院金属研究所 中国科学院核用材料与安全评价重点实验室 沈阳 110016
吴欣强,男,1971年生,研究员,博士
戎利建,ljrong@imr.ac.cn,主要从事核用材料研究

收稿日期: 2022-10-20

  修回日期: 2022-11-10

  网络出版日期: 2023-01-13

基金资助

国家自然科学基金项目(52271077);国家自然科学基金项目(51871218);中核集团领创科研项目及中国科学院青年创新促进会项目(2021189)

Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels

  • WU Xinqiang ,
  • RONG Lijian ,
  • TAN Jibo ,
  • CHEN Shenghu ,
  • HU Xiaofeng ,
  • ZHANG Yangpeng ,
  • ZHANG Ziyu
Expand
  • CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
RONG Lijian, professor, Tel: (024)23971979, E-mail: ljrong@imr.ac.cn

Received date: 2022-10-20

  Revised date: 2022-11-10

  Online published: 2023-01-13

Supported by

National Natural Science Foundation of China(52271077);National Natural Science Foundation of China(51871218);LingChuang Research Project of China National Nuclear Corporation, and Youth Innovation Promotion Association CAS(2021189)

摘要

结构材料是制约铅冷快堆建设的关键因素之一,原因是其组成元素在液态Pb-Bi共晶(LBE)中会发生不同程度的溶解,影响结构安全。候选结构材料铁素体/马氏体钢T91与不锈钢316在550℃饱和氧LBE环境中发生快速氧化腐蚀;溶解氧浓度降至1.26 × 10-6% (质量分数)可减轻T91的液态LBE腐蚀,但低于1 × 10-6%时,T91与316钢发生溶解腐蚀;T91液态LBE脆化敏感性高,导致其在350℃液态LBE中腐蚀疲劳寿命显著降低。与商用的(9%~12%)Cr铁素体/马氏体钢和316型奥氏体不锈钢相比,经微合金化的Si增强型铁素体/马氏体钢(9Cr-Si和12Cr-Si)和奥氏体不锈钢(ASS-Si),具有较好的组织稳定性和综合力学性能,且在液态LBE中形成的富Si氧化物提高了氧化膜的致密性,改善了其耐腐蚀性能,在550℃下静态饱和氧和动态控氧LBE环境中的溶解腐蚀受到抑制,有望满足铅冷快堆的设计需求。

本文引用格式

吴欣强 , 戎利建 , 谭季波 , 陈胜虎 , 胡小锋 , 张洋鹏 , 张兹瑜 . 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023 , 59(4) : 502 -512 . DOI: 10.11900/0412.1961.2022.00531

Abstract

Structural materials are one of the major factors that restrict the lead-cooled fast reactor construction due to metallic elements that can dissolve in the liquid lead-bismuth eutectic (LBE), which may affect the structure's safety. T91 steel and 316 stainless steel are the leading structural materials for critical equipment such as fuel cladding, reactor vessels, and reactor core internals. The environmental compatibility of those steels with the liquid LBE needs to be systematically evaluated. However, T91 steel and 316 stainless steel suffer from rapid oxidation corrosion in oxygen-saturated LBE at 550oC. T91 steel's corrosion resistance in liquid LBE can be improved by decreasing the oxygen concentration (1.26 × 10-6%, mass fraction), but dissolved corrosion occurred at dissolved oxygen concentration below 1 × 10-6% for T91 steel and 316 stainless steel. T91 steel is sensitive to liquid metal embrittlement, significantly reducing its corrosion fatigue life in the liquid LBE. Compared to the standard (9%-12%)Cr ferritic/martensitic steel and 316 stainless steel, the microalloyed Si enhanced (9%-12%)Cr ferritic/martensitic steel (9Cr-Si and 12Cr-Si) and 316 stainless steel (ASS-Si) have good microstructural stability and comprehensive mechanical properties. The Si-rich oxide formation in liquid LBE improves the oxide film compactness and corrosion resistance. The dissolution corrosion was inhibited in static oxygen-saturation and oxygen-controlled (10-6%-10-7%) flowing liquid LBE (0.3 m/s) at 550oC for 9Cr-Si, 12Cr-Si, and ASS-Si. These alloys are expected to meet the design requirements for a lead-cooled fast reactor.

参考文献

1 Was G S. Challenges to the use of ion irradiation for emulating reactor irradiation [J]. J. Mater. Res., 2015, 30: 1158
2 OECD, Nuclear Energy Agency. Handbook on lead-bismuth eutectic alloy and lead properties, materials compatibility, thermalhydraulics and technologies [R]. OECD/NEA No. 6195, 2015
3 Gong X, Short M P, Auger T, et al. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors [J]. Prog. Mater. Sci., 2022, 126: 100920
4 Zhu Z G, Zhang Q, Tan J B, et al. Corrosion behavior of T91 steel in liquid lead-bismuth eutectic at 550oC: Effects of exposure time and dissolved oxygen concentration [J]. Corros. Sci., 2022, 204: 110405
5 Yeliseyeva O, Tsisar V, Benamati G. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb-Bi melt saturated by oxygen [J]. Corros. Sci., 2008, 50: 1672
6 Martinelli L, Dufrenoy T, Jaakou K, et al. High temperature oxidation of Fe-9Cr-1Mo steel in stagnant liquid lead-bismuth at several temperatures and for different lead contents in the liquid alloy [J]. J. Nucl. Mater., 2008, 376: 282
7 Sapundjiev D, Van Dyck S, Bogaerts W. Liquid metal corrosion of T91 and A316L materials in Pb-Bi eutectic at temperatures 400-600oC [J]. Corros. Sci., 2006, 48: 577
8 Klok O, Lambrinou K, Gavrilov S, et al. Effect of deformation twinning on dissolution corrosion of 316L stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500oC [J]. J. Nucl. Mater., 2018, 510: 556
9 Kurata Y, Futakawa M, Saito S. Comparison of the corrosion behavior of austenitic and ferritic/martensitic steels exposed to static liquid Pb-Bi at 450 and 550oC [J]. J. Nucl. Mater., 2005, 343: 333
10 Tsisar V, Schroer C, Wedemeyer O, et al. Effect of structural state and surface finishing on corrosion behavior of 1.4970 austenitic steel at 400 and 500oC in flowing Pb-Bi eutectic with dissolved oxygen [J]. J. Nucl. Eng. Rad. Sci., 2018, 4: 041001
11 Schroer C, Wedemeyer O, Skrypnik A, et al. Corrosion kinetics of Steel T91 in flowing oxygen-containing lead-bismuth eutectic at 450oC [J]. J. Nucl. Mater., 2012, 431: 105
12 Tian S J. Growth and exfoliation behavior of the oxide scale on 316L and T91 in flowing liquid lead-bismuth eutectic at 480oC [J]. Oxid. Met., 2020, 93: 183
13 Kolman D G. A review of recent advances in the understanding of liquid metal embrittlement [J]. Corrosion, 2019, 75: 42
14 Gong X, Stergar E, Marmy P, et al. Tensile fracture behavior of notched 9Cr-1Mo ferritic-martensitic steel specimens in contact with liquid lead-bismuth eutectic at 350oC [J]. Mater. Sci. Eng., 2017, A692: 139
15 Wang H, Gong X, Xiao J, et al. Liquid metal embrittlement of 12Cr ferritic/martensitic steel thin-walled tubes exposed to liquid lead-bismuth eutectic [J]. Corros. Sci., 2022, 195: 110024
16 Xue B Q, Tan J B, Zhang Z Y, et al. Effect of temperature on low cycle fatigue behavior of T91 steel in liquid lead-bismuth eutectic environment at 150-550oC [J]. Int. J. Fatigue, 2023, 167: 107344
17 Gong X, Marmy P, Verlinden B, et al. Low cycle fatigue behavior of a modified 9Cr-1Mo ferritic-martensitic steel in lead-bismuth eutectic at 350oC—Effects of oxygen concentration in the liquid metal and strain rate [J]. Corros. Sci., 2015, 94: 377
18 Vogt J B, Bouquerel J, Carle C, et al. Stability of fatigue cracks at 350?oC in air and in liquid metal in T91 martensitic steel [J]. Int. J. Fatigue, 2020, 130: 105265
19 Gong X, Marmy P, Qin L, et al. Temperature dependence of liquid metal embrittlement susceptibility of a modified 9Cr-1Mo steel under low cycle fatigue in lead-bismuth eutectic at 160-450oC [J]. J. Nucl. Mater., 2016, 468: 289
20 Van Den Bosch J, Coen G, Almazouzi A, et al. Fracture toughness assessment of ferritic-martensitic steel in liquid lead-bismuth eutectic [J]. J. Nucl. Mater., 2009, 385: 250
21 Auger T, Gorse D, Hamouche-Hadjem Z, et al. Fracture mechanics behavior of the T91 martensitic steel in contact with liquid lead-bismuth eutectic for application in an accelerator driven system [J]. J. Nucl. Mater., 2011, 415: 293
22 Weisenburger A, Jianu A, An W, et al. Creep, creep-rupture tests of Al-surface-alloyed T91 steel in liquid lead bismuth at 500 and 550oC [J]. J. Nucl. Mater., 2012, 431: 77
23 Yurechko M, Schroer C, Skrypnik A, et al Creep-to-rupture of the steel P 92 at 650oC in oxygen-controlled stagnant lead in comparison to air [J]. J. Nucl. Mater., 2013, 432: 78
24 Yurechko M, Schroer C, Skrypnik A, et al. Creep-to-rupture of 12Cr- and 14Cr-ODS steels in oxygen-controlled lead and air at 650oC [J]. J. Nucl. Mater., 2014, 450: 88
25 Yurechko M, Schroer C, Wedemeyer O, et al. Creep-rupture tests on chromium-containing conventional and ODS steels in oxygen-controlled Pb and air at 650 oC[J]. Nucl. Eng. Des., 2014, 280: 686
26 Schroer C, Koch V, Wedemeyer O, et al. Silicon-containing ferritic/martensitic steel after exposure to oxygen-containing flowing lead-bismuth eutectic at 450 and 550oC [J]. J. Nucl. Mater., 2016, 469: 162
27 Shi H, Jianu A, Fetzer R, et al. Compatibility and microstructure evolution of Al-Cr-Fe-Ni high entropy model alloys exposed to oxygen-containing molten lead [J]. Corros. Sci., 2021, 189: 109593
28 Li N, Parker S S, Saleh T A, et al. Intermediate temperature corrosion behaviour of Fe-12Cr-6Al-2Mo-0.2Si-0.03Y alloy (C26M) at 300-600oC [J]. Corros. Sci., 2019, 157: 274
29 Popovic M P, Chen K, Shen H, et al. A study of deformation and strain induced in bulk by the oxide layers formation on a Fe-Cr-Al alloy in high-temperature liquid Pb-Bi eutectic [J]. Acta Mater., 2018, 151: 301
30 Kurata Y. Corrosion behavior of Si-enriched steels for nuclear applications in liquid lead-bismuth [J]. J. Nucl. Mater., 2013, 437: 401
31 Short M P, Ballinger R G, H?nninen H E. Corrosion resistance of alloys F91 and Fe-12Cr-2Si in lead-bismuth eutectic up to 715oC [J]. J. Nucl. Mater., 2013, 434: 259
32 Chen L Z, Tsisar V, Wang M, et al. Effect of oxygen on corrosion of an alumina-forming duplex steel in static liquid lead-bismuth eutectic at 550oC [J]. Corros. Sci., 2021, 189: 109591
33 Wang J, Lu S P, Rong L J, et al. Effect of silicon on the oxidation resistance of 9 wt.% Cr heat resistance steels in 550oC lead-bismuth eutectic [J]. Corros. Sci., 2016, 111: 13
34 Shi H, Wang H, Fetzer R, et al. Influence of Si addition on the corrosion behavior of 9 wt% Cr ferritic/ martensitic steels exposed to oxygen-controlled molten Pb-Bi eutectic at 550 and 600oC [J]. Corros. Sci., 2021, 193: 109871
35 Ejenstam J, Szakálos P. Long term corrosion resistance of alumina forming austenitic stainless steels in liquid lead [J]. J. Nucl. Mater., 2015, 461: 164
36 Chen S H, Rong L J. Effect of silicon on the microstructure and mechanical properties of reduced activation ferritic/martensitic steel [J]. J. Nucl. Mater., 2015, 459: 13
37 Van Den Bosch J, Coen G, Hosemann P, et al. On the LME susceptibility of Si enriched steels [J]. J. Nucl. Mater., 2012, 429: 105
38 Gong X, Sun L, Zhang F F, et al. Effect of alloying elements on liquid metal embrittlement of pure BCC Fe in contact with liquid lead-bismuth eutectic: Experiments and first principles calculation [J]. Corros. Sci., 2022, 208: 110522
39 Tan J B, Zhang Q, Wang X, et al. Slow tension and creep test device in high temperature liquid lead-bismuth environment [P]. Chin Pat, 202120775739.5, 2021
  谭季波, 张 强, 王 翔 等. 高温液态铅铋环境中的慢拉伸及蠕变试验装置 [P]. 中国专利, 202120775739.5, 2021)
40 Tan J B, Zhang Q, Wang X, et al. A fatigue test device in high temperature liquid lead-bismuth environment [P]. Chin Pat, 2021207-75649.6, 2021
  谭季波, 张 强, 王 翔 等. 一种高温液态铅铋环境中的疲劳试验装置 [P]. 中国专利, 202120775649.6, 2021)
41 Pan X, Zhang Y P, Dong Z H, et al. Effect of pre-oxidation treatment on the corrosion resistance in stagnant liquid Pb-Bi eutectic of 12Cr ferritic/martensitic steel [J]. Acta Metall. Sin., doi: 10.11900/0412.1961.2022.00267
  潘 霞, 张洋鹏, 董志宏 等. 预氧化处理对12Cr铁素体/马氏体钢耐Pb-Bi腐蚀性能的影响 [J]. 金属学报, doi: 10.11900/0412.1961.2022.00267
42 Roy A, Kumar P, Maitra D. The effect of silicon content on impact toughness of t91 grade steels [J]. J. Mater. Eng. Perform., 2009, 18: 205
43 Cabet C, Dalle F, Gaganidze E, et al. Ferritic-martensitic steels for fission and fusion applications [J]. J. Nucl. Mater., 2019, 523: 510
44 Chen S H, Xie A, Lv X L, et al. Tailoring microstructure of austenitic stainless steel with improved performance for generation-IV fast reactor application: A review [J]. Crystals, 2023, 13: 268
45 Wang Q Y, Chen S H, Rong L J. δ-Ferrite formation and its effect on the mechanical properties of heavy-section AISI 316 stainless steel casting [J]. Metall. Mater. Trans., 2020, 51A: 2998
46 Wang Q Y, Chen S H, Lv X L, et al. Role of δ-ferrite in fatigue crack growth of AISI 316 austenitic stainless steel [J]. J. Mater. Sci. Technol., 2022, 114: 7
47 Padilha A F, Rios P R. Decomposition of austenite in austenitic stainless steels [J]. ISIJ Int., 2002, 42: 325
48 Etienne A, Radiguet B, Pareige P. Understanding silicon-rich phase precipitation under irradiation in austenitic stainless steels [J]. J. Nucl. Mater., 2010, 406: 251
49 Xie A, Chen S H, Wu Y, et al. Homogenization temperature dependent microstructural evolution and mechanical properties in a Nb-stabilized cast austenitic stainless steel [J]. Mater. Charact., 2022, 194: 112384
文章导航

/