电弧熔丝增材制造2Cr13合金组织与性能各向异性行为
收稿日期: 2022-08-25
修回日期: 2022-10-17
网络出版日期: 2022-10-20
基金资助
中国博士后科学基金面上项目(2021M693230);广西自然科学基金青年项目(2021JJB160022)
Anisotropy in Microstructures and Mechanical Properties of 2Cr13 Alloy Produced by Wire Arc Additive Manufacturing
Received date: 2022-08-25
Revised date: 2022-10-17
Online published: 2022-10-20
Supported by
China Postdoctoral Science Foundation(2021M693230);Natural Science Foundation of Guangxi Province(2021JJB160022)
采用电弧熔丝增材制造(WAAM)技术进行多层单道结构2Cr13构件制备,揭示不同层间停留温度(110~550℃)下2Cr13电弧沉积件组织、性能各向异性演变规律,以实现关键工艺参数调控下力学性能主动控制。结果表明,550℃沉积件内针状马氏体因重熔碎晶呈细长外延状生长并具有略强织构取向,且于马氏体间隙处零散分布着很少量细小不规则逆变奥氏体。550℃沉积件因细晶强化获得了较高强度与硬度,但拉伸性能具有明显各向异性。110~180℃沉积件各区域间板条状马氏体虽大致沿沉积方向生长但无明显织构取向,马氏体晶粒因层间停留温度降低导致冷凝速率增加而略呈细化趋势。110~180℃沉积件因具有相近板条状马氏体组织,其力学性能较相近且呈各向同性。
葛进国 , 卢照 , 何思亮 , 孙妍 , 殷硕 . 电弧熔丝增材制造2Cr13合金组织与性能各向异性行为[J]. 金属学报, 2023 , 59(1) : 157 -168 . DOI: 10.11900/0412.1961.2022.00414
2Cr13 martensite stainless steel has been widely used for the manufacturing of surgical tools and turbine blades. Contrary to the conventional fabrication technologies, there are several remarkable advantages in the fabrication of 2Cr13 parts by adopting wire arc additive manufacturing (WAAM) technologies, such as excellent metallurgical bonding, high production efficiency, near-net-shape production, and limited environmental contamination. In this work, the effect of interlayer dwelling temperature (110-550oC) on microstructural and mechanical properties has been revealed, providing a new approach for the active control of the performances of 2Cr13 buildups produced by wire-arc additive manufacturing. The part with a dwelling temperature of 550oC was featured by elongated acicular martensite features, with a slightly enhanced fiber-like texture, along with minor fine irregular-reverse austenite structures, dispersed among martensite gaps. This special martensitic distribution was mainly caused by the grain-broken effect under the intensive thermal shock from liquid melting pool. Consequently, the enhanced tensile strength and microhardness were obtained due to grain refinement, although exhibiting an obvious anisotropy in tensile properties. The parts with dwelling temperatures of 110-180oC were characterized by relatively coarsened martensite laths, with a random texture type, within block-shaped ferrite matrix. The average martensite size was gradually refined due to the increased cooling rate by lowering interlayer temperature. The isotropic mechanical properties of all three parts (110-180oC) were similar because of the similar martensite laths.
| 1 | Ge J G, Lin J, Fu H G, et al. A spatial periodicity of microstructural evolution and anti-indentation properties of wire-arc additive manufacturing 2Cr13 thin-wall part [J]. Mater. Des., 2018, 160: 218 |
| 2 | Zhao M P, You P P, Liu M H. Pockmarks on ground surface of nitrided 2Cr13 steel [J]. Heat Treat. Met., 2020, 45(5): 176 |
| 2 | 赵明鹏, 游平平, 刘明虎. 2Cr13钢渗氮后磨削面的“麻点”问题 [J]. 金属热处理, 2020, 45(5): 176 |
| 3 | Liu X, Yang J C, Yang L, et al. Effect of Ce on inclusions and impact property of 2Cr13 stainless steel [J]. J. Iron Steel Res. Int., 2010, 17: 59 |
| 4 | Shao Y K. Effects of laser shock peening on cavitation erosion and cavitation-silt erosion resistance of 2Cr13 stainless steel [D]. Zhenjiang: Jiangsu University, 2020 |
| 4 | 邵亦锴. 激光冲击强化2Cr13不锈钢抗气蚀和空化—颗粒侵蚀行为研究 [D]. 镇江: 江苏大学, 2020 |
| 5 | Ge J G, Lin J, Long Y H, et al. Microstructural evolution and mechanical characterization of wire arc additively manufactured 2Cr13 thin-wall part [J]. J. Mater. Res. Technol., 2021, 13: 1767 |
| 6 | Javurek M, Brummayer M, Wincor R. Turbulent flow measurements in continuous steel casting mold water model [J]. Mater. Today, 2022, 62: 2581 |
| 7 | Wang H W, Zhang X Y, Tian Z P, et al. Effects of heat treatment process on microstructure, strength and toughness of 2Cr13 stainless steel [J]. Hot Work. Technol., 2020, 49(20): 124 |
| 7 | 王浩伟, 张戌有, 田志平 等. 热处理工艺对2Cr13不锈钢组织和强韧性的影响 [J]. 热加工工艺, 2020, 49(20): 124 |
| 8 | Cao J C. Research on CAD&FEM of turbine blade die forging [D]. Qinhuangdao: Yanshan University, 2006 |
| 8 | 曹竟成. 汽轮机叶片模锻工艺CAD与模锻过程有限元分析 [D]. 秦皇岛: 燕山大学, 2006 |
| 9 | Kumar N, Bhavsar H, Mahesh P V S, et al. Wire arc additive manufacturing—A revolutionary method in additive manufacturing [J]. Mater. Chem. Phys., 2022, 285: 126144 |
| 10 | Ren X L, Jiang X Q, Yuan T, et al. Microstructure and properties research of Al-Zn-Mg-Cu alloy with high strength and high elongation fabricated by wire arc additive manufacturing [J]. J. Mater. Process. Technol., 2022, 307: 117665 |
| 11 | Tomar B, Shiva S, Nath T. A review on wire arc additive manufacturing: Processing parameters, defects, quality improvement and recent advances [J]. Mater. Today, 2022, 31: 103739 |
| 12 | Xia C Y, Pan Z X, Polden J, et al. A review on wire arc additive manufacturing: Monitoring, control and a framework of automated system [J]. J. Manuf. Syst., 2020, 57: 31 |
| 13 | Sun J X, Yang K, Wang Q Y, et al. Microstructure and mechanical properties of 5356 aluminum alloy fabricated by TIG arc additive manufacturing [J]. Acta Metall. Sin., 2021, 57: 665 |
| 13 | 孙佳孝, 杨 可, 王秋雨 等. 5356铝合金TIG电弧增材制造组织与力学性能 [J]. 金属学报, 2021, 57: 665 |
| 14 | Du Z J, Li W Y, Liu J R, et al. Study on the uniformity of structure and mechanical properties of TC4-DT alloy deposited by CMT process [J]. Acta Metall. Sin., 2020, 56: 1667 |
| 14 | 杜子杰, 李文渊, 刘建荣 等. CMT增材制造TC4-DT合金组织均匀性与力学性能一致性研究 [J]. 金属学报, 2020, 56: 1667 |
| 15 | Priarone P C, Campatelli G, Catalano A R, et al. Life-cycle energy and carbon saving potential of wire arc additive manufacturing for the repair of mold inserts [J]. CIRP J. Manuf. Sci. Technol., 2021, 35: 943 |
| 16 | Hassen A A, Noakes M, Nandwana P, et al. Scaling Up metal additive manufacturing process to fabricate molds for composite manufacturing [J]. Addit. Manuf., 2020, 32: 101093 |
| 17 | Jing C C, Chen Z, Liu B, et al. Improving mechanical strength and isotropy for wire-arc additive manufactured 304L stainless steels via controlling arc heat input [J]. Mater. Sci. Eng., 2022, A845: 143223 |
| 18 | Rodideal N, Machado C M, Infante V, et al. Mechanical characterization and fatigue assessment of wire and arc additively manufactured HSLA steel parts [J]. Int. J. Fatigue, 2022, 164: 107146 |
| 19 | Ge J G, Xu R W, Wang C L, et al. Deposition structure dependence of microstructural evolution and mechanical anisotropy of H13 buildups using cold metal transfer technology [J]. J. Alloys Compd., 2022, 904: 163283 |
| 20 | Klein T, Wojcik T, Arnoldt A. A hypoeutectic Al-Ni-Mg in situ composite processed by wire-arc additive manufacturing: Phase evolution and mechanical behavior [J]. Mater. Des., 2022, 222: 111066 |
| 21 | Nagasai B P, Malarvizhi S, Balasubramanian V. Mechanical properties and microstructural characteristics of wire arc additive manufactured 308 L stainless steel cylindrical components made by gas metal arc and cold metal transfer arc welding processes [J]. J. Mater. Process. Technol., 2022, 307: 117655 |
| 22 | Krakhmalev P, Yadroitsava I, Fredriksson G, et al. In situ heat treatment in selective laser melted martensitic AISI 420 stainless steels [J]. Mater. Des., 2015, 87: 380 |
| 23 | Zhu X C, Wen S F, Wei Q S. Microstructure and mechanical properties of mould steels AISI 420 and S136 by selective laser melting manufacturing [J]. Spec. Cast. Nonferrous Alloys, 2019, 39: 506 |
| 23 | 朱学超, 文世峰, 魏青松. AISI420与S136模具钢SLM成形组织及性能 [J]. 特种铸造及有色合金, 2019, 39: 506 |
| 24 | Alvarez L F, Garcia C, Lopez V. Continuous cooling transformations in martensitic stainless steels [J]. ISIJ Int., 1994, 34: 516 |
| 25 | Fang R R, Deng N N, Zhang H B, et al. Effect of selective laser melting process parameters on the microstructure and properties of a precipitation hardening stainless steel [J]. Mater. Des., 2021, 212: 110265 |
| 26 | Deng F B, Yang G, Zhou S Y, et al. Effect of heat treatment on microstructural heterogeneity and mechanical properties of maraging steel fabricated by wire arc additive manufacturing using 4% nitrogen shielding gas [J]. Mater. Charact., 2022, 191: 112160 |
| 27 | Fang Y J, Kim M K, Zhang Y L, et al. Particulate-reinforced iron-based metal matrix composites fabricated by selective laser melting: A systematic review [J]. J. Manuf. Process., 2022, 74: 592 |
/
| 〈 |
|
〉 |