低密度Ti2AlNb基合金热轧板微观组织的热稳定性
收稿日期: 2021-07-30
修回日期: 2022-05-09
网络出版日期: 2022-08-23
基金资助
国家重点研发计划项目(2018YFB0704100);国家自然科学基金项目(51871168);西南技术工程研究所合作基金项目(HDHDW5902020102)
Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate
Received date: 2021-07-30
Revised date: 2022-05-09
Online published: 2022-08-23
Supported by
National Key Research and Development Program of China(2018YFB0704100);National Natural Science Foundation of China(51871168);Southwest Technology and Engineering Research Institute Cooperation Fund(HDHDW5902020102)
采用OM、SEM、XRD和TEM研究了低密度Ti2AlNb基合金热轧板在600~1100℃保温12 h微观组织的热稳定性。结果表明,Ti2AlNb基合金原始态热轧板主要由α2、B2以及O相组成,颗粒状的α2相分布在B2相基体中。Ti2AlNb基合金热轧板600℃保温12 h,颗粒状的α2相分布在B2相基体中,B2相基体中分布着大量细小的O相板条。随着温度的升高,合金热轧板800~900℃保温12 h的微观组织由α2、B2以及O相三相构成,α2相颗粒逐渐球化,O相板条粗化并固溶于B2相基体中。当温度升高至950℃时,B2相基体中的O相板条消失。合金热轧板在950~1000℃保温12 h形成α2 + B2两相区,α2相颗粒球化并趋向于分布在B2相基体的晶界处。当温度升高至1100℃时,合金基体为B2单相,B2晶界处分布着极少量的残留α2相颗粒。Vickes显微硬度分布结果显示,随着温度的升高,合金板材在600℃时硬度达到峰值(509 HV),这与大量细小的O相板条有关。
关键词: Ti2AlNb基合金; 相变; 轧板; 微观组织; 热稳定性
冯艾寒 , 陈强 , 王剑 , 王皞 , 曲寿江 , 陈道伦 . 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023 , 59(6) : 777 -786 . DOI: 10.11900/0412.1961.2021.00315
Multielement and multiphase intermetallic alloys based on an ordered orthorhombic (O) phase Ti2AlNb, where the presence of a long-range order superlattice structure effectively impedes the movement of dislocations and high-temperature diffusion, are a class of highly promising lightweight high-temperature structural materials for aerospace applications due to their high specific strength and superior fracture toughness. Thermal stability of microstructures in the hot rolled sheet of a low-density Ti2AlNb-based alloy has been investigated in a temperature range from 600oC to 1100oC for 12 h via OM, SEM, XRD, and TEM/STEM. The results showed that the initial Ti2AlNb-based alloy hot rolled sheet consisted of α2, B2, and O phases. Furthermore, the Ti2AlNb-based alloy hot rolled sheet at 600oC for 12 h consisted of α2, B2, and O phases, where the particle shaped α2 phase was distributed in the B2 matrix, and lath-like O phase lay inbetween the α2 particles. The spheroidization of the α2 phase started to occur along with the coarsening and solutionizing of the lath O phase in the B2 matrix at a temperature between 800oC and 900oC for 12 h, while the hot rolled Ti2AlNb-based alloy plate was still composed of α2, B2, and O phases. When the temperature reached 950oC, the O phase disappeared in the B2 matrix. Only α2 + B2 two phases were present in the hot rolled Ti2AlNb-based alloy at 950-1000oC for 12 h, where the α2 phase was spheroidized and tended to distribute surrounding B2 grain boundaries. When the temperature rose to 1100oC, the alloy contained a B2 single phase with only some residual α2 phase. Moreover, the Vickers microhardness contour vs temperature plot revealed that a peak hardness of as high as 509 HV appeared at 600oC due to the presence of numerous fine O laths.
| 1 | Banerjee D, Gogia A K, Nandi T K, et al. A new ordered orthorhombic phase in a Ti3Al-Nb alloy [J]. Acta Metall., 1988, 36: 871 |
| 2 | Banerjee D. The intermetallic Ti2AlNb [J]. Prog. Mater. Sci., 1997, 42: 135 |
| 3 | Qu S J, Feng A H, Shagiev M R, et al. Superplastic behavior of the fine-grained Ti-21Al-18Nb-1Mo-2V-0.3Si intermetallic alloy [J]. Lett. Mater., 2018, 8: 567 |
| 4 | Zhu H P, Qu S J, Qi G Y, et al. High temperature oxidation behavior of as-rolled Ti2AlNb-based alloy [J]. Chin. J. Rare Met., 2016, 40: 104 |
| 朱慧萍, 曲寿江, 祁广源 等. Ti2AlNb基合金轧板高温抗氧化性能研究 [J]. 稀有金属, 2016, 40: 104 | |
| 5 | Xiang J M, Mi G B, Qu S J, et al. Thermodynamic and microstructural study of Ti2AlNb oxides at 800oC [J]. Sci. Rep., 2018, 8: 12761 |
| 6 | Zhang Y L, Feng A H, Qu S J, et al. Microstructure and low cycle fatigue of a Ti2AlNb-based lightweight alloy [J]. J. Mater. Sci. Technol., 2020, 44: 140 |
| 7 | Feng A H, Li B B, Shen J. Recent advances on Ti2AlNb-based alloys [J]. J. Mater. Metall., 2011, 10: 30 |
| 冯艾寒, 李渤渤, 沈 军. Ti2AlNb基合金的研究进展 [J]. 材料与冶金学报, 2011, 10: 30 | |
| 8 | Shen J, Feng A H. Recent advances on microstructural controlling and hot forming of Ti2AlNb-based alloys [J]. Acta Metall. Sin., 2013, 49: 1286 |
| 沈 军, 冯艾寒. Ti2AlNb基合金微观组织调制及热成形研究进展 [J]. 金属学报, 2013, 49: 1286 | |
| 9 | Li Z J, Tian W, Li J W, et al. Application of Ti2AlNb alloy electron beam welding on aero-engine casing [J]. Gas Turbine Exp. Res., 2020, 33(3): 52 |
| 李祚军, 田 伟, 李晋炜 等. Ti2AlNb合金电子束焊接在航空发动机机匣中的应用 [J]. 燃气涡轮试验与研究, 2020, 33(3): 52 | |
| 10 | Zhang H Y, Yan N, Liang H Y, et al. Phase transformation and microstructure control of Ti2AlNb-based alloys: A review [J]. J. Mater. Sci. Technol., 2021, 80: 203 |
| 11 | Ravi C, Vajeeston P, Mathijaya S, et al. Electronic structure, phase stability, and cohesive properties of Ti2 XAl (X = Nb, V, Zr) [J]. Phys. Rev., 1999, 60B: 15683 |
| 12 | Pathak A, Singh A K. A first principles study of Ti2AlNb intermetallic [J]. Solid State Commun., 2015, 204: 9 |
| 13 | Morris M A, Morris D G. Strain localization, slip-band formation and twinning associated with deformation of a Ti-24at.%Al-11at.%Nb alloy [J]. Philos. Mag., 1991, 63A: 1175 |
| 14 | Kazantseva N V, Demakov S L, Popov A A. Microstructure and plastic deformation of orthorhombic titanium aluminides Ti2AlNb. III. Formation of transformation twins upon the B2→Ophase transformation [J]. Phys. Met. Metallogr., 2007, 103: 378 |
| 15 | Kazantseva N V, Demakov S L, Popov A A. Microstructure and plastic deformation of orthorhombic titanium aluminides Ti2AlNb. IV. Formation of the transformation twins upon the α2→O phase transformation [J]. Phys. Met. Metallogr., 2007, 103: 388 |
| 16 | Liang X B, Zhou J J, Zhang J W, et al. High cycle fatigue at high temperatures of the lamellar microstructure of Ti-22Al-25Nb alloy [J]. Titanium Ind. Prog., 2019, 36(2): 20 |
| 梁晓波, 周俊吉, 张建伟 等. 板条组织Ti-22Al-25Nb合金高温高周疲劳行为 [J]. 钛工业进展, 2019, 36(2): 20 | |
| 17 | Luo C, Zhang Y, Wang X Y, et al. Effect of heat treatment on microstructure and properties of cast Ti-22Al-25Nb alloy [J]. Aerosp. Manuf. Technol., 2020, (2): 18 |
| 骆 晨, 张 寅, 王新英 等. 热处理对铸造Ti2AlNb合金组织和力学性能的影响 [J]. 航天制造技术, 2020, (2): 18 | |
| 18 | Li B B. Plate preparation, microstructure and mechanical properties of low-density Ti2AlNb-based alloys [D]. Harbin: Harbin Institute of Technology, 2011 |
| 李渤渤. 低密度Ti2AlNb基合金板材制备及组织与力学性能研究 [D] 哈尔滨: 哈尔滨工业大学, 2011 | |
| 19 | Chen Z. Research on microstructure and mechanical properties of Ti2AlNb-based alloy fabricated by multiple isothermal forging [D]. Harbin: Harbin Institute of Technology, 2013 |
| 陈 卓. Ti2AlNb基合金多向等温锻造组织与力学性能研究 [D]. 哈尔滨: 哈尔滨工业大学, 2013 | |
| 20 | Li S Y. Phase transformation and superplasticity deformation mechanism in Ti2AlNb-based alloys [D]. Harbin: Harbin Institute of Technology, 2013 |
| 李少雨. Ti2AlNb基合金相变及超塑性变形机理研究 [D]. 哈尔滨: 哈尔滨工业大学, 2013 | |
| 21 | Zhou Y, Cao J X, Huang X, et al. Microstructure evolution and comprehensive mechanical properties of β/B2 processed Ti-22Al-23Nb-2(Mo, Zr) alloy [J]. J. Aeronaut. Mater., 2020, 40(4): 25 |
| 周 毅, 曹京霞, 黄 旭 等. β/B2锻造Ti-22Al-23Nb-2(Mo, Zr)合金的组织演化与综合力学性能 [J]. 航空材料学报, 2020, 40(4): 25 | |
| 22 | Li J J, Zeng W D, Xue C. Effects of hot deformation parameters on lamellar microstructure evolution of Ti2AlNb based alloy [J]. Chin. J. Nonferrous Met., 2014, 24: 1998 |
| 李君珺, 曾卫东, 薛 晨. 热变形参数对Ti2AlNb基合金片层组织演变的影响 [J]. 中国有色金属学报, 2014, 24: 1998 | |
| 23 | Wang S L, Zeng W D, Ma X, et al. Effect of solution temperature on microstructure of Ti-22Al-25Nb alloy [J]. Mater. Heat Treat., 2009, 38(8): 106 |
| 王邵丽, 曾卫东, 马 雄 等. 固溶温度对Ti-22Al-25Nb合金微观组织的影响 [J]. 材料热处理技术, 2009, 38(8): 106 | |
| 24 | Boehlert C J, Majumdar B S, Seetharaman V, et al. Part I. The microstructural evolution in Ti-Al-Nb O + bcc orthorhombic alloys [J]. Metall. Mater. Trans., 1999, 30A: 2305 |
| 25 | Boehlert C J. The phase evolution and microstructural stability of an orthorhombic Ti-23Al-27Nb alloy [J]. J. Phase Equilib., 1999, 20: 101 |
| 26 | Boehlert C J, Miracle D B. Part II. The creep behavior of Ti-Al-Nb O + bcc orthorhombic alloys [J]. Metall. Mater. Trans., 1999, 30A: 2349 |
| 27 | Boehlert C J. Microstructure, creep, and tensile behavior of a Ti-12Al-38Nb (at.%) beta+orthorhombic alloy [J]. Mater. Sci. Eng., 1999, A267: 82 |
| 28 | Boehlert C J. Part III. The tensile behavior of Ti-Al-Nb O + bcc orthorhombic alloys [J]. Metall. Mater. Trans., 2001, 32A: 1977 |
| 29 | Lin P, He Z B, Yuan S J, et al. Instability of the O-phase in Ti-22Al-25Nb alloy during elevated-temperature deformation [J]. J. Alloys Compd., 2013, 578: 96 |
| 30 | Bendersky L A, Boettinger W J, Roytburd A. Coherent precipitates in the b.c.c./orthorhombic two-phase field of the Ti-Al-Nb system [J]. Acta Metall. Mater., 1991, 39: 1959 |
| 31 | Muraleedharan K, Gogia A K, Nandy T K, et al. Transformations in a Ti-24Al-15Nb alloy: Part I. Phase equilibria and microstructure [J]. Metall. Trans., 1992, 23A: 401 |
| 32 | Popov A A, Illarionov A G, Grib S V, et al. Phase and structural transformations in the alloy on the basis of the orthorhombic titanium aluminide [J]. Phys. Met. Metallogr., 2008, 106: 399 |
| 33 | Kazantseva N V, Lepikhin S V. Study of the Ti-Al-Nb phase diagram [J]. Phys. Met. Metall., 2006, 102: 169 |
/
| 〈 |
|
〉 |