初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响
收稿日期: 2021-12-06
修回日期: 2022-01-09
网络出版日期: 2022-07-15
基金资助
中国博士后科学基金项目(2017M6132235)
Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy
Received date: 2021-12-06
Revised date: 2022-01-09
Online published: 2022-07-15
Supported by
China Postdoctoral Science Foundation(2017M6132235)
以镍基变形高温合金GH4096为研究对象,进行了不同组织状态下的热压缩实验,分析了该合金热变形流变行为特点,并采用OM、SEM、EBSD和TEM等手段研究了热压缩过程中初始晶粒尺寸(晶界面积和数量)和强化相对动态再结晶行为及组织演变的影响。结果表明:在1050~1120℃温度范围内,随着初始晶粒尺寸的减小,峰值流变应力降低,动态再结晶分数增加,实现完全动态再结晶所需热变形温度降低,发生动态再结晶的临界应变降低;在亚固溶温度下热变形时,动态再结晶晶粒尺寸与初始晶粒尺寸和变形量没有相关性;计算了与初始晶粒尺寸相关的热变形激活能,并建立了与热变形前的初始晶粒尺寸相关的热变形本构方程;研究了铸态组织中强化相γ'相形态对热变形行为的影响,在亚固溶温度下热变形时,随着强化相γ'相尺寸的增加,可一定程度降低热变形峰值流变应力,降低动态再结晶的临界应变,提高动态再结晶分数。分析讨论了GH4096合金不同组织状态下的主导动态软化机制。
李福林 , 付锐 , 白云瑞 , 孟令超 , 谭海兵 , 钟燕 , 田伟 , 杜金辉 , 田志凌 . 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响[J]. 金属学报, 2023 , 59(7) : 855 -870 . DOI: 10.11900/0412.1961.2021.00532
GH4096 alloy were used for disks and shafts of advanced gas turbine engines owing to its excellent properties such as resistance to creep, fatigue, and corrosion as well as microstructure stability up to about 700oC. In this study, GH4096, a hard-to-deform disk superalloy, was processed through an advanced cast and wrought route to avoid the expensive power metallurgy (P/M) route. Many types of full-scale disk forgings possessing homogeneous fine-grained microstructures were successfully carried out, and the ultrasonic inspectability was comparative to that of the alloy produced by the P/M route. The effects of the initial grain size and strengthening phase on hot deformation behavior and dynamic recrystallization (DRX) were studied by OM, SEM, EBSD, and TEM under different deformation parameters. The results showed that as the initial grain size decreased within the temperature range of 1050-1120oC, the flow peak stresses decreased and the fractions of DRX increased. With an increase in the initial grain size, the thermal deformation temperature required for complete dynamic recrystallization decreased, and also the critical strain of dynamic recrystallization decreased. The initial grain size and the strain did not affect the recrystallized grain size when deformed at a sub-solvus temperature. The thermal deformation constitutive equations related to the initial grain sizes were established and the activation energies of thermal deformation related to the original grain sizes were calculated. The effect of γ' phase size on the thermal deformation behavior in as-cast microstructure was studied. In the sub-solvus temperature range, the thermal deformation resistance could be effectively reduced with the increase in the size of γ' phase, the critical strain of DRX was decreased, and the DRX fraction was also increased. The dynamic recrystallization mechanisms related to the γ' phase and initial grain size were also discussed. DRX nucleation takes place at the sub-grains near original grain boundaries for samples with larger initial grain size deformed at sub-solvus temperature. For samples with fine initial grain size, the interface slip of incoherent γ' phase is the significant dynamic softening mechanism during the sub-solvus temperature deformation. For as-cast samples, the main dynamic softening mechanism is original grain boundary bowing out DRX nucleation and coarse second-phase-induced DRX nucleation.
| 1 | Tian W, Zhong Y, Liu Y F, et al. Development and testing of novel casted & wrought GH4096 alloy labyrinth disk [J]. Rare Met. Mater. Eng., 2021, 50: 1325 |
| 田 伟, 钟 燕, 刘砚飞 等. 新型铸&锻GH4096合金篦齿盘研制与考核 [J]. 稀有金属材料与工程, 2021, 50: 1325 | |
| 2 | Reed R C. The Superalloys Fundamentals and Applications [M]. New York: Cambridge University Press, 2006: 1 |
| 3 | Du J H, Zhao G P, Deng Q, et al. Development of wrought superalloy in China [J]. J. Aeronaut. Mater., 2016, 36(3): 27 |
| 杜金辉, 赵光普, 邓 群 等. 中国变形高温合金研制进展 [J]. 航空材料学报, 2016, 36(3): 27 | |
| 4 | Tian S F, Zhang G Q, Li Z, et al. The disk superalloys and disk manufacturing technologies for advanced aero engine [J]. J. Aeronaut. Mater., 2003, 23(suppl.1) : 233 |
| 田世藩, 张国庆, 李 周 等. 先进航空发动机涡轮盘合金及涡轮盘制造 [J]. 航空材料学报, 2003, 23(): 233 | |
| 5 | Fu R, Chen X C, Ren H, et al. Structure and hot deformation behavior of ESR-CDS René88DT [J]. J. Aeronaut. Mater., 2011, 31(3): 8 |
| 付 锐, 陈希春, 任 昊 等. 电渣重熔连续定向凝固René88DT合金的组织与热变形行为 [J]. 航空材料学报, 2011, 31(3): 8 | |
| 6 | Du J H, Lv X D, Dong J X, et al. Research progress of wrought superalloys in China [J]. Acta Metall. Sin., 2019, 55: 1115 |
| 杜金辉, 吕旭东, 董建新 等. 国内变形高温合金研制进展 [J]. 金属学报, 2019, 55: 1115 | |
| 7 | Zhang R, Liu P, Cui C Y, et al. Present research situation and prospect of hot working of cast & wrought superalloys for aero-engine turbine disk in China [J]. Acta Metall. Sin., 2021, 57: 1215 |
| 张 瑞, 刘 鹏, 崔传勇 等. 国内航空发动机涡轮盘用铸锻难变形高温合金热加工研究现状与展望 [J]. 金属学报, 2021, 57: 1215 | |
| 8 | Sellars C M, McTegart W J. On the mechanism of hot deformation [J]. Acta Metall., 1966, 14: 1136 |
| 9 | Ning Y Q, Yao Z K, Li H, et al. High temperature deformation behavior of hot isostatically pressed P/M FGH4096 superalloy [J]. Mater. Sci. Eng., 2010, A527: 961 |
| 10 | Wang Y, Shao W Z, Zhen L, et al. Tensile deformation behavior of superalloy 718 at elevated temperatures [J]. J. Alloys Compd., 2009, 471: 331 |
| 11 | Srinivasan N, Prasad Y V R K, Rao P R. Hot deformation behaviour of Mg-3Al alloy—A study using processing map [J]. Mater. Sci. Eng., 2008, A476: 146 |
| 12 | Monajati H, Taheri A K, Jahazi M, et al. Deformation characteristics of isothermally forged UDIMET 720 nickel-base superalloy [J]. Metall. Mater. Trans., 2005, 36A: 895 |
| 13 | Wu K, Liu G Q, Hu B F, et al. Effect of processing parameters on hot compressive deformation behavior of a new Ni-Cr-Co based P/M superalloy [J]. Mater. Sci. Eng., 2011, A528: 4620 |
| 14 | Mostafaei M A, Kazeminezhad M. Hot deformation behavior of hot extruded Al-6Mg alloy [J]. Mater. Sci. Eng., 2012, A535: 216 |
| 15 | Zhang M J, Li F G, Wang S Y, et al. Characterization of hot deformation behavior of a P/M nickel-base superalloy using processing map and activation energy [J]. Mater. Sci. Eng., 2010, A527: 6771 |
| 16 | Samantaray D, Mandal S, Bhaduri A K. Optimization of hot working parameters for thermo-mechanical processing of modified 9Cr-1Mo (P91) steel employing dynamic materials model [J]. Mater. Sci. Eng., 2011, A528: 5204 |
| 17 | Gu Y, Zhong Z, Yuan Y, et al. An advanced cast-and-wrought superalloy (TMW-4M3) for turbine disk applications beyond 700oC [A]. Superalloys 2012 [C]. Hoboken: Wiley, 2012: 903 |
| 18 | Ning Y Q, Yao Z K, Lei Y Y, et al. Hot deformation behavior of the post-cogging FGH4096 superalloy with fine equiaxed microstructure [J]. Mater. Charact., 2011, 62: 887 |
| 19 | Mirzadeh H, Cabrera J M, Prado J M, et al. Hot deformation behavior of a medium carbon microalloyed steel [J]. Mater. Sci. Eng., 2011, A528: 3876 |
| 20 | Ozturk U, Cabrera J M, Calvo J. High-temperature deformation of inconel 718PlusTM [J]. J. Eng. Gas Turbines Power, 2017, 139: 032101 |
| 21 | Huron E, Srivatsa S, Raymond E. Control of grain size via forging strain rate limits for R'88DT [A]. Superalloys 2000 [C]. Warrendale: TMS, 2000: 49 |
| 22 | Zhou H T, Liu R R, Liu Z C, et al. Hot deformation characteristics of GH625 and development of a processing map [J]. J. Mater. Eng. Perform., 2013, 22: 2515 |
| 23 | Wang Y, Shao W Z, Zhen L, et al. Hot deformation behavior of delta-processed superalloy 718 [J]. Mater. Sci. Eng., 2011, A528: 3218 |
| 24 | Li H Y, Gao Z H, Yin H, et al. Effects of Er and Zr additions on precipitation and recrystallization of pure aluminum [J]. Scr. Mater., 2013, 68: 59 |
| 25 | Ning Y Q, Yao Z K, Fu M W, et al. Recrystallization of the hot isostatic pressed nickel-base superalloy FGH4096: I. Microstructure and mechanism [J]. Mater. Sci. Eng., 2011, A528: 8065 |
| 26 | Fahrmann M, Suzuki A. Effect of cooling rate on gleeble hot ductility of UDIMET alloy 720 billet [A]. Superalloys 2008 [M]. Warrendale, PA: TMS, 2008: 311 |
| 27 | Wang C Y, Song X J, Zou J W, et al. Effect of original microstructure on thermal compression deformation behavior and microstructure of FGH96 alloy [J]. Hot Work. Technol., 2019, 48(11): 39 |
| 王超渊, 宋晓俊, 邹金文 等. 原始组织对FGH96合金热压缩变形行为和组织的影响 [J]. 热加工工艺, 2019, 48(11): 39 | |
| 28 | Zhang B J, Zhao G P, Zhang W Y, et al. Deformation mechanisms and microstructural evolution of γ + γ' duplex aggregates generated during thermomechanical processing of nickel-base superalloys [A]. Superalloys 2016: Proceedings of the 13th Intenational Symposium of Superalloys [C]. Warrendale, PA: TMS, 2016: 487 |
| 29 | Fu R, Li F L, Yin F J, et al. Microstructure evolution and deformation mechanisms of the electroslag refined-continuous directionally solidified (ESR-CDS?) superalloy Rene88DT during isothermal compression [J]. Mater. Sci. Eng., 2015, A638: 152 |
| 30 | Lu X D, Du J H, Deng Q, et al. Effect of slow cooling treatment on hot deformation behavior of GH4742 superalloy [J]. J. Alloys Compd., 2009, 486: 195 |
| 31 | Li F L, Fu R, Yin F J, et al. Impact of γ' (Ni3(Al, Ti)) phase on dynamic recrystallization of a Ni-based disk superalloy during isothermal compression [J]. J. Alloys Compd., 2017, 693: 1076 |
| 32 | Liu Y. Study of hot deformation behavior of Ni-Cr-W base superalloy [D]. Xi'an: Northwestern Polytechnical University, 2010 |
| 刘 毅. Ni-Cr-W基高温合金的热变形行为研究 [D]. 西安: 西北工业大学, 2010 | |
| 33 | Yuan H, Liu W C. Effect of the δ phase on the hot deformation behavior of Inconel l718 [J]. Mater. Sci. Eng., 2005, A408: 281 |
| 34 | Dehghan-manshadi A, Hodgson P D. Dependency of recrystallization mechanism to the initial grain size [J]. Metall. Mater. Trans., 2008, 39A: 2830 |
| 35 | Belyakov A, Miura H, Sakai T. Dynamic recrystallization in ultra fine-grained 304 stainless steel [J]. Scr. Mater., 2000, 43: 21 |
| 36 | Oudin A, Barnett M R, Hodgson P D. Grain size effect on the warm deformation behaviour of a Ti-IF steel [J]. Mater. Sci. Eng., 2004, A367: 282 |
| 37 | Fu R, Li F L, Yin F J, et al. Application of multiple integral forging in preparation of wrought superalloy FGH96 turbine disk [J]. Chin. J. Rare Met., 2017, 41: 113 |
| 付 锐, 李福林, 尹法杰 等. 多向整体锻造在变形FGH96合金涡轮盘制备中的应用 [J]. 稀有金属, 2017, 41: 113 | |
| 38 | Poliak E I, Jonas J J. Initiation of dynamic recrystallization in constant strain rate hot deformation [J]. ISIJ Int., 2003, 43: 684 |
| 39 | Stewart G R, Jonas J J, Montheillet F. Kinetics and critical conditions for the initiation of dynamic recrystallization in 304 stainless Steel [J]. ISIJ Int., 2004, 44: 1581 |
| 40 | Liu C, Yao Z H, Jiang H, et al. The feasibility and process control of uniform equiaxed grains by hot deformation in GH4720Li alloy with millimeter-level coarse grains [J]. Acta Metall. Sin., 2021, 57: 1309 |
| 刘 超, 姚志浩, 江 河 等. GH4720Li合金毫米级粗大晶粒热变形获得均匀等轴晶粒的可行性及工艺控制 [J]. 金属学报, 2021, 57: 1309 | |
| 41 | Forbord B, Hallem H, Ryum N, et al. Precipitation and recrystallisation in Al-Mn-Zr with and without Sc [J]. Mater. Sci. Eng., 2004, A387-389: 936 |
| 42 | Wan Z P, Wang T, Sun Y, et al. Dynamic softening mechanisms of GH4720Li alloy during hot deformation [J]. Acta Metall. Sin., 2019, 55: 213 |
| 万志鹏, 王 涛, 孙 宇 等. GH4720Li合金热变形过程动态软化机制 [J]. 金属学报, 2019, 55: 213 | |
| 43 | Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena [M]. Oxford: Elsevier Science Ltd., 1995: 1 |
/
| 〈 |
|
〉 |