Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing

  • XU Lei ,
  • TIAN Xiaosheng ,
  • WU Jie ,
  • LU Zhengguan ,
  • YANG Rui
Expand
  • 1Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China

Received date: 2021-12-28

  Revised date: 2022-02-11

  Online published: 2022-05-24

Supported by

National Science and Technology Major Project of China(J2019-VII-0005-0145);Strategic Priority Research Program of the Chinese Academy of Sciences(XDA22010102);CAS Project for Yo-ung Scientists in Basic Research(YSBR-025)

摘要

采用无坩埚感应熔炼超声气体雾化法(electrode induction melting gas atomization,EIGA)制备了Inconel 718预合金粉末,并利用SEM对合金粉末进行了表征,通过预合金粉末热等静压工艺制备了Inconel 718粉末合金坯料并测试了力学性能。研究结果表明,镍基合金Inconel 718易于制得化学成分满足要求的洁净粉末,但热等静压过程中碳化物形成元素扩散至粉末表面,并以氧化物为核心生成包含Ti和Nb的碳化物以及Ni3Nb的硬质薄膜,形成粉末高温合金的原始颗粒边界(prior particle boundaries,PPBs),使粉末合金的塑性、韧性和持久性能低于锻造合金。通过后续工艺抑制或消除热等静压过程中产生的原始颗粒边界可显著提升材料的综合力学性能。

本文引用格式

徐磊 , 田晓生 , 吴杰 , 卢正冠 , 杨锐 . 热等静压成形Inconel 718粉末合金的显微组织和力学性能[J]. 金属学报, 2023 , 59(5) : 693 -702 . DOI: 10.11900/0412.1961.2021.00586

Abstract

Inconel 718 alloy, with outstanding high-temperature resistance and mechanical properties, has been widely used in aviation fields. However, large and complex structural components are difficult to produce by traditional processes, which may lead to segregation, micropores, and Laves phases. Net-shape hot isostatic pressing (HIP) is a powder metallurgy processing technology that produces near-shape or net-shape components with the desired microstructures, properties, and cost effectiveness. In this study, Inconel 718 pre-alloyed powder was prepared using the electrode induction melting gas atomization technique, and then the pre-alloyed powder was characterized. Powder compacts were prepared by the HIP of the pre-alloyed powder, and their mechanical properties were tested. Although clean, high-quality powder can be obtained from Inconel 718 alloy due to its lower chemical reactivity compared to titanium alloys, carbide-forming elements diffuse to the powder surface during HIP. These form a hard film with the original oxide particles as nuclei, consisting of Ni3Nb and carbides of Ti and Nb. These films become prior particle boundaries (PPBs) in the obtained powder metallurgy Inconel 718 alloy, resulting in lower ductility, toughness, and stress rupture life than those of the wrought version of the alloy. Suppressing the formation of the PPBs during HIP or eliminating them via subsequent processing significantly improves the comprehensive mechanical properties of the material.

参考文献

1 Chamanfar A, Sarrat L, Jahazi M, et al. Microstructural characteristics of forged and heat treated Inconel-718 disks[J]. Mater. Des., 2013, 52: 791
2 Yeh A C, Lu K W, Kuo C M, et al. Effect of serrated grain boundaries on the creep property of Inconel 718 superalloy[J]. Mater. Sci. Eng., 2011, A530: 525
3 Baccino R, Moret F, Pellerin F, et al. High performance and high complexity net shape parts for gas turbines: The ISOPREC? powder metallurgy process[J]. Mater. Des., 2000, 21: 345
4 Samarov V, Seliverstov D, Froes F H. Fabrication of near-net shape cost-effective titanium components by use of prealloyed powder and hot isostatic pressing[A]. Powder Metallurgy[M]. Almere: ASM International, 2015: 313
5 Yang R. Advances and challenges of TiAl base alloys[J]. Acta Metall. Sin., 2015, 51: 129
  杨 锐. 钛铝金属间化合物的进展与挑战[J]. 金属学报, 2015, 51: 129
6 Xu L, Guo R P, Wu J, et al. Progress in hot isostatic pressing technology of titanium alloy powder[J]. Acta Metall. Sin., 2018, 54: 1537
  徐 磊, 郭瑞鹏, 吴 杰 等. 钛合金粉末热等静压近净成形研究进展[J]. 金属学报, 2018, 54: 1537
7 Raisson G, Guédou J Y, Guichard D, et al. Production of net-shape static parts by direct HIPing of nickel base superalloy prealloyed powders[J]. Adv. Mater. Res., 2011, 278: 277
8 Kracke A. Superalloys, the most successful alloy system of modern times - past, present and future[A]. Proceedings of the 7th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh, Pennsylvania: TMS, 2010: 13
9 Chang L T. Preparation and hot isostatic press compaction of superalloy powder with less ceramic inclusions[D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2014
  常立涛. 洁净高温合金粉末的制备及其热等静压工艺研究[D]. 沈阳: 中国科学院金属研究所, 2014
10 Habel U. Microstructure and mechanical properties of HIP PM 718[A]. Superalloys 718. 625. 706 and Various Derivatives[M]. Pittsburgh, Pennsylvania: TMS, 2001: 625
11 Rao G A, Srinivas M, Sarma D S. Effect of oxygen content of powder on microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 718[J]. Mater. Sci. Eng., 2006, A435-436: 84
12 Rao G A, Srinivas M, Sarma D S. Influence of modified processing on structure and properties of hot isostatically pressed superalloy Inconel 718[J]. Mater. Sci. Eng., 2006, A418: 282
13 Chang L T, Sun W R, Cui Y Y, et al. Influences of hot-isostatic-pressing temperature on microstructure, tensile properties and tensile fracture mode of Inconel 718 powder compact[J]. Mater. Sci. Eng., 2014, A599: 186
14 Chang L T, Sun W R, Cui Y Y, et al. Microstructure, tensile properties, and hot-working characteristics of a hot isostatic-pressed powder metallurgy superalloy[J]. Metall. Mater. Trans., 2017, 48A: 1273
15 Chang L T, Sun W R, Cui Y Y, et al. Preparation of hot-isostatic-pressed powder metallurgy superalloy Inconel 718 free of prior particle boundaries[J]. Mater. Sci. Eng., 2017, A682: 341
16 Xu L, Guo R P, Bai C G, et al. Effect of hot isostatic pressing conditions and cooling rate on microstructure and properties of Ti-6Al-4V alloy from atomized powder[J]. J. Mater. Sci. Technol., 2014, 30: 1289
17 Wu J, Guo R P, Xu L, et al. Effect of hot isostatic pressing loading route on microstructure and mechanical properties of powder metallurgy Ti2AlNb alloys[J]. J. Mater. Sci. Technol., 2017, 33: 172
18 Guo R P, Xu L, Zong B Y, et al. Preparation and ring rolling processing of large size Ti-6Al-4V powder compact[J]. Mater. Des., 2016, 99: 341
19 Rao G A, Kumar M, Srinivas M, et al. Effect of thermomechanical working on the microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 718[J]. Mater. Sci. Eng., 2004, 383: 201
20 Wu J, Xu L, Guo R P, et al. Preparation of γ-TiAl alloy from powder metallurgy route and analysis of the influence factors of mechanical properties[J]. Chin. J. Mater. Res., 2015, 29: 127
  吴 杰, 徐 磊, 郭瑞鹏 等. 粉末冶金Ti-47Al-2Cr-2Nb-0.15B合金的制备及力学性能影响因素[J]. 材料研究学报, 2015, 29: 127
21 Wu J. Densification behavior of Ti-5Al-2.5Sn ELI pre-alloyed powders under hot isostatic pressing[D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2011
  邬 军. Ti-5Al-2.5Sn ELI预合金粉末热等静压致密化行为研究[D]. 沈阳: 中国科学院金属研究所, 2011
22 Cheng W X. Investigation on densification behavior and finite element modeling of Ti-5Al-2.5Sn ELI pre-alloyed powders during HIPing[D]. Beijing: University of Chinese Academy of Science, 2013
  程文祥. Ti-5Al-2.5Sn ELI预合金粉末热等静压致密化行为与有限元模拟研究[D]. 北京: 中国科学院大学, 2013
23 Guo R P, Xu L, Bai C G, et al. Effects of can design on tensile properties of typical powder metallurgy titanium alloys[J]. Chin. J. Nonferrous Met., 2014, 24: 2050
  郭瑞鹏, 徐 磊, 柏春光 等. 包套设计对典型粉末钛合金拉伸性能的影响[J]. 中国有色金属学报, 2014, 24: 2050
24 Qiu C L. Net-shape hot isostatic pressing of a nickel-based powder superalloy[D]. Birmingham, UK: University of Birmingham, 2010
25 Lang L H, Wang G, Huang X N, et al. Shielding effect of capsules and its impact on mechanical properties of P/M aluminium alloys fabricated by hot isostatic pressing[J]. Chin. J. Nonferrous Met., 2016, 26: 261
  郎利辉, 王 刚, 黄西娜 等. 包套在铝合金粉末热等静压成形中的屏蔽效应及其对性能的影响[J]. 中国有色金属学报, 2016, 26: 261
26 Lu Z G, Wu J, Xu L, et al. Ring rolling forming and properties of Ti2AlNb special shaped ring prepared by powder metallurgy[J]. Acta Metall. Sin., 2019, 55: 729
  卢正冠, 吴 杰, 徐 磊 等. Ti2AlNb异形粉末环件的轧制成形与性能研究[J]. 金属学报, 2019, 55: 729
27 Hou J, Dong J X, Yao Z H, et al. Influences of PPB, PPB affect zone, grain boundary and phase boundary on crack propagation path for a P/M superalloy FGH4096[J]. Mater. Sci. Eng., 2018, A724: 17
28 Ingesten N G, Warren R, Winberg L. The nature and origin of previous particle boundary precipitates in P/M superalloys[A]. Proceedings of a Conference held in Liège on High Temperature Alloys for Gas Turbines 1982[C]. Belgium: Springer, 1982: 1013
文章导航

/