Preparation and Bioactivity of Micro-Nano Structure on Ti6Al4V Surface

  • GAO Han ,
  • LIU Li ,
  • ZHOU Xiaoyu ,
  • ZHOU Xinyi ,
  • CAI Wenjun ,
  • ZHOU Hongling
Expand
  • 1.Key Laboratory for Liquid-Solid Structural Evolution and Processing of Materials, Ministry of Education, Shandong University, Jinan 250061, China
    2.School of Materials Science and Engineering, Shandong University, Jinan 250061, China
GAO Han, Tel: 15194105516, E-mail: 201713597@mail.sdu.edu.cn

Received date: 2021-09-26

  Revised date: 2021-12-06

  Online published: 2022-05-09

Supported by

National College Student Innovation and Entrepreneurship Training Program(S202010422074)

摘要

基于喷砂酸蚀技术,分别采用(36%~38%)HCl (质量分数)和20%HCl∶30%H2SO4 = 1∶1 (体积比)混合酸,同时施加超声场,研究了酸蚀试剂、酸蚀时间和超声场等不同工艺参数对Ti6Al4V合金表面酸洗结构和形貌的影响规律。通过喷砂酸洗+感应加热的复合工艺,实现了Ti6Al4V合金表面微纳米多级结构的制备。结果表明,在一定时间内随酸洗时间的延长,微孔内壁的阶梯结构更加明显,超声可以加速酸蚀;在喷砂酸蚀的表面进行800℃感应加热后,表面得到了微米复合孔+纳米氧化物的多级结构,模拟体液浸泡实验表明得到的微纳米多级结构具有较高的生物活性。

本文引用格式

高晗 , 刘力 , 周笑宇 , 周心怡 , 蔡汶君 , 周泓伶 . Ti6Al4V表面微纳结构的制备及生物活性[J]. 金属学报, 2023 , 59(11) : 1466 -1474 . DOI: 10.11900/0412.1961.2021.00410

Abstract

Titanium (Ti) and its alloys have been widely used in the medical field for dental and orthopedic surgeries owing to their excellent mechanical and biological properties. However, much effort has been devoted to the surface modification on Ti-based implants for better biological response in medical applications. Bioactive layers with micro- and nano-scale structures and morphologies can increase the specific surface area of the implants and facilitate rapid osseointegration, which has shown good biological behaviors both in the laboratory and clinical setting. Sandblasting and acid-etching (SLA) technology has become one of the most commonly used surface modification processes for currently marketed dental implants, since it can be easily operated and is efficient. However, studies on etching behavior are still limited. In this study, concentrated hydrochloric acid ((36%-38%)HCl, mass fraction) and mixed diluted acid (20%HCl : 30%H2SO4 = 1 : 1, volume fraction) were used to etch Ti6Al4V, and an ultrasonic field was applied to the acid etching treatment. The influence of different etching parameters on the surface structure and morphology of Ti6Al4V was discussed, including the acid etching reagent, acid etching time, and ultrasonic field. Moreover, through the combination of SLA and induction heating treatment (IHT) oxidation, the micro- and nano-scale hierarchical structure was prepared on the surface of Ti6Al4V. The evolution of surface topography, chemistry, roughness, wettability, and bioactivity of the hierarchical structure was discussed. The micro-scale composite pores combing dozens of micron pores and several micron pores were obtained by SLA. Within a certain etching time range, with the prolonging of the etching time, the step structure on the inner wall of the micro-pores becomes more obvious, and ultrasound can accelerate the acid etching. After the IHT at 800oC, the micro- and nano-scale hierarchical surface with micro-scale composite pores and nanoscale oxide was obtained. Compared with the SLA surface, there was a decrease in surface roughness and an increase in wettability. Furthermore, after soaking in simulated body fluid (SBF) for 14 d, a homogeneous hydroxyapatite (HA) layer was formed on the micro- and nano-scale structured Ti6Al4V surface, suggesting high biological activity of the fabricated structure.

参考文献

1 Dong H Q, Guo Z M, Mao X M, et al. Prospect of development trend of melting technology of titanium and/or its alloys with high efficiency and low energy consumption [J]. Mater. Rev., 2008, 22(5):68
  董和泉, 国子明, 毛协民 等. 低能耗节约型钛及钛合金熔炼技术的发展趋势 [J]. 材料导报, 2008, 22(5): 68
2 Lin C W, Ju C P, Lin J H C. A comparison of the fatigue behavior of cast Ti-7.5Mo with c.p. titanium, Ti-6Al-4V and Ti-13Nb-13Zr alloys [J]. Biomaterials, 2005, 26: 2899
3 Zhao L C, Cui C X, Huang N. Design and performance study on two new low elastic modulus metastable β titanium alloys for biomedical application [J]. Tianjin Metall., 2009, (2): 13
  赵立臣, 崔春翔, 黄 楠. 两种新型生物医用低弹性模量亚稳β钛合金的设计与性能研究 [J]. 天津冶金, 2009, (2): 13
4 Rao S, Ushida T, Tateishi T, et al. Effect of Ti, Al, and V ions on the relative growth rate of fibroblasts (L929) and osteoblasts (MC3T3-E1) cells [J]. Bio-Med. Mater. Eng., 1996, 6: 79
5 Walker P R, LeBlanc J, Sikorska M. Effects of aluminum and other cations on the structure of brain and liver chromatin [J]. Biochemistry, 1989, 28: 3911
6 Sumitomo N, Noritake K, Hattori T, et al. Experiment study on fracture fixation with low rigidity titanium alloy: Plate fixation of tibia fracture model in rabbit [J]. J. Mater. Sci.: Mater. Med., 2008, 19: 1581
7 Ferraris S, Spriano S. Antibacterial titanium surfaces for medical implants [J]. Mater. Sci. Eng., 2016, C61: 965
8 Geetha M, Singh A K, Asokamani R, et al. Ti based biomaterials, the ultimate choice for orthopaedic implants—A review [J]. Prog. Mater. Sci., 2009, 54: 397
9 Ning C Q, Zhou Y. Development and research status of biomedical titanium alloys [J]. Mater. Sci. Technol., 2002, 10: 100
  宁聪琴, 周 玉. 医用钛合金的发展及研究现状 [J]. 材料科学与工艺, 2002, 10: 100
10 Málek J, Hnilica F, Vesely J, et al. Microstructure and mechanical properties of Ti-35Nb-6Ta alloy after thermomechanical treatment [J]. Mater. Charact., 2012, 66: 75
11 Ren B, Wan Y, Wang G S, et al. Effects of surface morphology and composition of medical titanium alloys on biocompatibility [J]. Surf. Technol., 2018, 47(4): 160
  任 冰, 万 熠, 王桂森 等. 医用钛合金表面形貌与成分对生物相容性影响研究综述 [J]. 表面技术, 2018, 47(4): 160
12 Zhao X F, Niinomi M, Nakai M, et al. Beta type Ti-Mo alloys with changeable Young's modulus for spinal fixation applications [J]. Acta Biomater., 2012, 8: 1990
13 Elahinia M H, Hashemi M, Tabesh M, et al. Manufacturing and processing of NiTi implants: A review [J]. Prog. Mater. Sci., 2012, 57: 911
14 Mendon?a G, Mendon?a D B S, Arag?o F J L, et al. Advancing dental implant surface technology—From micron- to nanotopography [J]. Biomaterials, 2008, 29: 3822
15 Jiao Y. Surface treatment and microstructure of biomedical titanium alloy [D]. Dalian: Dalian University of Technology, 2013
  焦 岩. 生物医用钛合金表面处理及其微结构 [D]. 大连: 大连理工大学, 2013
16 Liu X Y, Chu P K, Ding C X. Surface modification of titanium, titanium alloys, and related materials for biomedical applications [J]. Mater. Sci. Eng., 2004, R47: 49
17 Hung K Y, Lin Y C, Feng H P. The effects of acid etching on the nanomorphological surface characteristics and activation energy of titanium medical materials [J]. Materials, 2017, 10: 1164
18 Petersen A G, Klenerman D, Hedges W M, et al. Effect of cavitation on carbon dioxide corrosion and the development of a test for evaluating inhibitors [J]. Corrosion, 2002, 58: 216
19 Hori N, Iwasa F, Ueno T, et al. Selective cell affinity of biomimetic micro-nano-hybrid structured TiO2 overcomes the biological dilemma of osteoblasts [J]. Dent. Mater., 2010, 26: 275
20 Gittens R A, McLachlan T, Olivares-Navarrete R, et al. The effects of combined micron-/submicron-scale surface roughness and nanoscale features on cell proliferation and differentiation [J]. Biomaterials, 2011, 32: 3395
21 Li N B. Biological behaviors of micro/nano-scale bioactive oxide coatings prepared by induction heating on medical titanium and its alloys [D]. Jinan: Shandong University, 2018
  李宁波. 医用钛及钛合金表面微-纳尺度生物活性氧化膜的感应加热制备及其生物学行为 [D]. 济南: 山东大学, 2018
22 Verheul M, Drijfhout J W, Pijls B G, et al. Non-contact induction heating and SAAP-148 eliminate persisters within MRSA biofilms mimicking a metal implant infection [J]. Eur. Cell. Mater., 2021, 42: 34
23 Kokubo T, Takadama H. How useful is SBF in predicting in vivo bone bioactivity? [J]. Biomaterials, 2006, 27: 2907
24 Wang H Y, Zhu R F, Lu Y P, et al. Structures and properties of layered bioceramic coatings on pure titanium using a hybrid technique of sandblasting and micro-arc oxidation [J]. Appl. Surf. Sci., 2013, 282: 271
25 Jung S C, Lee K, Kim B H. Biocompatibility of plasma polymerized sandblasted large grit and acid titanium surface [J]. Thin Solid Films, 2012, 521: 150
26 Salda?a L, Barranco V, González-Carrasco J L, et al. Thermal oxidation enhances early interactions between human osteoblasts and alumina blasted Ti6Al4V alloy [J]. J. Biomed. Mater. Res., 2007, 81A: 334
27 Gobbato L, Arguello E, Martin I S, et al. Early bone healing around 2 different experimental, HA grit-blasted, and dual acid-etched titanium implant surfaces. A pilot study in rabbits [J]. Implant Dent., 2012, 21: 454
28 Szmukler-Moncler S, Perrin D, Ahossi V, et al. Biological properties of acid etched titanium implants: Effect of sandblasting on bone anchorage [J]. J. Biomed. Mater. Res., 2004, 68B: 149
29 Vanzillotta P S, Sader M S, Bastos I N, et al. Improvement of in vitro titanium bioactivity by three different surface treatments [J]. Dent. Mater., 2006, 22: 275
30 Le Guéhennec L, Soueidan A, Layrolle P, et al. Surface treatments of titanium dental implants for rapid osseointegration [J]. Dent. Mater., 2007, 23: 844
31 Aparicio C, Padrós A, Gil F J. In vivo evaluation of micro-rough and bioactive titanium dental implants using histometry and pull-out tests [J]. J. Mech. Behav. Biomed. Mater., 2011, 4: 1672
32 Chauhan P, Koul V, Bhatnagar N. Effect of acid etching temperature on surface physiochemical properties and cytocompatibility of Ti6Al4V ELI alloy [J]. Mater. Res. Express, 2019, 6: 105412
33 Park J Y, Davies J E. Red blood cell and platelet interactions with titanium implant surfaces [J]. Clin. Oral Implants Res., 2000, 11: 530
34 Ren B, Wan Y, Wang G S, et al. Influence of different acid-etching time on the surface morphology and corrosion resistance of TC4 titanium alloys after sandblasting [J]. J. Shandong Univ. (Eng. Sci.), 2017, 47(3): 139
  任 冰, 万 熠, 王桂森 等. 酸蚀时间对喷砂后TC4钛合金表面形貌及抗腐蚀性的影响 [J]. 山东大学学报(工学版), 2017, 47(3):139
35 Ge Y M. Preparation and properties of nano-porous film on pure medical titanium [D]. Guangzhou: South China University of Technology, 2011
  葛永梅. 医用纯钛表面纳米膜层的制备及其生物性能研究 [D]. 广州: 华南理工大学, 2011
36 Lu Y G, Song H L. Effect of ultrasonic on corrosion of zinc in hydrochloric acid [J]. J. South China Univ. Technol. (Nat. Sci. Ed.), 2011, 39(8): 77
  卢义刚, 宋恒玲. 超声波对盐酸腐蚀锌的影响 [J]. 华南理工大学学报(自然科学版), 2011, 39(8): 77
37 Ooi S K, Biggs S. Ultrasonic initiation of polystyrene latex synthesis [J]. Ultrason. Sonochem., 2000, 7: 125
38 Suslick K S, Hammerton D A, Cline R E. Sonochemical hot spot [J]. J. Am. Chem. Soc., 1986, 108: 5641
39 Rohanizadeh R, Al-Sadeq M, LeGeros R Z. Preparation of different forms of titanium oxide on titanium surface: Effects on apatite deposition [J]. J. Biomed. Mater. Res., 2004, 71A: 343
40 Paital S R, Dahotre N B. Wettability and kinetics of hydroxyapatite precipitation on a laser-textured Ca-P bioceramic coating [J]. Acta Biomater., 2009, 5: 2763
41 Li N B, Zhao X C, Geng S N, et al. Microstructures of Ti6Al4V matrices induce structural evolution of bioactive surface oxide layers via cold compression and induction heating [J]. Appl. Surf. Sci., 2021, 552: 149504
42 Wang W M, Lin S H, Li L, et al. Composition, microstructure and mechanical properties of Ti6Al4V (ELI) alloy bars for surgical implants [A]. The 14th National Titanium and Proceedings of the Titanium Alloy Academic Exchange Conference (Volume 1) [C]. Shanghai: Shanghai Scientific and Technological Literature Press, 2010: 555
  王卫民, 林劭华, 李 雷 等. 外科植入物用Ti6Al4V(ELI)合金棒材的成分、组织和力学性能 [A]. 第十四届全国钛及钛合金学术交流会论文集 (上册) [C]. 上海: 上海科学技术文献出版社, 2010: 555
43 Singhvi R, Stephanopoulos G, Wang D I C. Effects of substratum morphology on cell physiology [J]. Biotechnol. Bioeng., 1994, 43: 764
44 Kim H K, Jang J W, Lee C H. Surface modification of implant materials and its effect on attachment and proliferation of bone cells [J]. J. Mater. Sci.: Mater. Med., 2004, 15: 825
45 R?nold H J, Ellingsen J E. Effect of micro-roughness produced by TiO2 blasting—Tensile testing of bone attachment by using coin-shaped implants [J]. Biomaterials, 2002, 23: 4211
46 Ponsonnet L, Reybier K, Jaffrezic N, et al. Relationship between surface properties (roughness, wettability) of titanium and titanium alloys and cell behaviour [J]. Mater. Sci. Eng., 2003, C23: 551
47 Zhao X. Mechanism investigation on osteoblast adhesion affected by Ti6Al4V biological materials surface roughness [D]. Harbin: Harbin Institute of Technology, 2010
  赵 昕. Ti6Al4V生物材料表面粗糙度对成骨细胞黏附的影响机制研究 [D]. 哈尔滨: 哈尔滨工业大学, 2010
48 Jiang H Y, Zhang Y X, Liang A G, et al. Influencing factors and prediction model of material surface wettability [J]. Surf. Technol., 2018, 47(1): 60
  蒋华义, 张亦翔, 梁爱国 等. 材料表面润湿性的影响因素及预测模型 [J]. 表面技术, 2018, 47(1): 60
文章导航

/