纳米金属层状材料强塑性的界面调控
收稿日期: 2021-09-18
修回日期: 2021-11-05
网络出版日期: 2022-04-11
基金资助
国家自然科学基金项目(51771201);国家自然科学基金项目(52071124);河北省自然科学基金重点项目(E2021202135);天津市自然科学基金重点项目(20JCZDJC00440);东北大学轧制技术与连轧自动化国家重点实验室开放课题(2020RALKFKT002)
Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites
Received date: 2021-09-18
Revised date: 2021-11-05
Online published: 2022-04-11
Supported by
National Natural Science Foundation of China(51771201);National Natural Science Foundation of China(52071124);Key Project of Natural Science Foundation of Hebei Province(E2021202135);Key Project of Natural Science Foundation of Tianjin City(20JCZDJC00440);Open Research Fund from the State Key Laboratory of Rolling and Automation, Northeastern University(2020RALKFKT002)
纳米金属层状材料具有优异的力学性能、抗辐照损伤性能和热稳定性,在诸多领域有着广阔的应用前景。但强度的上升往往伴随着塑性的降低,如何有效地平衡层状材料强度与塑性之间的矛盾,仍是目前层状材料界面设计的巨大挑战。当层厚减小至纳米尺度,界面所占比重大幅上升,可动位错的密度急剧降低,界面成为塑性变形的源头。因此研究界面结构与其塑性变形行为之间的关系,是理解纳米层状金属材料微观变形机制及其对力学性能影响的关键。结合目前国内外纳米金属层状材料研究的最新进展,本文以常见层状材料体系为例,系统阐述了界面强化机制、界面结构、界面主导的强度及塑性变形行为和主要界面调控方法等关键科学问题,并对层状材料界面研究发展趋势进行了展望。
郑士建 , 闫哲 , 孔祥飞 , 张瑞丰 . 纳米金属层状材料强塑性的界面调控[J]. 金属学报, 2022 , 58(6) : 709 -725 . DOI: 10.11900/0412.1961.2021.00402
Nanolayered metallic composites exhibit many extraordinary properties, such as high strength, high radiation damage resistance, and good thermal stability. Therefore, it has broad potential applications in many fields. However, similar to other nanocrystalline metallic materials, the strength-ductility trade-off in nanolayered metallic composites is significant. Therefore, how to effectively balance the strength and ductility of nanolayered metallic composites is still a huge challenge in interface engineering. When the layer thickness is reduced to the nanoscale, the proportion of the interface increases substantially, and the density of mobile dislocations in grains decreases sharply, at the same time interface becomes the main source of plastic deformation. Thus, research into the relationship between the interface structure and its plastic behaviors is the key to understanding the microdeformation mechanisms of nanolayered metallic composites and their influence on mechanical properties. Based on the latest research progress, taking typical nanolayered metallic composites as examples, the key points, such as strengthening mechanisms, interface structures, plastic behaviors, and interface design methods are disscussed, and the prospects for future research trends are proposed. This review provides theoretical guidance for developing high-strength and high-ductility nanolayered metallic composites via interface engineering.
| 1 | Meyers M A, Mishra A, Benson D J. Mechanical properties of nanocrystalline materials [J]. Prog. Mater. Sci., 2005, 51: 427 |
| 2 | Antolovich S D, Armstrong R W. Plastic strain localization in metals: Origins and consequences [J]. Prog. Mater. Sci., 2014, 59: 1 |
| 3 | Zhang J Y, Lei S, Liu Y, et al. Length scale-dependent deformation behavior of nanolayered Cu/Zr micropillars [J]. Acta Mater., 2012, 60: 1610 |
| 4 | Zhang J Y, Niu J J, Zhang X, et al. Tailoring nanostructured Cu/Cr multilayer films with enhanced hardness and tunable modulus [J]. Mater. Sci. Eng., 2012, A543: 139 |
| 5 | Zhang J Y, Li J, Liang X Q, et al. Achieving optimum mechanical performance in metallic nanolayered Cu/X (X = Zr, Cr) micropillars [J]. Sci. Rep., 2014, 4: 4205 |
| 6 | Wu K, Zhang J Y, Li J, et al. Length-scale-dependent cracking and buckling behaviors of nanostructured Cu/Cr multilayer films on compliant substrates [J]. Acta Mater., 2015, 100: 344 |
| 7 | Wu K, Yuan H Z, Liang X Q, et al. Size dependence of buckling strains of Cr films, Cu films and Cu/Cr multilayers on compliant substrates [J]. Scr. Mater., 2018, 146: 1 |
| 8 | Zhang J Y, Zhang X, Wang R H, et al. Length-scale-dependent deformation and fracture behavior of Cu/X (X = Nb, Zr) multilayers: The constraining effects of the ductile phase on the brittle phase [J]. Acta Mater., 2011, 59: 7368 |
| 9 | Malow T R, Koch C C. Grain growth in nanocrystalline iron prepared by mechanical attrition [J]. Acta Mater., 1997, 45: 2177 |
| 10 | Bai X M, Voter A F, Hoagland R G, et al. Efficient annealing of radiation damage near grain boundaries via interstitial emission [J]. Science, 2010, 327: 1631 |
| 11 | Avallone J T, Nizolek T J, Bales B B, et al. Creep resistance of bulk copper-niobium composites: An inverse effect of multilayer length scale [J]. Acta Mater., 2019, 176: 189 |
| 12 | Yan Z, Liu Z R, Kong X F, et al. Effect of void morphology on void facilitated plasticity in irradiated Cu/Nb metallic nanolayered composites [J]. J. Nucl. Mater., 2022, 558: 153380 |
| 13 | Misra A, Hirth J P, Hoagland R G. Length-scale-dependent deformation mechanisms in incoherent metallic multilayered composites [J]. Acta Mater., 2005, 53: 4817 |
| 14 | Liu Y, Bufford D, Wang H, et al. Mechanical properties of highly textured Cu/Ni multilayers [J]. Acta Mater., 2011, 59: 1924 |
| 15 | Zheng S J, Beyerlein I J, Carpenter J S, et al. High-strength and thermally stable bulk nanolayered composites due to twin-induced interfaces [J]. Nat. Commun., 2013, 4: 1696 |
| 16 | Zeng L F, Gao R, Fang Q F, et al. High strength and thermal stability of bulk Cu/Ta nanolamellar multilayers fabricated by cross accumulative roll bonding [J]. Acta Mater., 2016, 110: 341 |
| 17 | Misra A, Hoagland R G, Kung H. Thermal stability of self-supported nanolayered Cu/Nb films [J]. Philos. Mag., 2004, 84: 1021 |
| 18 | Misra A, Hoagland R G. Effects of elevated temperature annealing on the structure and hardness of copper/niobium nanolayered films [J]. J. Mater. Res., 2005, 20: 2046 |
| 19 | Carpenter J S, Zheng S J, Zhang R F, et al. Thermal stability of Cu-Nb nanolamellar composites fabricated via accumulative roll bonding [J]. Philos. Mag., 2013, 93: 718 |
| 20 | Han W Z, Cerreta E K, Mara N A, et al. Deformation and failure of shocked bulk Cu-Nb nanolaminates [J]. Acta Mater., 2014, 63: 150 |
| 21 | Zhang R F, Germann T C, Liu X Y, et al. Layer size effect on the shock compression behavior of fcc-bcc nanolaminates [J]. Acta Mater., 2014, 79: 74 |
| 22 | Zhang R F, Germann T C, Wang J, et al. Role of interface structure on the plastic response of Cu/Nb nanolaminates under shock compression: Non-equilibrium molecular dynamics simulations [J]. Scr. Mater., 2013, 68: 114 |
| 23 | Demkowicz M J, Hoagland R G, Hirth J P. Interface structure and radiation damage resistance in Cu-Nb multilayer nanocomposites [J]. Phys. Rev. Lett., 2008, 100: 136102 |
| 24 | Demkowicz M J, Bellon P, Wirth B D. Atomic-scale design of radiation-tolerant nanocomposites [J]. MRS Bull., 2010, 35: 992 |
| 25 | Beyerlein I J, Caro A, Demkowicz M J, et al. Radiation damage tolerant nanomaterials [J]. Mater. Today, 2013, 16: 443 |
| 26 | Yu K Y, Sun C, Chen Y, et al. Superior tolerance of Ag/Ni multilayers against Kr ion irradiation: An in situ study [J]. Philos. Mag., 2013, 93: 3547 |
| 27 | Kashinath A, Misra A, Demkowicz M J. Stable storage of helium in nanoscale platelets at semicoherent interfaces [J]. Phys. Rev. Lett., 2013, 110: 086101 |
| 28 | Carpenter J S, Vogel S C, LeDonne J E, et al. Bulk texture evolution of Cu-Nb nanolamellar composites during accumulative roll bonding [J]. Acta Mater., 2012, 60: 1576 |
| 29 | Spitzig W A, Pelton A R, Laabs F C. Characterization of the strength and microstructure of heavily cold worked Cu/Nb composites [J]. Acta Metall., 1987, 35: 2427 |
| 30 | McKeown J, Misra A, Kung H, et al. Microstructures and strength of nanoscale Cu-Ag multilayers [J]. Scr. Mater., 2002, 46: 593 |
| 31 | Beyerlein I J, Mara N A, Bhattacharyya D, et al. Texture evolution via combined slip and deformation twinning in rolled silver-copper cast eutectic nanocomposite [J]. Int. J. Plast., 2011, 27: 121 |
| 32 | Labat S, Bocquet F, Gilles B, et al. Stresses and interfacial structure in Au-Ni and Ag-Cu metallic multilayers [J]. Scr. Mater., 2004, 50: 717 |
| 33 | Misra A, Verdier M, Lu Y C, et al. Structure and mechanical properties of Cu-X (X = Nb, Cr, Ni) nanolayered composites [J]. Scr. Mater., 1998, 39: 555 |
| 34 | Zhu X Y, Liu X J, Zong R L, et al. Microstructure and mechanical properties of nanoscale Cu/Ni multilayers [J]. Mater. Sci. Eng., 2010, A527: 1243 |
| 35 | Wang Y C, Liang F, Tan H F, et al. Enhancing fatigue strength of high-strength ultrafine-scale Cu/Ni laminated composites [J]. Mater. Sci. Eng., 2018, A714: 43 |
| 36 | Tan H F, Zhang B, Luo X M, et al. High‐cycle fatigue properties of ultrafine‐scale Cu/Ni laminated composites? [J]. Adv. Eng. Mater., 2016, 18: 2003 |
| 37 | Tran A S. Phase transformation and interface fracture of Cu/Ta multilayers: A molecular dynamics study [J]. Eng. Fract. Mech., 2020, 239: 107292 |
| 38 | Li J J, Lu W J, Zhang S Y, et al. Large strain synergetic material deformation enabled by hybrid nanolayer architectures [J]. Sci. Rep., 2017, 7: 11371 |
| 39 | Zhang J Y, Liu Y, Chen J, et al. Mechanical properties of crystalline Cu/Zr and crystal-amorphous Cu/Cu-Zr multilayers [J]. Mater. Sci. Eng., 2012, A552: 392 |
| 40 | Wu K, Wang Y Q, Yuan H Z, et al. Interfacial stress transfer mechanism of Cu-Zr amorphous films on polyimide substrates: Effect of deformation-induced devitrification [J]. J. Alloys Compd., 2019, 783: 841 |
| 41 | Mitchell T E, Lu Y C, Griffin A J, et al. Structure and mechanical properties of copper/niobium multilayers [J]. J. Am. Ceram. Soc., 1997, 80: 1673 |
| 42 | Zhang J Y, Zhang X, Liu G, et al. Scaling of the ductility with yield strength in nanostructured Cu/Cr multilayer films [J]. Scr. Mater., 2010, 63: 101 |
| 43 | Fu E G, Li N, Misra A, et al. Mechanical properties of sputtered Cu/V and Al/Nb multilayer films [J]. Mater. Sci. Eng., 2008, A493: 283 |
| 44 | Zheng S J, Wang J, Carpenter J S, et al. Plastic instability mechanisms in bimetallic nanolayered composites [J]. Acta Mater., 2014, 79: 282 |
| 45 | Zheng S J, Shao S, Zhang J, et al. Adhesion of voids to bimetal interfaces with non-uniform energies [J]. Sci. Rep., 2015, 5: 1696 |
| 46 | Ma X L, Huang C X, Moering J, et al. Mechanical properties of copper/bronze laminates: Role of interfaces [J]. Acta Mater., 2016, 116: 43 |
| 47 | Ghalandari L, Moshksar M M. High-strength and high-conductive Cu/Ag multilayer produced by ARB [J]. J. Alloys Compd., 2010, 506: 172 |
| 48 | Sun Y F, Tsuji N, Fujii H, et al. Cu/Zr nanoscaled multi-stacks fabricated by accumulative roll bonding [J]. J. Alloys Compd., 2010, 504(): S443 |
| 49 | Lee S B, LeDonne J E, Lim S C V, et al. The heterophase interface character distribution of physical vapor-deposited and accumulative roll-bonded Cu-Nb multilayer composites [J]. Acta Mater., 2012, 60: 1747 |
| 50 | Hansen B L, Carpenter J S, Sintay S D, et al. Modeling the texture evolution of Cu/Nb layered composites during rolling [J]. Int. J. Plast., 2013, 49: 71 |
| 51 | Beyerlein I J, Mayeur J R, McCabe R J, et al. Influence of slip and twinning on the crystallographic stability of bimetal interfaces in nanocomposites under deformation [J]. Acta Mater., 2014, 72: 137 |
| 52 | Beyerlein I J, Mayeur J R, Zheng S J, et al. Emergence of stable interfaces under extreme plastic deformation [J]. Proc. Natl. Acad. Sci. USA, 2014, 111: 4386 |
| 53 | Hall E O. The deformation and ageing of mild steel: III Discussion of results [J]. Proc. Phys. Soc., 1951, 64B: 747 |
| 54 | Petch N J. The cleavage strength of polycrystals [J]. J. Iron Steel Inst., 1953, 174: 25 |
| 55 | Jankowski A F, Nyakiti L O. Anomalies in Hall-Petch strengthening for nanocrystalline Au-Cu alloys below 10nm grain size [J]. Surf. Coat. Technol., 2010, 205: 1398 |
| 56 | Kim W J. Explanation for deviations from the Hall-Petch relation based on the creep behavior of an ultrafine-grained Mg-Li alloy with low diffusivity [J]. Scr. Mater., 2009, 61: 652 |
| 57 | Li N, Wang J, Misra A, et al. Direct observations of confined layer slip in Cu/Nb multilayers [J]. Microsc. Microanal., 2012, 18: 1155 |
| 58 | Bufford D, Bi Z, Jia Q X, et al. Nanotwins and stacking faults in high-strength epitaxial Ag/Al multilayer films [J]. Appl. Phys. Lett., 2012, 101: 223112 |
| 59 | Rao S I, Hazzledine P M. Atomistic simulations of dislocation-interface interactions in the Cu-Ni multilayer system [J]. Philos. Mag., 2000, 80A: 2011 |
| 60 | Koehler J S. Attempt to design a strong solid [J]. Phys. Rev., 1970, 2B: 547 |
| 61 | Beyerlein I J, Wang J, Zhang R F. Interface-dependent nucleation in nanostructured layered composites [J]. APL Mater., 2013, 1: 32112 |
| 62 | Ratheneau G W. Report of the conference on defects in crystalline solids [J]. Acta Crystallogr., 1955, 8: 855 |
| 63 | Shao S, Wang J, Misra A, et al. Spiral patterns of dislocations at nodes in (111) semi-coherent fcc interfaces [J]. Sci. Rep., 2013, 3: 2448 |
| 64 | Shao S, Wang J, Misra A. Energy minimization mechanisms of semi-coherent interfaces [J]. J. Appl. Phys., 2014, 116: 23508 |
| 65 | Zhang J Y, Lei S, Niu J, et al. Intrinsic and extrinsic size effects on deformation in nanolayered Cu/Zr micropillars: From bulk-like to small-volume materials behavior [J]. Acta Mater., 2012, 60: 4054 |
| 66 | Xiao Y Y, Kong X F, Yao B N, et al. Atomistic insight into the dislocation nucleation at crystalline/crystalline and crystalline/amorphous interfaces without full symmetry [J]. Acta Mater., 2019, 162: 255 |
| 67 | Chen Y, Shao S, Liu X Y, et al. Misfit dislocation patterns of Mg-Nb interfaces [J]. Acta Mater., 2017, 126: 552 |
| 68 | Shen X P, Yao B N, Liu Z R, et al. Mechanistic insights into interface-facilitated dislocation nucleation and phase transformation at semicoherent bimetal interfaces [J]. Int. J. Plast., 2021, 146: 103105 |
| 69 | Chen X Y, Kong X F, Misra A, et al. Effect of dynamic evolution of misfit dislocation pattern on dislocation nucleation and shear sliding at semi-coherent bimetal interfaces [J]. Acta Mater., 2018, 143: 107 |
| 70 | Saito Y, Utsunomiya H, Tsuji N, et al. Novel ultra-high straining process for bulk materials—Development of the accumulative roll-bonding (ARB) process [J]. Acta Mater., 1999, 47: 579 |
| 71 | Zheng S J, Carpenter J S, Mccabe R J, et al. Engineering interface structures and thermal stabilities via SPD processing in bulk nanostructured metals [J]. Sci. Rep., 2014, 4: 4226 |
| 72 | Zhang Y F, Li Q, Gong M, et al. Deformation behavior and phase transformation of nanotwinned Al/Ti multilayers [J]. Appl. Surf. Sci., 2020, 527: 146776 |
| 73 | Shen Z, Wagoner R H, Clark W A T. Dislocation and grain boundary interactions in metals [J]. Acta Metall., 1988, 36: 3231 |
| 74 | Lee T C, Robertson I M, Birnbaum H K. TEM in situ deformation study of the interaction of lattice dislocations with grain boundaries in metals [J]. Philos. Mag., 1990, 62A: 131 |
| 75 | Lee T C, Robertson I M, Birnbaum H K. An in situ transmission electron microscope deformation study of the slip transfer mechanisms in metals [J]. Metall. Trans., 1990, 21A: 2437 |
| 76 | Wang J. Atomistic simulations of dislocation pileup: Grain boundaries interaction [J]. JOM, 2015, 67: 1515 |
| 77 | Spearot D E, Jacob K I, McDowell D L. Nucleation of dislocations from [001] bicrystal interfaces in aluminum [J]. Acta Mater., 2005, 53: 3579 |
| 78 | Spearot D E, Jacob K I, McDowell D L. Dislocation nucleation from bicrystal interfaces with dissociated structure [J]. Int. J. Plast., 2007, 23: 143 |
| 79 | Zhang R F, Wang J, Beyerlein I J, et al. Dislocation nucleation mechanisms from fcc/bcc incoherent interfaces [J]. Scr. Mater., 2011, 65: 1022 |
| 80 | Zhang R F, Wang J, Beyerlein I J, et al. Atomic-scale study of nucleation of dislocations from fcc-bcc interfaces [J]. Acta Mater., 2012, 60: 2855 |
| 81 | Beyerlein I J, Wang J, Zhang R F. Mapping dislocation nucleation behavior from bimetal interfaces [J]. Acta Mater., 2013, 61: 7488 |
| 82 | Mara N A, Beyerlein I J. Review: Effect of bimetal interface structure on the mechanical behavior of Cu-Nb fcc-bcc nanolayered composites [J]. J. Mater. Sci., 2014, 49: 6497 |
| 83 | Wang J, Hoagland R G, Liu X Y, et al. The influence of interface shear strength on the glide dislocation-interface interactions [J]. Acta Mater., 2011, 59: 3164 |
| 84 | Wang J, Hoagland R G, Hirth J P, et al. Atomistic simulations of the shear strength and sliding mechanisms of copper-niobium interfaces [J]. Acta Mater., 2008, 56: 3109 |
| 85 | Demkowicz M J, Structure Thilly L., shear resistance and interaction with point defects of interfaces in Cu-Nb nanocomposites synthesized by severe plastic deformation [J]. Acta Mater., 2011, 59: 7744 |
| 86 | Pan Q S, Zhou H F, Lu Q H, et al. History-independent cyclic response of nanotwinned metals [J]. Nature, 2017, 551: 214 |
| 87 | Lu L, Shen Y F, Chen X H, et al. Ultrahigh strength and high electrical conductivity in copper [J]. Science, 2004, 304: 422 |
| 88 | Lu L, Chen X, Huang X, et al. Revealing the maximum strength in nanotwinned copper [J]. Science, 2009, 323: 607 |
| 89 | McCabe R J, Beyerlein I J, Carpenter J S, et al. The critical role of grain orientation and applied stress in nanoscale twinning [J]. Nat. Commun., 2014, 5: 3806 |
| 90 | Misra A, Hirth J P, Hoagland R G, et al. Dislocation mechanisms and symmetric slip in rolled nano-scale metallic multilayers [J]. Acta Mater., 2004, 52: 2387 |
| 91 | Mara N A, Tamayo T, Sergueeva A V, et al. The effects of decreasing layer thickness on the high temperature mechanical behavior of Cu/Nb nanoscale multilayers [J]. Thin Solid Films, 2006, 515: 3241 |
| 92 | Mara N A, Misra A, Hoagland R G, et al. High-temperature mechanical behavior/microstructure correlation of Cu/Nb nanoscale multilayers [J]. Mater. Sci. Eng., 2008, A493: 274 |
| 93 | Mara N A, Bhattacharyya D, Hoagland R G, et al. Tensile behavior of 40 nm Cu/Nb nanoscale multilayers [J]. Scr. Mater., 2008, 58: 874 |
| 94 | Mara N A, Bhattacharyya D, Dickerson P, et al. Deformability of ultrahigh strength 5 nm Cu/Nb nanolayered composites [J]. Appl. Phys. Lett., 2008, 92: 1765 |
| 95 | Li N, Mara N A, Wang J, et al. Ex situ and in situ measurements of the shear strength of interfaces in metallic multilayers [J]. Scr. Mater., 2012, 67: 479 |
| 96 | Han W Z, Misra A, Mara N A, et al. Role of interfaces in shock-induced plasticity in Cu/Nb nanolaminates [J]. Philos. Mag., 2011, 91: 4172 |
| 97 | Zhang R F, Beyerlein I J, Zheng S J, et al. Manipulating dislocation nucleation and shear resistance of bimetal interfaces by atomic steps [J]. Acta Mater., 2016, 113: 194 |
| 98 | Kong X F, Beyerlein I J, Liu Z R, et al. Stronger and more failure-resistant with three-dimensional serrated bimetal interfaces [J]. Acta Mater., 2019, 166: 231 |
| 99 | Han W Z, Carpenter J S, Wang J, et al. Atomic-level study of twin nucleation from face-centered-cubic/body-centered-cubic interfaces in nanolamellar composites [J]. Appl. Phys. Lett., 2012, 100: 011911 |
| 100 | Saroukhani S, Warner D H. Investigating dislocation motion through a field of solutes with atomistic simulations and reaction rate theory [J]. Acta Mater., 2017, 128: 77 |
| 101 | Wang C J, Yao B N, Liu Z R, et al. Effects of solutes on dislocation nucleation and interface sliding of bimetal semi-coherent interface [J]. Int. J. Plast., 2020, 131: 102725 |
| 102 | Subramanian P R, Perepezko J H. The Ag-Cu (silver-copper) system [J]. J. Phase Equilib., 1993, 14: 62 |
| 103 | Borovikov V, Mendelev M I, King A H. Effects of solutes on dislocation nucleation from grain boundaries [J]. Int. J. Plast., 2017, 90: 146 |
| 104 | Larché F C, Cahn J W. Overview no. 41 the interactions of composition and stress in crystalline solids [J]. Acta Metall., 1985, 33: 331 |
| 105 | Wu X B, You Y W, Kong X S, et al. First-principles determination of grain boundary strengthening in tungsten: Dependence on grain boundary structure and metallic radius of solute [J]. Acta Mater., 2016, 120: 315 |
| 106 | Lenchuk O, Rohrer J, Albe K. Cohesive strength of zirconia/molybdenum interfaces and grain boundaries in molybdenum: A comparative study [J]. Acta Mater., 2017, 135: 150 |
| 107 | Li X G, Cao L F, Zhang J Y, et al. Tuning the microstructure and mechanical properties of magnetron sputtered Cu-Cr thin films: The optimal Cr addition [J]. Acta Mater., 2018, 151: 87 |
| 108 | Gola A, Gumbsch P, Pastewka L. Atomic-scale simulation of structure and mechanical properties of Cu1 - x Ag x |Ni multilayer systems [J]. Acta Mater., 2018, 150: 236 |
| 109 | Guo W, Jägle E, Yao J H, et al. Intrinsic and extrinsic size effects in the deformation of amorphous CuZr/nanocrystalline Cu nanolaminates [J]. Acta Mater., 2014, 80: 94 |
| 110 | Fan Z, Xue S, Wang J, et al. Unusual size dependent strengthening mechanisms of Cu/amorphous CuNb multilayers [J]. Acta Mater., 2016, 120: 327 |
| 111 | Cheng B, Trelewicz J R. Design of crystalline-amorphous nanolaminates using deformation mechanism maps [J]. Acta Mater., 2018, 153: 314 |
| 112 | Bellou A, Overman C T, Zbib H M, et al. Strength and strain hardening behavior of Cu-based bilayers and trilayers [J]. Scr. Mater., 2011, 64: 641 |
| 113 | Chen Y, Li N, Hoagland R G, et al. Effects of three-dimensional Cu/Nb interfaces on strengthening and shear banding in nanoscale metallic multilayers [J]. Acta Mater., 2020, 199: 593 |
| 114 | Yang W F, Gong M Y, Yao J H, et al. Hardening induced by dislocation core spreading at disordered interface in Cu/Nb multilayers [J]. Scr. Mater., 2021, 200: 113917 |
/
| 〈 |
|
〉 |