高温低周疲劳下C-HRA-5奥氏体耐热钢中孪晶界演变
收稿日期: 2021-09-07
修回日期: 2022-01-04
网络出版日期: 2022-02-22
基金资助
安徽省自然科学基金项目(2008085ME127);安徽省高等学校自然科学研究重点项目(KJ2020A0252);山西省重大科技攻关项目(20181101014)
Twin Boundary Evolution Under Low-Cycle Fatigue of C-HRA-5 Austenitic Heat-Resistant Steel at High Temperature
Received date: 2021-09-07
Revised date: 2022-01-04
Online published: 2022-02-22
Supported by
Anhui Natural Science Foundation(2008085ME127);Natural Science Foundation of Anhui Provincial Education Department(KJ2020A0252);Key Project of Science and Technology in Shanxi Province(20181101014)
研究了先进超超临界燃煤机组用新型奥氏体耐热钢C-HRA-5在700℃低周疲劳下退孪生行为,利用SEM、EBSD和TEM等对孪晶界(TBs)的演变、退孪生机制及残留TBs对疲劳裂纹的影响进行了分析。结果表明,C-HRA-5钢经高温固溶处理后,低Σ重合位置点阵(CSL)晶界比例达到69%,以Σ3型TBs为主。在高温低周疲劳下,出现了显著的退孪生现象,且退孪生程度随着应变幅的增加而增加。退孪生机制主要与位错-TBs交互作用和TBs上相析出有关。疲劳试样中塑性变形以平面滑移为主,形成了大量的位错滑移带结构。位错滑移带循环碰撞TBs,导致晶界共格关系消失并最终退孪生。位错-TBs交互作用诱导部分TBs析出M23C6相,析出相加剧TBs对位错的钉扎作用,强化位错-TBs的交互作用,加速退孪生过程。与C-HRA-5钢中随机晶界相比,残留TBs仍然具有较高的强度,抑制疲劳裂纹的萌生与扩展。
周红伟 , 高建兵 , 沈加明 , 赵伟 , 白凤梅 , 何宜柱 . 高温低周疲劳下C-HRA-5奥氏体耐热钢中孪晶界演变[J]. 金属学报, 2022 , 58(8) : 1013 -1023 . DOI: 10.11900/0412.1961.2021.00385
C-HRA-5 steel is a new type of austenitic heat-resistant steel with excellent oxidation resistance and corrosion resistance, and high endurance strength at high temperatures. This steel can be used in superheaters and reheaters applied in 630-700oC advanced ultrasupercritical fossil-fired power plants, which is of great strategic significance to realize national energy savings and emission reduction targets. Detwinning often occurs in austenitic stainless steel when high-temperature fatigue and creep set in. However, the detwinning mechanism in C-HRA-5 steel during high-temperature fatigue and its influence on fatigue crack initiation and propagation remain unclear. Therefore, in this work, the detwinning behavior of C-HRA-5 steel under strain-controlled low-cycle fatigue (LCF) was studied at 700oC. The evolution of twin boundaries (TBs), detwinning mechanism, and influence of residual TBs on fatigue cracks were analyzed using SEM, EBSD, and TEM. After solution treatment at high temperatures, the fraction of low coincidence site lattice boundaries reached 69% in C-HRA-5 steel with dominant Σ3-type TBs. There was a remarkable detwinning effect under LCF loading. The degree of detwinning increased with increasing strain amplitude ranging from 0.3% to 0.7%. The detwinning mechanism was mainly related to the interactions at the dislocation TBs and precipitation of M23C6 at TBs. The plastic deformation of C-HRA-5 steel was dominated by planar slip under LCF loading, which resulted in dislocation gliding on particular planes. Therefore, numerous dislocation slip bands were formed. The collision of dislocation slip bands with TBs changed the coherent orientation of TBs and eventually led to detwinning. Meanwhile, the dislocation-TBs interaction induced the precipitation of M23C6 carbide at some TBs during LCF at 700oC, which strengthened the pinning of TBs on dislocations, thus accelerating the detwinning process. The residual TBs had higher strength than random grain boundaries and could inhibit the initiation and propagation of fatigue cracks.
Key words: austenitic heat-resistant steel; low-cycle fatigue; detwinning; EBSD; fatigue crack
| 1 | Liu Z D, Chen Z Z, He X K, et al. Systematical innovation of heat resistant materials used for 630-700oC advanced ultra-supercritical (A-USC) fossil fired boilers [J]. Acta Metall. Sin., 2020, 56: 539 |
| 1 | 刘正东, 陈正宗, 何西扣 等. 630~700℃超超临界燃煤电站耐热管及其制造技术进展 [J]. 金属学报, 2020, 56: 539 |
| 2 | Fang X D, Bao H S, Li Y, et al. Development of model heat resisting seamless tube C-HRA-5 for ultra-supercritical power plant boiler [J]. Iron Steel, 2020, 55(2): 119 |
| 2 | 方旭东, 包汉生, 李 阳 等. 超超临界锅炉用新型耐热无缝管C-HRA-5的开发 [J]. 钢铁, 2020, 55(2): 119 |
| 3 | Zhu C Z, Yuan Y, Yin H F, et al. Research progress of austenitic heat resistant steel Sanicro 25 used in ultra supercritical unit [J]. Mater. Rev., 2017, 31(13): 78 |
| 3 | 朱传志, 袁 勇, 尹宏飞 等. 超超临界机组用Sanicro 25耐热钢研究进展 [J]. 材料导报, 2017, 31(13): 78 |
| 4 | Wang L, Fang X D, Wang J, et al. The precipitation control of grain boundary M23C6 phases and the ductility improvement in aged 22Cr-25Ni-WCuNbN austenitic stainless steel by Co addition [J]. Mater. Lett., 2020, 264: 127348 |
| 5 | Hu C L, Xia S, Li H, et al. Effect of grain boundary network on the intergranular stress corrosion cracking of 304 stainless steel [J]. Acta Metall. Sin., 2011, 47: 939 |
| 5 | 胡长亮, 夏 爽, 李 慧 等. 晶界网络特征对304不锈钢晶间应力腐蚀开裂的影响 [J]. 金属学报, 2011, 47: 939 |
| 6 | Trillo E A, Murr L E. TEM investigation of M23C6 carbide precipitation behaviour on varying grain boundary misorientations in 304 stainless steels [J]. J. Mater. Sci., 1998, 33: 1263 |
| 7 | Shi F, Gao R H, Guan X J, et al. Application of grain boundary engineering to improve intergranular corrosion resistance in a Fe-Cr-Mn-Mo-N high-nitrogen and nickel-free austenitic stainless steel [J]. Acta Metall. Sin. (Engl. Lett.), 2020, 33: 789 |
| 8 | Guan X J, Shi F, Jia Z P, et al. Grain boundary engineering of AL6XN super-austenitic stainless steel: distinctive effects of planar-slip dislocations and deformation twins [J]. Mater. Charact., 2020, 170: 110689 |
| 9 | Yang H, Xia S, Zhang Z L, et al. Improving the intergranular corrosion resistance of the weld heat-affected zone by grain boundary engineering in 304 austenitic stainless steel [J]. Acta Metall. Sin., 2015, 51: 333 |
| 9 | 杨 辉, 夏 爽, 张子龙 等. 晶界工程对于改善304奥氏体不锈钢焊接热影响区耐晶间腐蚀性能的影响 [J]. 金属学报, 2015, 51: 333 |
| 10 | Ren S, Sun Z Y, Xu Z Z, et al. Effects of twins and precipitates at twin boundaries on Hall-Petch relation in high nitrogen stainless steel [J]. J. Mater. Res., 2018, 33: 1764 |
| 11 | Mahajan S, Pande C S, Imam M A, et al. Formation of annealing twins in f.c.c. crystals [J]. Acta Mater., 1997, 45: 2633 |
| 12 | Zhang Z F, Shao C W, Wang B, et al. Tensile and fatigue properties and deformation mechanisms of twinning-induced plasticity steels [J]. Acta Metall. Sin., 2020, 56: 476 |
| 12 | 张哲峰, 邵琛玮, 王 斌 等. 孪生诱发塑性钢拉伸与疲劳性能及变形机制 [J]. 金属学报, 2020, 56: 476 |
| 13 | Lall A, Sarkar S, Ding R G, et al. Performance of Alloy 709 under creep-fatigue at various dwell times [J]. Mater. Sci. Eng., 2019, A761: 138028 |
| 14 | Hong H U, Rho B S, Nam S W. Correlation of the M23C6 precipitation morphology with grain boundary characteristics in austenitic stainless steel [J]. Mater. Sci. Eng., 2001, A318: 285 |
| 15 | Sakaguchi N, Ohguchi Y, Shibayama T, et al. Surface cracking on Σ3, Σ9 CSL and random grain boundaries in helium implanted 316L austenitic stainless steel [J]. J. Nucl. Mater., 2013, 432: 23 |
| 16 | Guan X J, Shi F, Ji H M, et al. A possibility to synchronously improve the high-temperature strength and ductility in face-centered cubic metals through grain boundary engineering [J]. Scr. Mater., 2020, 187: 216 |
| 17 | Zhang X Y, Li D F, Guo S L, et al. Influence of annealing time on Σ3 boundary and Σ9 boundary evolutions in hastelloy C-276 Alloy [J]. Rare Met. Mater. Eng., 2016, 45: 2253 |
| 18 | Zheng H F, Shi M J, Mao Q, et al. Chromium concentration near grain boundaries with various characters in Inconel alloy 600 [J]. Chin. J. Mater. Res., 2020, 34: 511 |
| 18 | 郑合凤, 师梦杰, 毛 强 等. Inconel 600合金中不同类型晶界处铬的浓度 [J]. 材料研究学报, 2020, 34: 511 |
| 19 | Li H Z, Jing H Y, Xu L Y, et al. Microstructure mechanism, cyclic deformation behavior of an Fe-Ni-Cr alloy considering non-masing behavior [J]. Int. J. Fatigue, 2019, 127: 537 |
| 20 | Sarkar A, Dash M K, Nagesha A, et al. EBSD based studies on various modes of cyclic deformation at 923?K in a type 316LN stainless steel [J]. Mater. Sci. Eng., 2018, A723: 229 |
| 21 | Zhang P, Zhang Z J, Li L L, et al. Twin boundary: Stronger or weaker interface to resist fatigue cracking? [J]. Scr. Mater., 2012, 66: 854 |
| 22 | Wang J, Li N, Anderoglu O, et al. Detwinning mechanisms for growth twins in face-centered cubic metals [J]. Acta Mater., 2010, 58: 2262 |
| 23 | Bai J S, Lu Q H, Lu L. Detwinning behavior induced by local shear strain in nanotwinned Cu [J]. Acta Metall. Sin., 2016, 52: 491 |
| 23 | 白敬胜, 卢秋虹, 卢 磊. 纳米孪晶Cu中局部剪切应变诱导的退孪生行为 [J]. 金属学报, 2016, 52: 491 |
| 24 | Li Q, Song J, Liu G S, et al. Migration kinetics of twinning disconnections in nanotwinned Cu: An in situ HRTEM deformation study [J]. Scripta Mater., 2021, 194: 113621 |
| 25 | Ni S, Liao X Z, Zhu Y T. Effect of severe plastic deformation on the structure and mechanical properties of bulk nanocrystalline metals [J]. Acta Metall. Sin., 2014, 50: 156 |
| 25 | 倪 颂, 廖晓舟, 朱运田. 剧烈塑性变形对块体纳米金属材料结构和力学性能的影响 [J]. 金属学报, 2014, 50: 156 |
| 26 | He W J, Hu R. Portevin-Le Chatelier effect, twinning-detwinning and disordering in an aged Ni-Cr-Mo alloy during large plastic deformation [J]. Mater. Sci. Eng., 2021, A803: 140506 |
| 27 | Zhou H W, Zhang H Y, Bai F M, et al. Planar dislocation structure during creep-fatigue interactions of TP347H heat-resistant austenitic steel at 600oC [J]. Mater. Sci. Eng., 2020, A779: 139141 |
| 28 | Jang M H, Kang J Y, Jang J H, et al. Microstructure control to improve creep strength of alumina-forming austenitic heat-resistant steel by pre-strain [J]. Mater. Charact., 2018, 137: 1 |
| 29 | Heczko M, Polák J, Kruml T. Microstructure and dislocation arrangements in Sanicro 25 steel fatigued at ambient and elevated temperatures [J]. Mater. Sci. Eng., 2017, A680: 168 |
| 30 | Guo Q Y, Li Y M, Chen B, et al. Effect of high-temperature ageing on microstructure and creep properties of S31042 heat-resistant steel [J]. Acta Metall. Sin., 2021, 57: 82 |
| 30 | 郭倩颖, 李彦默, 陈 斌 等. 高温时效处理对S31042耐热钢组织和蠕变性能的影响 [J]. 金属学报, 2021, 57: 82 |
| 31 | Zhou R Y, Zhu L H, Liu Y Y, et al. Precipitates and precipitation strengthening of sanicro 25 welded joint base metal crept at 973 K [J]. Steel Res. Int., 2017, 88: 1600414 |
| 32 | Peng Z F, Ren W, Yang C, et al. Relationship between the evolution of phase parameters of grain boundary M23C6 and embrittlement of HR3C super-heater tubes in service [J]. Acta Metall. Sin., 2015, 51: 1325 |
| 32 | 彭志方, 任 文, 杨 超 等. HR3C钢运行过热器管的脆化与晶界M23C6相参量演化的关系 [J]. 金属学报, 2015, 51: 1325 |
| 33 | Zhang Z, Hu Z F, Tu H Y, et al. Microstructure evolution in HR3C austenitic steel during long-term creep at 650oC [J]. Mater. Sci. Eng., 2017, A681: 74 |
| 34 | Zhao W, Zhou H W, Fang L W, et al. Study on diversified carbide precipitation in high-strength low-alloy steel during tempering [J]. Steel Res. Int., 2021, 92: 2000723 |
| 35 | Kaneko K, Fukunaga T, Yamada K, et al. Formation of M23C6-type precipitates and chromium-depleted zones in austenite stainless steel [J]. Scr. Mater., 2011, 65: 509 |
| 36 | Wen H Y, Zhao B B, Dong X P, et al. How big is the difference between precipitation at twin boundary and normal grain boundary in an alumina-forming austenitic steel during creep at 700oC? [J]. Mater. Lett., 2020, 274: 128019 |
| 37 | Calmunger M, Chai G C, Eriksson R, et al. Characterization of austenitic stainless steels deformed at elevated temperature [J]. Metall. Mater. Trans., 2017, 48A: 4525 |
| 38 | Zhou H W, Bai F M, Yang L, et al. Mechanism of dynamic strain aging in a niobium-stabilized austenitic stainless steel [J]. Metall. Mater. Trans., 2018, 49A: 1202 |
| 39 | Zhou H W, He Y Z, Cui M, et al. Dependence of dynamic strain ageing on strain amplitudes during the low-cycle fatigue of TP347H austenitic stainless steel at 550oC [J]. Int. J. Fatigue, 2013, 56: 1 |
| 40 | Song T, Wang Z W. Microstructure and properties of TP347HFG steel after high temperature service [J]. Heat Treat. Met., 2020, 45(4): 60 |
| 40 | 宋 涛, 王志武. 高温服役后TP347HFG钢的组织与性能 [J]. 金属热处理, 2020, 45(4): 60 |
/
| 〈 |
|
〉 |