研究论文

电弧增材制造2024铝合金的微观组织与力学性能

  • 吴东江 ,
  • 刘德华 ,
  • 张子傲 ,
  • 张逸伦 ,
  • 牛方勇 ,
  • 马广义
展开
  • 大连理工大学 高性能精密制造全国重点实验室 大连 116024
吴东江,男,1964年生,教授,博士
马广义,gyma@dlut.edu.cn,主要从事激光增材制造、激光精密加工技术与装备研究

收稿日期: 2021-07-30

  修回日期: 2021-09-25

  网络出版日期: 2022-02-14

基金资助

中央高校基本科研业务费专项资金项目(DUT21YG116)

Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing

  • WU Dongjiang ,
  • LIU Dehua ,
  • ZHANG Ziao ,
  • ZHANG Yilun ,
  • NIU Fangyong ,
  • MA Guangyi
Expand
  • State Key Laboratory of High-Performance Precision Manufacturing, Dalian University of Technology, Dalian 116024, China
MA Guangyi, professor, Tel:(0411)84707625, E-mail: gyma@dlut.edu.cn

Received date: 2021-07-30

  Revised date: 2021-09-25

  Online published: 2022-02-14

Supported by

Fundamental Research Funds for the Central Universities(DUT21YG116)

摘要

采用电弧增材制造工艺制备了三元Al-Cu-Mg (2024)铝合金成形试样,并对试样的晶粒形貌、物相组成、元素分布与力学性能进行研究。结果表明,2024铝合金成形试样宏观上表现出层状特征,单一沉积层可以分为层间区域与层中区域2部分,晶粒形貌由层中区域的等轴晶转变为层间区域的柱状晶;成形试样微观组织主要包括α-Al、θ-Al2Cu与S-Al2CuMg相;由于增材制造非平衡凝固过程,成形试样出现元素偏析,层中区域Mg元素在Al基体中均匀分布;电弧重熔作用下,层间区域元素偏析严重,Cu元素以共晶组织的形式在晶界偏析,Mg元素出现局部富集;成形试样的平均抗拉强度、屈服强度与断后伸长率分别为(323.5 ± 6.6) MPa、(178.7 ± 6.2) MPa和(9.03 ± 0.67)%,高于铸造退火态2024铝合金的力学性能;由于微观组织的不同,层中区域与层间区域出现不同的裂纹扩展行为,层间区域裂纹沿着共晶组织分布路径扩展,表现为沿晶断裂,层中区域裂纹扩展模式变为穿晶断裂。

本文引用格式

吴东江 , 刘德华 , 张子傲 , 张逸伦 , 牛方勇 , 马广义 . 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023 , 59(6) : 767 -776 . DOI: 10.11900/0412.1961.2021.00314

Abstract

Owing to its outstanding advantages, such as low specific gravity, high specific strength, and good machinability, 2024 aluminum alloy has been used as various load components in the aerospace field and has become an important lightweight material. The properties of the 2024 aluminum alloy are highly correlated with its microstructures. Accordingly, in this study, 2024 aluminum alloy deposited specimens were fabricated using wire arc additive manufacturing. Further, the microstructures and mechanical properties of the deposited specimens were investigated in different regions. The layered characteristics could be observed macroscopically in the deposited specimens, and a single deposition layer was divided into two regions: interlayer and innerlayer. The grain morphology changed from equiaxed grains in the innerlayer region to columnar grains in the interlayer region. The deposited specimens mainly included α-Al, θ-Al2Cu, and S-Al2CuMg phases. In the nonequilibrium solidification process of additive manufacturing, the deposited specimens presented element segregation. The distribution of Mg in the Al matrix was uniform for the innerlayer region. However, Cu was segregated as eutectics at the grain boundary in the interlayer region. The average tensile strength, yield strength, and elongation of deposited specimens were (323.5 ± 6.6) MPa, (178.7 ± 6.2) MPa, and (9.03 ± 0.67)%, respectively, which were higher than those of cast annealing 2024 aluminum alloy. Owing to the difference in the microstructure, the innerlayer and interlayer regions showed different crack propagation behavior. The cracks in the interlayer region propagated along the distribution path of eutectics, showing intergranular fracture, and the crack propagation mode in the innerlayer region changed to transgranular fracture.

参考文献

1 Starke E A, Staley J T. Application of modern aluminum alloys to aircraft [J]. Prog. Aeosp. Sci., 1996, 32: 131
2 Zhang X M, Deng Y L, Zhang Y. Development of high strength aluminum alloys and processing techniques for the materials [J]. Acta Metall. Sin., 2015, 51: 257
  张新明, 邓运来, 张 勇. 高强铝合金的发展及其材料的制备加工技术 [J]. 金属学报, 2015, 51: 257
3 Ren Y M, Lin X, Fu X, et al. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming [J]. Acta Mater., 2017, 132: 82
4 Li Q, Wang F D, Wang G Q, et al. Wire and arc additive manufacturing of lightweight metal components in aeronautics and astronautics [J]. Aeron. Manuf. Technol., 2018, 61(3): 74
  李 权, 王福德, 王国庆 等. 航空航天轻质金属材料电弧熔丝增材制造技术 [J]. 航空制造技术, 2018, 61(3): 74
5 Gu D D, Zhang H M, Chen H Y, et al. Laser additive manufacturing of high-performance metallic aerospace components [J]. Chin. J. Lasers, 2020, 47: 0500002
  顾冬冬, 张红梅, 陈洪宇 等. 航空航天高性能金属材料构件激光增材制造 [J]. 中国激光, 2020, 47: 0500002
6 Herzog D, Seyda V, Wycisk E, et al. Additive manufacturing of metals [J]. Acta Mater., 2016, 117: 371
7 Sun J X, Yang K, Wang Q Y, et al. Microstructure and mechanical properties of 5356 aluminum alloy fabricated by TIG arc additive manufacturing [J]. Acta Metall. Sin., 2021, 57: 665
  孙佳孝, 杨 可, 王秋雨 等. 5356铝合金TIG电弧增材制造组织与力学性能 [J]. 金属学报, 2021, 57: 665
8 Yang G, Peng H J, Li C F, et al. Microstructure and mechanical property research on wire + arc additive manufactured 5356-aluminum alloy [J]. Chin. J. Rare Met., 2020, 44: 249
  杨 光, 彭晖杰, 李长富 等. 电弧增材制造5356铝合金的组织与性能研究 [J]. 稀有金属, 2020, 44: 249
9 Li C D, Gu H M, Wang W, et al. Microstructure and properties of ZL114A aluminum alloy prepared by wire arc additive manufacturing [J]. Rare Met. Mater. Eng., 2019, 48: 2917
  李承德, 顾惠敏, 王 伟 等. 电弧增材制造ZL114A铝合金的组织与性能 [J]. 稀有金属材料与工程, 2019, 48: 2917
10 Gu J L, Ding J L, Williams S W, et al. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys [J]. J. Mater. Process. Technol., 2016, 230: 26
11 Gu J L, Ding J L, Williams S W, et al. The strengthening effect of inter-layer cold working and post-deposition heat treatment on the additively manufactured Al-6.3Cu alloy [J]. Mater. Sci. Eng., 2016, A651: 18
12 Cong B Q, Ding J L, Williams S. Effect of arc mode in cold metal transfer process on porosity of additively manufactured Al-6.3%Cu alloy [J]. Int. J. Adv. Manuf. Technol., 2015, 76: 1593
13 Gu J L, Ding J L, Cong B Q, et al. The influence of wire properties on the quality and performance of wire + arc additive manufactured aluminium parts [J]. Adv. Mater. Res., 2014, 1081: 210
14 Cong B Q, Sun H Y, Peng P, et al. Porosity control of wire + arc additively manufactured Al-6.3Cu alloy deposition using AC-GTAW process [J]. Rare Met. Mater. Eng., 2017, 46: 1359
  从保强, 孙红叶, 彭 鹏 等. Al-6.3Cu AC-GTAW电弧增材成形的气孔控制 [J]. 稀有金属材料与工程, 2017, 46: 1359
15 Weingarten C, Buchbinder D, Pirch N, et al. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg [J]. J. Mater. Process. Technol., 2015, 221: 112
16 Bai J Y, Fan C L, Yang Y C, et al. Microstructures of 2219-Al thin-walled parts produced by shaped metal deposition [J]. Trans. China Weld. Inst., 2016, 37(6): 124
  柏久阳, 范成磊, 杨雨晨 等. 2219铝合金TIG填丝堆焊成形薄壁试样组织特征 [J]. 焊接学报, 2016, 37(6): 124
17 Ahuja B, Karg M, Nagulin K Y, et al. Fabrication and characterization of high strength Al-Cu alloys processed using laser beam melting in metal powder bed [J]. Phys. Procedia, 2014, 56: 135
18 Prashanth K G, Scudino S, Klauss H J, et al. Microstructure and mechanical properties of Al-12Si produced by selective laser melting: Effect of heat treatment [J]. Mater. Sci. Eng., 2014, A590: 153
19 Qian M, Cao P, Easton M A, et al. An analytical model for constitutional supercooling-driven grain formation and grain size prediction [J]. Acta Mater., 2010, 58: 3262
20 Chakraborty S, Sarkar S, Dutta P. Effect of constitutional supercooling on the numerical solution of species concentration distribution in laser surface alloying [J]. Metall. Mater. Trans., 2001, 32B: 969
21 Hunt J D. Steady state columnar and equiaxed growth of dendrites and eutectic [J]. Mater. Sci. Eng., 1984, 65: 75
22 Chen F Y, Jie W Q. Study of microsegregation in Al-Cu-Zn ternary alloys by experiment and scheil model [J]. Acta Metall. Sin., 2004, 40: 664
  陈福义, 介万奇. Al-Cu-Zn合金微观偏析的实验和Scheil模型研究 [J]. 金属学报, 2004, 40: 664
23 Bocklund B, Bobbio L D, Otis R A, et al. Experimental validation of Scheil-Gulliver simulations for gradient path planning in additively manufactured functionally graded materials [J]. Materialia, 2020, 11: 100689
24 Shi D K. Fundamentals of Materials Science [M]. 2nd Ed., Beijing: China Machine Press, 2003: 232
  石德珂. 材料科学基础 [M]. 第 2版, 北京: 机械工业出版社, 2003: 232
25 Marlaud T, Deschamps A, Bley F, et al. Influence of alloy composition and heat treatment on precipitate composition in Al-Zn-Mg-Cu alloys [J]. Acta Mater., 2010, 58: 248
26 Bai J Y, Fan C L, Lin S B, et al. Effects of thermal cycles on microstructure evolution of 2219-Al during GTA-additive manufacturing [J]. Int. J. Adv. Manuf. Technol., 2016, 87: 2615
27 Staley J T, Haupin W. Aluminum and aluminum alloys [M]. New York: John Wiley & Sons Inc, 2000: 186
28 Olakanmi E O, Cochrane R F, Dalgarno K W. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: Processing, microstructure, and properties [J]. Prog. Mater. Sci., 2015, 74: 401
29 Bai J Y, Fan C L, Lin S B, et al. Mechanical properties and fracture behaviors of GTA-additive manufactured 2219-Al after an especial heat treatment [J]. J. Mater. Eng. Perform., 2017, 26: 1808
30 Liu D H, Wu D J, Ma G Y, et al. Effect of post-deposition heat treatment on laser-TIG hybrid additive manufactured Al-Cu alloy [J]. Virtual Phys. Prototyp., 2020, 15: 445
文章导航

/