冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响

  • 王长胜 ,
  • 付华栋 ,
  • 张洪涛 ,
  • 谢建新
展开
  • 1北京科技大学 北京材料基因工程高精尖创新中心 北京 100083
    2北京科技大学 现代交通金属材料与加工技术北京实验室 北京 100083
    3北京科技大学 材料先进制备技术教育部重点实验室 北京 100083
王长胜,男,1986年生,博士生

收稿日期: 2021-05-17

  修回日期: 2021-07-06

  网络出版日期: 2022-01-05

基金资助

国家重点研发计划项目(2020YFB0311101);国家自然科学基金项目(51974028);国家自然科学基金项目(92066205);北京市科技新星计划项目(Z191100001119125);小米青年学者项目

Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys

  • WANG Changsheng ,
  • FU Huadong ,
  • ZHANG Hongtao ,
  • XIE Jianxin
Expand
  • 1Beijing Advanced Innovation Center for Materials Genome Engineering, University of Science and Technology Beijing, Beijing 100083, China
    2Beijing Laboratory of Metallic Materials and Processing for Modern Transportation, University of Science and Technology Beijing, Beijing 100083, China
    3Key Laboratory for Advanced Materials Processing (MOE), University of Science and Technology Beijing, Beijing 100083, China

Received date: 2021-05-17

  Revised date: 2021-07-06

  Online published: 2022-01-05

Supported by

National Key Research and Development Program of China(2020YFB0311101);National Natural Science Foundation of China(51974028);National Natural Science Foundation of China(92066205);Beijing Nova Programs(Z191100001119125);Fund for Xiaomi Young Scholars

摘要

采用DSC、TEM、导电率和力学性能等测试方法,研究了不同冷轧变形量对Cu-3.0Ni-0.60Si-0.16Zn-0.15Cr-0.03P (质量分数,%)合金组织性能与析出行为的影响,旨在通过工艺调控提升该合金的综合性能。通过对比不同冷轧变形后合金的开始析出温度和再结晶温度以及时效后合金的组织性能,确定了高性能Cu-Ni-Si系合金的形变-时效工艺参数,明确了冷轧变形量对合金时效析出动力学的影响规律和强化相析出的调控机制;合金经过95%冷轧+ 450℃、60 min形变热处理后获得了显著优于现有Cu-Ni-Si合金(如C70250)的性能,其抗拉强度为(841 ± 10) MPa,导电率为(52.2 ± 0.3)%IACS。

本文引用格式

王长胜 , 付华栋 , 张洪涛 , 谢建新 . 冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响[J]. 金属学报, 2023 , 59(5) : 585 -598 . DOI: 10.11900/0412.1961.2021.00208

Abstract

The advancement of integrated circuit manufacturing process and chip packaging technology has improved the performance requirements for lead frame copper alloy. In the field of high-performance copper alloys, balancing and improving mechanical and electrical conductivity (EC) has been a challenge. This work investigates the effect of different cold-rolling deformations (0, 65%, 75%, 85%, and 95%) on the microstructure, properties, and precipitation behavior of Cu-3.0Ni-0.60Si-0.16Zn-0.15Cr-0.03P alloy to enhance its comprehensive performance through process control. The deformation-aging process parameters of high-performance Cu-Ni-Si alloys were determined by comparing the precipitation and recrystallization initial temperatures, microstructures, and properties of the samples after aging. The effect of cold-rolling deformation on precipitation kinetics and mechanism was studied. By optimizing the process parameters, the properties of the alloy are observed to be better than the existing Cu-Ni-Si alloys after 95% cold-rolling deformation and aging at 450oC for 60 min, with an ultimate tensile strength of (841 ± 10) MPa, and an EC of (52.2 ± 0.3)%IACS. This work's relevant research findings can provide theoretical reference and data support for realizing the comprehensive property enhancement of high-performance copper alloys.

参考文献

1 Jiang Y X, Lou H F, Xie H F, et al. Development status and prospects of advanced copper alloy[J]. Strateg. Study CAE, 2020, 22(5): 84
  姜业欣, 娄花芬, 解浩峰 等. 先进铜合金材料发展现状与展望[J]. 中国工程科学, 2020, 22(5): 84
2 Lei Q, Xiao Z, Hu W P, et al. Phase transformation behaviors and properties of a high strength Cu-Ni-Si alloy[J]. Mater. Sci. Eng., 2017, A697: 37
3 Lee S, Matsunaga H, Sauvage X, et al. Strengthening of Cu-Ni-Si alloy using high-pressure torsion and aging[J]. Mater. Charact., 2014, 90: 62
4 Wang C S, Fu H D, Xie J X. Dynamic recrystallization behavior and microstructure evolution of high-performance Cu-3.28Ni-0.6Si-0.22Zn-0.11Cr-0.04P during hot compression[J]. Rare Met., 2021, 40: 156
5 Xu S, Fu H D, Wang Y T, et al. Effect of Ag addition on the microstructure and mechanical properties of Cu-Cr alloy[J]. Mater. Sci. Eng., 2018, A726: 208
6 Zhao Z Q, Xiao Z, Li Z, et al. Effect of magnesium on microstructure and properties of Cu-Cr alloy[J]. J. Alloys Compd., 2018, 752: 191
7 Gholami M, Vesely J, Altenberger I, et al. Effects of microstructure on mechanical properties of CuNiSi alloys[J]. J. Alloys Compd., 2017, 696: 201
8 Li D M, Jiang B B, Li X N, et al. Composition rule of high hardness and electrical conductivity Cu-Ni-Si alloys[J]. Acta Metall. Sin., 2019, 55: 1291
  李冬梅, 姜贝贝, 李晓娜 等. 高硬导电Cu-Ni-Si合金成分规律[J]. 金属学报, 2019, 55: 1291
9 Monzen R, Watanabe C. Microstructure and mechanical properties of Cu-Ni-Si alloys[J]. Mater. Sci. Eng., 2008, A483-484: 117
10 Liu F, Li J, Peng L J, et al. Simultaneously enhanced hardness and electrical conductivity in a Cu-Ni-Si alloy by addition of Cobalt[J]. J. Alloys Compd., 2021, 862: 158667
11 Wang W, Kang H J, Chen Z N, et al. Effects of Cr and Zr additions on microstructure and properties of Cu-Ni-Si alloys[J]. Mater. Sci. Eng., 2016, A673: 378
12 Hou L L, Yin Z X, Gan C L, et al. Research progress of Cu-Ni-Si alloy for lead frame and its preparation and processing technology[J]. Mater. Res. Appl., 2020, 14: 59
  侯绿林, 尹振兴, 甘春雷 等. 引线框架用Cu-Ni-Si合金及其制备加工工艺的研究进展[J]. 材料研究与应用, 2020, 14: 59
13 Li J, Huang G J, Mi X J, et al. Effect of Ni/Si mass ratio and thermomechanical treatment on the microstructure and properties of Cu-Ni-Si alloys[J]. Materials, 2019, 12: 2076
14 Ghosh G, Miyake J, Fine M E. The systems-based design of high-strength, high-conductivity alloys[J]. JOM, 1997, 49(3): 56
15 Chen W, Li Z, Xie H, et al. Influence of Zinc on coarsening of δ-Ni2Si particles, aging behavior and hardness in a Cu-Ni-Si alloy[J]. J. Mater. Eng. Perform., 2017, 26: 2459
16 Zhang Y, Tian B H, Volinsky A A, et al. Microstructure and precipitate's characterization of the Cu-Ni-Si-P alloy[J]. J. Mater. Eng. Perform., 2016, 25: 1336
17 Wang W, Guo E Y, Chen Z N, et al. Correlation between microstructures and mechanical properties of cryorolled CuNiSi alloys with Cr and Zr alloying[J]. Mater. Charact., 2018, 144: 532
18 Peng L J, Ma J M, Liu X Y, et al. Influence of different treatment processes on microstructure and properties of Cu-Ni-Co-Si alloy[J]. Rare Met. Mater. Eng., 2019, 48: 1969
  彭丽军, 马吉苗, 刘兴宇 等. 不同处理工艺对Cu-Ni-Co-Si合金组织与性能的影响[J]. 稀有金属材料与工程, 2019, 48: 1969
19 Xiao X P, Xu H, Chen J S, et al. Coarsening behavior of (Ni, Co)2Si particles in Cu-Ni-Co-Si alloy during aging treatment[J]. Rare Met., 2019, 38: 1062
20 Feng G B, Yu F X, Cheng J Y, et al. Re-aging behaviour and precipitated phase characteristics of high-performance Cu-Ni-Co-Si alloy[J]. Trans. Mater. Heat Treat., 2019, 40(8): 76
  冯桄波, 余方新, 程建奕 等. 高性能Cu-Ni-Co-Si合金的二次时效行为及析出相特征[J]. 材料热处理学报, 2019, 40(8): 76
21 Wang C S, Fu H D, Jiang L, et al. A property-oriented design strategy for high performance copper alloys via machine learning[J]. npj Comput. Mater., 2019, 5: 87
22 Xiao X P, Xiong B Q, Wang Q S, et al. Microstructure and properties of Cu-Ni-Si-Zr alloy after thermomechanical treatments[J]. Rare Met., 2013, 32: 144
23 Kareva N T, Yakovleva I L, Samoilova O V. On the precipitation strengthening of Cu-2.6Ni-0.6Si-0.6Cr bronzes[J]. Phys. Met. Metallogr., 2017, 118: 795
24 Li H X, Hao X J, Zhao G, et al. Effect of plastic deformation on discontinuous coarsening of spinodally decomposed microstructure in Cu-Ni-Fe alloy[J]. Acta Metall. Sin., 1999, 35: 449
  李洪晓, 郝新江, 赵 刚 等. 塑性变形对Cu-Ni-Fe合金失稳分解组织不连续粗化的影响[J]. 金属学报, 1999, 35: 449
25 Rdzawski Z, Stobrawa J. Thermomechanical processing of Cu-Ni-Si-Cr-Mg alloy[J]. Mater. Sci. Technol., 1993, 9: 142
26 Suzuki S, Shibutani N, Mimura K, et al. Improvement in strength and electrical conductivity of Cu-Ni-Si alloys by aging and cold rolling[J]. J. Alloys Compd., 2006, 417: 116
27 Watanabe H, Kunimine T, Watanabe C, et al. Tensile deformation characteristics of a Cu-Ni-Si alloy containing trace elements processed by high-pressure torsion with subsequent aging[J]. Mater. Sci. Eng., 2018, A730: 10
28 Liu F, Mi X J, Ma J M, et al. Microstructure and properties of low concentration of Cu-Ni-Si alloy[J]. Chin. J. Nonferrous Met., 2019, 29: 286
  刘 峰, 米绪军, 马吉苗 等. 低浓度Cu-Ni-Si合金的组织与性能[J]. 中国有色金属学报, 2019, 29: 286
29 Wang Y H, Wang M P, Hong B, et al. Microstructure and properties of Cu-15Ni-8Sn-0.4Si alloy[J]. Trans. Nonferrous Met. Soc. China, 2003, 13: 1051
30 Sun X L, Jie J C, Wang T M, et al. Effect of two-step cryorolling and aging on mechanical and electrical properties of a Cu-Cr-Ni-Si alloy for lead frames applications[J]. Mater. Sci. Eng., 2021, A809: 140521
31 Lei Q, Li Z, Gao Y, et al. Microstructure and mechanical properties of a high strength Cu-Ni-Si alloy treated by combined aging processes[J]. J. Alloys Compd., 2017, 695: 2413
32 Yang J Z, Bu K, Song K X, et al. Influence of low-temperature annealing temperature on the evolution of the microstructure and mechanical properties of Cu-Cr-Ti-Si alloy strips[J]. Mater. Sci. Eng., 2020, A798: 140120
33 Han S Z, Choi E A, Lim S H, et al. Alloy design strategies to increase strength and its trade-offs together[J]. Prog. Mater. Sci., 2021, 117: 100720
34 Yang H Y, Ma Z C, Lei C H, et al. High strength and high conductivity Cu alloys: A review[J]. Sci. China Technol. Sci., 2020, 63: 2505
35 Geng Y F, Ban Y J, Wang B J, et al. A review of microstructure and texture evolution with nanoscale precipitates for copper alloys[J]. J. Mater. Res. Technol., 2020, 9: 11918
36 Jiang L, Fu H D, Wang C S, et al. Enhanced mechanical and electrical properties of a Cu-Ni-Si alloy by thermo-mechanical processing[J]. Metall. Mater. Trans., 2020, 51A: 331
37 Huang G J, Xiao X P, Ma J M, et al. Effect of solid solution and aging process on microstructure and properties of Cu-1.4Ni-1.2Co-0.6Si alloy[J]. Trans. Mater. Heat Treat., 2014, 35(8): 58
  黄国杰, 肖翔鹏, 马吉苗 等. 固溶时效对Cu-1.4Ni-1.2Co-0.6Si合金组织性能的影响[J]. 材料热处理学报, 2014, 35(8): 58
38 Yi J, Jia Y L, Zhao Y Y, et al. Precipitation behavior of Cu-3.0Ni-0.72Si alloy[J]. Acta Mater., 2019, 166: 261
39 Wu Y K, Li Y, Lu J Y, et al. Effects of pre-deformation on precipitation behaviors and properties in Cu-Ni-Si-Cr alloy[J]. Mater. Sci. Eng., 2019, A742: 501
40 Hu T, Chen J Z, Liu J Z, et al. The crystallographic and morphological evolution of the strengthening precipitates in Cu-Ni-Si alloys[J]. Acta Mater., 2013, 61: 1210
41 Cheng J Y, Tang B B, Yu F X, et al. Evaluation of nanoscaled precipitates in a Cu-Ni-Si-Cr alloy during aging[J]. J. Alloys Compd., 2014, 614: 189
42 Liao Y H, Xie M W, Chen H M, et al. Thermodynamics and kinetics of discontinuous precipitation in Cu-9Ni-xSn alloy[J]. J. Alloys Compd., 2020, 827: 154314
43 Lei Q, Li Z, Pan Z Y, et al. Dynamics of phase transformation of Cu-Ni-Si alloy with super-high strength and high conductivity during aging[J]. Trans. Nonferrous Met. Soc. China, 2010, 20: 1006
44 Su J H, Liu P, Li H J, et al. Phase transformation in Cu-Cr-Zr-Mg alloy[J]. Mater. Lett., 2007, 61: 4963
文章导航

/